Sensing explosive taggants such as 3-nitrotoluene (3-NT) and 2,3-dimethyl-2,3-dinitrobutane has become a strategic priority in homeland security. This work reports the synthesis of a solid-state plasmonic sensor based on a nanocomposite of Ag nanoparticles (NPs) embedded in a molecularly imprinted polymer (MIP) for selective detection of 3-NT, an explosive taggant for 2,4,6-trinitrotoluene. In our approach, the in situ synthesis of Ag NPs and the molecular imprinting with 3-NT as a template take place simultaneously inside the polyethyleneimine (PEI) thin film during the baking step after spin coating. The MIP sensor fabrication is done by a low-cost, fast, and scalable one-step procedure. We demonstrate the chemosensing capabilities of Ag-PEI MIP nanocomposites to 3-NT using the localized surface plasmon resonance band intensity decay as a sensing parameter. The molecular imprinting approach results in an enhancement of specific sensor response to 3-NT, with a limit of detection of 54.8 ng for 3-NT and a sensitivity of 24.0% ± 3.0%. We tested the MIP sensor specificity by comparing the sensor response to several NO2-containing molecules. The Ag-PEI MIP sensor demonstrated a robust, specific molecular recognition toward 3-NT. Because the MIP nanocomposite sensor is easy to prepare, easy to use, and inexpensive, these plasmonic sensors can be easily implemented with portable reading platforms into remote explosive detection and bomb disposal robots.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00116
Chinese Library Classification Number:
Citation Information:
Sensing explosive taggants such as 3-nitrotoluene (3-NT) and 2,3-dimethyl-2,3-dinitrobutane has become a strategic priority in homeland security. This work reports the synthesis of a solid-state plasmonic sensor based on a nanocomposite of Ag nanoparticles (NPs) embedded in a molecularly imprinted polymer (MIP) for selective detection of 3-NT, an explosive taggant for 2,4,6-trinitrotoluene. In our approach, the in situ synthesis of Ag NPs and the molecular imprinting with 3-NT as a template take place simultaneously inside the polyethyleneimine (PEI) thin film during the baking step after spin coating. The MIP sensor fabrication is done by a low-cost, fast, and scalable one-step procedure. We demonstrate the chemosensing capabilities of Ag-PEI MIP nanocomposites to 3-NT using the localized surface plasmon resonance band intensity decay as a sensing parameter. The molecular imprinting approach results in an enhancement of specific sensor response to 3-NT, with a limit of detection of 54.8 ng for 3-NT and a sensitivity of 24.0% ± 3.0%. We tested the MIP sensor specificity by comparing the sensor response to several NO2-containing molecules. The Ag-PEI MIP sensor demonstrated a robust, specific molecular recognition toward 3-NT. Because the MIP nanocomposite sensor is easy to prepare, easy to use, and inexpensive, these plasmonic sensors can be easily implemented with portable reading platforms into remote explosive detection and bomb disposal robots.
quote
| GB/T 7714-2015 | [1] Eduardo AznarGadea, Pedro J. RodríguezCanto, Juan P. MartínezPastor, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00116. |
| MLA | [1] Eduardo AznarGadea, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00116. |
| APA | [1] Eduardo AznarGadea, Pedro J. RodríguezCanto, Juan P. MartínezPastor, Andrii Lopatynskyi, Vladimir Chegel, & Rafael Abargues. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00116 |
| IEEE | [1] Eduardo AznarGadea, Pedro J. RodríguezCanto, Juan P. MartínezPastor, Andrii Lopatynskyi, Vladimir Chegel, and Rafael Abargues, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00116. keywords: {silver nanoparticles;molecularly imprinted polymer;sensor;explosive taggant;3nitrotoluene;nanocomposite} |