Repair of the Extrusion Chamber with Cracked Lining and Precautions for Crack Formation AITranslate
Abstract AITranslate
In view of the difficulty in cracked lining withdrawl from the extrusion chamber of 3150T extru- der,specially-designed accessory unit is used to cut off and withdraw the cracked lining. Upon checkup and repair of the inner wall of the extrusion chamber,the extruder can again be put into operation. Through a- nalysis of the cause of the crack in the lining, corresponding improvement are made. The practice proved that this method and improvement are feasible and effective.
KeyWords AITranslate
1沈蔚,周庆.挤压筒参数的选择及其对应力的影响[J].科技通报,2001,17(1):56-59. 被引量:2
2胡洪全,房崇顺,赵玉军.挤压筒损坏原因分析及其预防措施[J].轻合金加工技术,2002,30(7):38-39. 被引量:8
3赵应璠.挤压筒加工工艺研究[J].轻合金加工技术,2005,33(3):38-40. 被引量:4
4羊玉兰,佟学文,杨陇林.TC2钛合金管材挤压工艺[J].钛工业进展,2005,22(3):22-24. 被引量:7
1施平.对箱形桥式起重机主梁下挠有关问题的研究[J].武汉造船,1994(2):27-31.
2郑建梅.干气密封的故障分析与修复[J].机械工程师,2012(11):151-152.
3维修·保养·管理[J].工程机械文摘,1996(4):17-18.
4卧式有色金属挤压机[J].机电新产品导报,1996(1):26-26.
5于林波,冯春.滑动轴承修理装配与调整的若干问题[J].金属加工:冷加工,2013(3):75-77. 被引量:1
6程孝福,周广宇.气化炉托砖盘底板及Inconel 825镍基合金内环的更换[J].压力容器,2015,32(11):69-74. 被引量:1
7陶大勇,焦维光.油浆阀门粘接修复[J].设备管理与维修,2010(8):63-63.
8张艳,张永军.冷挤压组合模具的ANSYS应力分析[J].黑龙江科技学院学报,2010,20(1):72-76. 被引量:2
9陈兵.2DW-72/0.1-7型氢气压缩机气缸盖裂纹故障分析及修复办法[J].广东化工,2015,42(19):145-145. 被引量:1
10王继荣,李军,佟河亭.卧式挤压机推压余过程的摩擦诱导振动分析[J].青岛大学学报:工程技术版,2002,17(2):77-79.
Basic Information:
DOI:
Chinese Library Classification Number:TH17[机械工程—机械制造及自动化]
Citation Information:
In view of the difficulty in cracked lining withdrawl from the extrusion chamber of 3150T extru- der,specially-designed accessory unit is used to cut off and withdraw the cracked lining. Upon checkup and repair of the inner wall of the extrusion chamber,the extruder can again be put into operation. Through a- nalysis of the cause of the crack in the lining, corresponding improvement are made. The practice proved that this method and improvement are feasible and effective.
quote
| GB/T 7714-2015 | [1] GUO Bao-yin, DOU Hai-gang. Repair of the Extrusion Chamber with Cracked Lining and Precautions for Crack Formation[J]. Rare Metals and Cemented Carbides, 2007(4): 27-30. |
| MLA | [1] GUO Bao-yin, and DOU Hai-gang. "Repair of the Extrusion Chamber with Cracked Lining and Precautions for Crack Formation." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 27-30. |
| APA | [1] GUO Bao-yin, & DOU Hai-gang. (2007). Repair of the Extrusion Chamber with Cracked Lining and Precautions for Crack Formation. Rare Metals and Cemented Carbides(4), 27-30. |
| IEEE | [1] GUO Bao-yin and DOU Hai-gang, "Repair of the Extrusion Chamber with Cracked Lining and Precautions for Crack Formation," Rare Metals and Cemented Carbides, no. 4, pp. 27-30, 2007. keywords: {lining of the extrusion chamber;crack;cut-off;repair;improvement} |