The Recovery of Alcohol and Benzene during Peparation of Ultrafine Powder by the Metal Alcoxidos Hydrolysis AITranslate

Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of recovery of organic reagents during the preparation of ultrafine powder by metal alcoxides hydrolysis.The Phase diagrams of isopropanol benzene system and isopropanol benzene water system have been plotted,based on which,isopropanol and benzene can be recovered and recirculated by distillation rectification process.The recovery and reused rate of alcohol and benzene are above 75%.So both the environmental pollution and cost of ultrfine powder are reduced.

KeyWords AITranslate

alcoxides hydrolysis ultra fine powder alchol benzene recovery distillation rectification

1尾崎义治.金属アルコキシドカらのセラミツワクスの制造(上)[J].工业材料,1981,29(5):85-85.

2段学臣,张多默,赵天从.超微锑白(Sb_2O_3)的研究[J].中南矿冶学院学报,1990,21(5):485-491. 被引量:11

3DUAN Xue-chen,et al.Phase Equilibrium of SbCI3-HCI-H2O System[J].Transatctions of Nonferrous Metals Society of China,1994,(1):15.

4张多默,陈慧光,陈文汨,罔田茂,矢沢彬.水-硫酸铜-乙二醇单丁醚体系相平衡研究[J].中南矿冶学院学报,1989,20(3):260-267. 被引量:2

1舒华,郭海福,吴文胜,吴燕妮,闫鹏.新型稀土固体超强酸S_2O_8^(2-)/Sb_2O_3/La^(3+)的制备与再生[J].精细石油化工,2008,25(5):12-16. 被引量:4

1宋华,石洋.SO_4^(2-)/M_xO_y型固体超强酸催化剂研究进展[J].精细石油化工进展,2011,12(11):17-23. 被引量:1

2陈英,周东亮,陈东,姬彬.高酸值生物柴油原料甘油酯化脱酸研究[J].燃料化学学报,2012,40(12):1429-1434. 被引量:8

3周曾艳,舒华,唐帮成,吴思展,陈美航.锑铁复合固体超强酸S_2O_8^(2-)/Sb_2O_3/Fe_2O_3催化合成丁醛乙二醇缩醛[J].广州化工,2013,41(10):68-70. 被引量:3

4张蔚欣,廖列文,胡文斌,龚红升.负载型固体超强酸催化剂研究进展[J].仲恺农业工程学院学报,2014,27(1):62-66. 被引量:1

1段学臣,黄蔚庄,赵天从.高纯超细锑白的研制[J].矿冶工程,1998,18(2):61-63. 被引量:2

2吕绪良,韩卫华,李玉科,王占峰,邵锦萍.超细SiO_2的制备及水合特性实验分析[J].解放军理工大学学报:自然科学版,2006,7(2):145-147.

3戴健,温廷琏,吕之奕.醇盐水解法制备的纳米级稳定氧化锆细粉[J].无机材料学报,1993,8(1):51-56. 被引量:11

4姚敏琪,卫英慧,胡兰青,许并社.溶胶-凝胶法制备纳米粉体[J].稀有金属材料与工程,2002,31(5):325-329. 被引量:30

5段学臣,张多默,赵天从.超微锑白(Sb_2O_3)的研究[J].中南矿冶学院学报,1990,21(5):485-491. 被引量:11

6赵治文,王俊.应用有机试剂解吸载金炭的研究[J].有色冶炼,2000,29(2):27-29. 被引量:2

7张琳,朱广军,罗军,王恒志.醇盐水解法制备纳米级Sb_2O_3粒子[J].化学世界,2003,44(12):619-621. 被引量:1

8赤泥大规模利用技术[J].中国有色冶金,2013,42(2):23-23.

9李历历,段学臣.超声水解法制备抗团聚纳米ATO粉末[J].稀有金属与硬质合金,2004,32(4):17-20. 被引量:3

10曹璇,郭华军,张宝,王志兴,李新海.NaOH-C_3H_8O_3的水溶液体系处理冶金副产物的研究[J].湖南有色金属,2008,24(6):23-26.

Basic Information:

DOI:

Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]

Citation Information:

Study is made of recovery of organic reagents during the preparation of ultrafine powder by metal alcoxides hydrolysis.The Phase diagrams of isopropanol benzene system and isopropanol benzene water system have been plotted,based on which,isopropanol and benzene can be recovered and recirculated by distillation rectification process.The recovery and reused rate of alcohol and benzene are above 75%.So both the environmental pollution and cost of ultrfine powder are reduced.

quote

GB/T 7714-2015 [1] DUAN Xue-chen, YANG Xiang-ping, WU Xiang-wei. The Recovery of Alcohol and Benzene during Peparation of Ultrafine Powder by the Metal Alcoxidos Hydrolysis[J]. Rare Metals and Cemented Carbides, 2001(2): 41-43.
MLA [1] DUAN Xue-chen, et al., "The Recovery of Alcohol and Benzene during Peparation of Ultrafine Powder by the Metal Alcoxidos Hydrolysis." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 41-43.
APA [1] DUAN Xue-chen, YANG Xiang-ping, & WU Xiang-wei. (2001). The Recovery of Alcohol and Benzene during Peparation of Ultrafine Powder by the Metal Alcoxidos Hydrolysis. Rare Metals and Cemented Carbides(2), 41-43.
IEEE [1] DUAN Xue-chen, YANG Xiang-ping, and WU Xiang-wei, "The Recovery of Alcohol and Benzene during Peparation of Ultrafine Powder by the Metal Alcoxidos Hydrolysis," Rare Metals and Cemented Carbides, no. 2, pp. 41-43, 2001. keywords: {alcoxides hydrolysis;ultra fine powder;alchol;benzene;recovery;distillation rectification}