Improvement of Physical Properties of Cemented Carbide Sprayed Powder AITranslate

Zhuzhou Cemented Carbide Factory Tantalum Niobium Processing Branch;Zhuzhou Cemented Carbide Factory Tantalum Niobium Processing Branch
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cemented carbide sprayed powder is a new hard material,mainly used for high temperature resistant and wear resistant parts in various motors,shafts ,large fan vanes and seal rings,etc,with extremely strict requirement for its physical properties.The paper describes the study of influence of sintering temperature and other processing technologies on the physical properties of the cemented carbide sprayed powder.The results showed that the use of the new technology can assure the physical properties of the cemented carbide sprayed powder up to the foreign clients requirement.

KeyWords AITranslate

cemented carbide sprayed powder sintering temperature ball milling

1王国栋.硬质合金生产原理[M].北京:冶金工业出版社,1990.

2黄培云.粉末冶金原理[M].北京:冶金工业出版社,1988.341.

3内藤牧男 等.粉末制造技术在热喷涂领域的作用[J].热喷涂技术,1997,(4).

1梁楚华,周建平,朱志坚,何英.短电弧加工技术及其应用[J].现代制造工程,2007(12):92-93. 被引量:39

2邹序救.碳化钨硬面材料和硬面技术[J].硬质合金,1991,8(1):36-43. 被引量:5

3李勇,谢淑华.粗晶硬质合金的研究现状及其发展前景[J].江西冶金,2008,28(6):42-46. 被引量:8

4桂业炜.硬面技术的应用[J].机械制造,1995,33(2):8-10. 被引量:2

5朱润生.堆焊管状焊丝及其应用[J].粉末冶金工业,2003,13(5):33-38. 被引量:1

6四川热喷涂硬面材料实现产业化[J].表面工程资讯,2013,13(2):21-21.

7印度JSL公司向中国二重订购1750mm不锈钢平整机组[J].不锈:市场与信息,2010(24):6-6.

8吴涛.上海市冶金高新技术产品发展状况及发展对策(待续)[J].上海冶金情报,1995(4):31-42.

9徐尚志,李玉玺,周伍喜.硬面技术-热喷涂现状及发展[J].中国钨业,2012,27(2):28-31. 被引量:3

10郭林,苑举勇.锥形破碎机主框架的铸造工艺[J].铸造工程,2013,37(1):26-28.

Basic Information:

DOI:

Chinese Library Classification Number:TG174.442[金属学及工艺—金属表面处理];TF125.3[冶金工程—粉末冶金]

Citation Information:

Cemented carbide sprayed powder is a new hard material,mainly used for high temperature resistant and wear resistant parts in various motors,shafts ,large fan vanes and seal rings,etc,with extremely strict requirement for its physical properties.The paper describes the study of influence of sintering temperature and other processing technologies on the physical properties of the cemented carbide sprayed powder.The results showed that the use of the new technology can assure the physical properties of the cemented carbide sprayed powder up to the foreign clients requirement.

quote

GB/T 7714-2015 [1] YANG Ge, CHEN Wei-hong. Improvement of Physical Properties of Cemented Carbide Sprayed Powder[J]. Rare Metals and Cemented Carbides, 2001(2): 57-60.
MLA [1] YANG Ge, and CHEN Wei-hong. "Improvement of Physical Properties of Cemented Carbide Sprayed Powder." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 57-60.
APA [1] YANG Ge, & CHEN Wei-hong. (2001). Improvement of Physical Properties of Cemented Carbide Sprayed Powder. Rare Metals and Cemented Carbides(2), 57-60.
IEEE [1] YANG Ge and CHEN Wei-hong, "Improvement of Physical Properties of Cemented Carbide Sprayed Powder," Rare Metals and Cemented Carbides, no. 2, pp. 57-60, 2001. keywords: {cemented carbide sprayed powder;sintering temperature;ball milling}