Versatile Functionality of Four-Terminal TiO2–x Memristive Devices as Artificial Synapses for Neuromorphic Computing Versatile Functionality of Four-Terminal TiO2–x Memristive Devices as Artificial Synapses for Neuromorphic Computing AITranslate
Abstract AITranslate
Brain-inspired computing systems, which emulate the activity of biological synapses and neurons, are becoming more and more essential owing to their potential ability to solve the von Neumann bottleneck. Various types of memristive devices have been proposed to achieve information processing through synaptic functions. However, biological synapses have many complicated functions, such as heterosynaptic plasticity and the related neuromodulation, that are difficult to implement in conventional two-terminal memristors because of the requirement for multiple inputs. In this study, simple four-terminal memristive devices consisting of epitaxial thin films of TiO2–x are fabricated and their capacity to implement synaptic functions are explored. These devices utilize the two-dimensional variation of the oxygen vacancy distribution in the TiO2–x film to realize advanced heterosynaptic functionality, including tunable spike-timing-dependent plasticity, heterosynaptic plasticity mimicking habituation and sensitization, and Pavlovian conditioning, through multiterminal voltage inputs. The present results demonstrate the striking versatility of our four-terminal device for implementing the diverse and complex functions of artificial synapses on a single memristive passive element.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00161
Chinese Library Classification Number:
Citation Information:
Brain-inspired computing systems, which emulate the activity of biological synapses and neurons, are becoming more and more essential owing to their potential ability to solve the von Neumann bottleneck. Various types of memristive devices have been proposed to achieve information processing through synaptic functions. However, biological synapses have many complicated functions, such as heterosynaptic plasticity and the related neuromodulation, that are difficult to implement in conventional two-terminal memristors because of the requirement for multiple inputs. In this study, simple four-terminal memristive devices consisting of epitaxial thin films of TiO2–x are fabricated and their capacity to implement synaptic functions are explored. These devices utilize the two-dimensional variation of the oxygen vacancy distribution in the TiO2–x film to realize advanced heterosynaptic functionality, including tunable spike-timing-dependent plasticity, heterosynaptic plasticity mimicking habituation and sensitization, and Pavlovian conditioning, through multiterminal voltage inputs. The present results demonstrate the striking versatility of our four-terminal device for implementing the diverse and complex functions of artificial synapses on a single memristive passive element.
quote
| GB/T 7714-2015 | [1] Ryotaro Miyake, Zenya Nagata, Kenta Adachi, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00161. |
| MLA | [1] Ryotaro Miyake, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00161. |
| APA | [1] Ryotaro Miyake, Zenya Nagata, Kenta Adachi, Yusuke Hayashi, Tetsuya Tohei, & Akira Sakai. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00161 |
| IEEE | [1] Ryotaro Miyake, Zenya Nagata, Kenta Adachi, Yusuke Hayashi, Tetsuya Tohei, and Akira Sakai, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00161. keywords: {artificial synapse memristive device heterosynaptic neuromodulation reduced TiO2−x gatetuning multiterminalShow More} |