daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

4D-Printed Resins and Nanocomposites Thermally Stimulated by Conventional Heating and IR Radiation AITranslate

University Rey Juan Carlos; University Rey Juan Carlos;Department of Applied Science and Technology, Politecnico di Torino; University Rey Juan Carlos; University Rey Juan Carlos;Department of Applied Science and Technology, Politecnico di Torino; University Rey Juan Carlos; University Rey Juan Carlos
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The shape memory (SM) capabilities of nanocomposites based on two photocurable acrylated/methacrylated resins, doped with carbon nanotubes (CNTs), and manufactured by digital light processing 3D printing were investigated. The mechanical properties and glass transition temperature (Tg) can be tailored in a broad range by varying the weight ratio of the two resins (Tg ranging from 15 to 190 °C; Young’s modulus from 1.5 to 2500 MPa). Shape fixity (SF) and recovery (SR) ratios are strongly influenced by the temperature being significantly higher at temperatures close to the Tg. The results confirm that the SF strongly depends on the stiffness of chain segments between cross-linking points, whereas the SR mainly depends on the cross-link density of the network. CNT addition barely affects the SF and SR in the conventional oven, whereas the recovery speed using IR heating is significantly increased for the doped nanocomposites due to their higher IR absorbance.

KeyWords AITranslate

shape memory 4D printing additive manufacturing carbon nanotubes nanocomposites
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00970

Chinese Library Classification Number:

Citation Information:

The shape memory (SM) capabilities of nanocomposites based on two photocurable acrylated/methacrylated resins, doped with carbon nanotubes (CNTs), and manufactured by digital light processing 3D printing were investigated. The mechanical properties and glass transition temperature (Tg) can be tailored in a broad range by varying the weight ratio of the two resins (Tg ranging from 15 to 190 °C; Young’s modulus from 1.5 to 2500 MPa). Shape fixity (SF) and recovery (SR) ratios are strongly influenced by the temperature being significantly higher at temperatures close to the Tg. The results confirm that the SF strongly depends on the stiffness of chain segments between cross-linking points, whereas the SR mainly depends on the cross-link density of the network. CNT addition barely affects the SF and SR in the conventional oven, whereas the recovery speed using IR heating is significantly increased for the doped nanocomposites due to their higher IR absorbance.

quote

GB/T 7714-2015 [1] A. Cortés, Jose L. Aguilar, A. Cosola, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00970.
MLA [1] A. Cortés, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00970.
APA [1] A. Cortés, Jose L. Aguilar, A. Cosola, Xoan Xosé Fernández SanchezRomate, A. JiménezSuárez, M. Sangermano, M. Campo, & Silvia G. Prolongo. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00970
IEEE [1] A. Cortés, Jose L. Aguilar, A. Cosola, Xoan Xosé Fernández SanchezRomate, A. JiménezSuárez, M. Sangermano, M. Campo, and Silvia G. Prolongo, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00970. keywords: {shape memory;4D printing;additive manufacturing;carbon nanotubes;nanocomposites}