Preparation of High Purity TiB_2 Powder By Vacuum Carbothermic Reduction AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper, TiB2 powder of 99.34% purity is prepared by vacuum carbothermic reduction of TiO, and B2O3 based on the thermodynamics analysis of the reaction TiO2+B2O3+5C→TiB2+5CO↑ The investigation results show that the actual reaction temperature can be decreased by about 200℃ by vacuum carbothermic reduction for TiB2preparation. Vacuum is very important for high purity TiB2 powder,while excessive amount of carbon in proper ratio can remarkably, enhance TiB2 purity.

KeyWords AITranslate

vacuum TiB2 powder carbothermic reduction preparation

1Brodkin D,et al.Microstructural optimization and mechanicalproperties of titanium carbide-titanium boride composites fabricated by transient plastic phase processing[A].TMS Processing and Fabrication of Advanced Materials[C].USA:Cleveland OH,1996.189.

2向军辉,肖汉宁.TiB_2材料的研究现状及其应用[J].陶瓷工程,1996,30(4):40-44. 被引量:35

3二硼化钛(TiB_2)──一种新型的极具开发应用前景的陶瓷原料[J].粉末冶金技术,1995,13(1):75-75. 被引量:7

4YuriditskyB.TiB2基硬质合金[J].国外难熔金属与硬质合金,1990,12(1):47-47.

5刘业翔,邹忠.导电陶瓷TiB_2开发与应用的最新进展[J].稀有金属,1996,20(6):438-443. 被引量:19

6Koc R,et al.Production of TiB2 from a precursor containing carbon coated TiO2 and B4C[J].Journal of Materials Science Letters,2000,19(8):667.

7赵昆渝,朱心昆,苏云生,张家棋.自蔓延高温合成制备TiB_2[J].粉末冶金技术,1997,15(1):26-28. 被引量:13

8徐强,张幸红,曲伟,韩杰才.SHS/PHIP法合成TiB_2陶瓷的研究[J].高技术通讯,2002,12(8):71-74. 被引量:4

9王兆文,邱竹贤,李涯.二硼化钛粉末的研制[J].轻金属,1997(8):28-32. 被引量:5

10刘希诚,孙阳,冯乃祥.电弧炉碳热还原制取二硼化钛[J].广东有色金属学报,1999,9(1):30-34. 被引量:3

1袁海滨,朱富龙,郁青春,李秋霞,徐宝强,杨斌,戴永年.Fe_2O_3、SiO_2和TiO_2对氧化铝真空碳热还原-氯化法炼铝过程的影响[J].中国有色金属学报,2010,20(9):1836-1842. 被引量:6

1周林.2010年云南金属材料与加工年评[J].云南冶金,2011,40(2):63-72. 被引量:1

2袁海滨,朱富龙,杨斌,徐宝强,戴永年.真空碳热还原法炼铝的研究进展[J].真空科学与技术学报,2011,31(6):765-774. 被引量:2

3罗启,曲涛,刘大春,田阳,杨斌,戴永年.红土镍矿真空碳热还原过程中硅的挥发行为[J].真空科学与技术学报,2012,32(5):430-436. 被引量:4

4冯月斌,郁青春,杨斌,戴永年.真空氯化亚铝歧化法从氧化铝中提取铝(英文)[J].中国有色金属学报:英文版,2013,23(9):2781-2785. 被引量:3

5冯月斌,杨斌,戴永年.真空AlCl歧化法生产铝的过程中C、Al_4C_3和Al_2O_3的形成热力学(英文)[J].中国有色金属学报:英文版,2014,24(10):3366-3371.

6李建军.钛冶金中沸腾氯化炉内衬材料损坏机理的研究[J].云南冶金,2017,46(5):47-51. 被引量:2

1黄正生.煅白真空碳热还原法炼镁[J].四川有色金属,1991(4):17-17.

2周书助,彭卫珍.硼热/碳热还原TiO_2合成高纯TiB_2粉末[J].硬质合金,2004,21(1):27-31. 被引量:1

3赵昆渝,严丙勇,李智东,李莉,朱心昆,段云彪,刘国玺,马秋花,葛伟萍.机械合金化制备TiB_2粉末的机理研究[J].机械工程材料,2004,28(3):25-27. 被引量:4

4李明怡,康志君,张宝生.自蔓延高温合成TiB_2粉末[J].稀有金属,1994,18(5):370-374. 被引量:3

5宋文杰,钟晖.TiB_2制备方法及其研究新进展[J].稀有金属与硬质合金,2005,33(2):47-52. 被引量:17

6孙红燕,孔馨,森维,王宝森,易中周,刘贵阳.真空碳热还原处理铅锌烟尘实验研究[J].真空科学与技术学报,2014,34(7):758-762. 被引量:5

7孙红燕,森维,孔馨,刘贵阳,陈昌兴.真空碳热还原法处理铅银渣热力学分析及实验研究[J].真空科学与技术学报,2017,37(3):327-331. 被引量:5

8张东明,傅正义,唐田,逄婷婷.球磨对放电等离子烧结TiB_2陶瓷的影响[J].武汉理工大学学报,2002,24(5):12-14.

9赵昆渝,朱心昆,苏云生,张家棋.自蔓延高温合成制备TiB_2[J].粉末冶金技术,1997,15(1):26-28. 被引量:13

10孙晓冬,袁润章.Al含量对Ti-B体系自蔓燃高温合成过程的影响[J].稀有金属与硬质合金,1998,26(2):27-31. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF123.121[冶金工程—粉末冶金]

Citation Information:

In this paper, TiB2 powder of 99.34% purity is prepared by vacuum carbothermic reduction of TiO, and B2O3 based on the thermodynamics analysis of the reaction TiO2+B2O3+5C→TiB2+5CO↑ The investigation results show that the actual reaction temperature can be decreased by about 200℃ by vacuum carbothermic reduction for TiB2preparation. Vacuum is very important for high purity TiB2 powder,while excessive amount of carbon in proper ratio can remarkably, enhance TiB2 purity.

quote

GB/T 7714-2015 [1] SONG Wen-jie, ZHONG Hui, YUAN Yan, et al. Preparation of High Purity TiB_2 Powder By Vacuum Carbothermic Reduction[J]. Rare Metals and Cemented Carbides, 2006(1): 9-13.
MLA [1] SONG Wen-jie, et al., "Preparation of High Purity TiB_2 Powder By Vacuum Carbothermic Reduction." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 9-13.
APA [1] SONG Wen-jie, ZHONG Hui, YUAN Yan, YANG Jian-wen, DAI Yan-yang, & ZHONG Hai-yun. (2006). Preparation of High Purity TiB_2 Powder By Vacuum Carbothermic Reduction. Rare Metals and Cemented Carbides(1), 9-13.
IEEE [1] SONG Wen-jie, ZHONG Hui, YUAN Yan, YANG Jian-wen, DAI Yan-yang, and ZHONG Hai-yun, "Preparation of High Purity TiB_2 Powder By Vacuum Carbothermic Reduction," Rare Metals and Cemented Carbides, no. 1, pp. 9-13, 2006. keywords: {vacuum;TiB2 powder;carbothermic reduction;preparation}