daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Dielectric Properties of Biaxially Oriented Polypropylene Nanocomposites Prepared Based on Reactor Granule Technology AITranslate

Japan Advanced Institute of Science and Technology; Japan Advanced Institute of Science and Technology; Japan Advanced Institute of Science and Technology;Advanced Film Research Center, Oji Holdings Corporation;Advanced Film Research Center, Oji Holdings Corporation; Japan Advanced Institute of Science and Technology; Japan Advanced Institute of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The addition of inorganic nanoparticles is one of the most widely studied strategies to improve dielectric properties of thin film capacitors, but its application to biaxially oriented polypropylene (BOPP) has rarely been reported due to the difficulty of stretching without break. Here, we have investigated dielectric properties of BOPP/TiO2 nanocomposites prepared by a reactor granule technology, in which precursors impregnated in the pores of PP reactor granule are converted into highly dispersed oxide nanoparticles during melt mixing. The permittivity of the nanocomposites was greatly enhanced beyond classical mixing rules by the addition of a small amount of TiO2 nanoparticles (1–5 wt %), and the enhancement was very sensitive to the stretching ratio. A critical role of the interphase region was suggested. The AC breakdown voltage (BDV) of the BOPP/TiO2 nanocomposites decreased sharply with respect to the amount of TiO2 added. The detailed analysis suggested the roughening of the film surface around the nanoparticles due to stretching as the main cause of the BDV reduction.

KeyWords AITranslate

biaxially oriented polypropylene dielectric properties nanocomposites reactor granule technology titanium dioxide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01335

Chinese Library Classification Number:

Citation Information:

The addition of inorganic nanoparticles is one of the most widely studied strategies to improve dielectric properties of thin film capacitors, but its application to biaxially oriented polypropylene (BOPP) has rarely been reported due to the difficulty of stretching without break. Here, we have investigated dielectric properties of BOPP/TiO2 nanocomposites prepared by a reactor granule technology, in which precursors impregnated in the pores of PP reactor granule are converted into highly dispersed oxide nanoparticles during melt mixing. The permittivity of the nanocomposites was greatly enhanced beyond classical mixing rules by the addition of a small amount of TiO2 nanoparticles (1–5 wt %), and the enhancement was very sensitive to the stretching ratio. A critical role of the interphase region was suggested. The AC breakdown voltage (BDV) of the BOPP/TiO2 nanocomposites decreased sharply with respect to the amount of TiO2 added. The detailed analysis suggested the roughening of the film surface around the nanoparticles due to stretching as the main cause of the BDV reduction.

quote

GB/T 7714-2015 [1] Xi Zhang, Dongzhi Zhu, Hui You, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01335.
MLA [1] Xi Zhang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01335.
APA [1] Xi Zhang, Dongzhi Zhu, Hui You, Yuya Hashimoto, Tadakazu Miyata, Patchanee Chammingkwan, & Toshiaki Taniike. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01335
IEEE [1] Xi Zhang, Dongzhi Zhu, Hui You, Yuya Hashimoto, Tadakazu Miyata, Patchanee Chammingkwan, and Toshiaki Taniike, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01335. keywords: {biaxially oriented polypropylene dielectric properties nanocomposites reactor granule technology titanium dioxide}