Synergistic Regulation of Hole and Electron Transport Layers for Efficient Injection Balance in Deep Blue Quantum Dot Light-Emitting Diodes AITranslate

Tianjin University; Tianjin University; China|School of Materials Science and Engineering Tianjin Key Laboratory of Composite and Functional Materials Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The insufficient hole injection and excess electron injection unfortunately result in inferior performance in blue QLEDs. To study the predominant factors for hole injection, six different hole transport materials were investigated. The smaller energy barrier between the hole transport layer (HTL) and QDs dominates the injection, and high hole mobility further accelerates the process, which qualifies 4,4′-bis(3-vinyl-9H-carbazol-9-yl)-1,1′-biphenyl (CBP-V) as the most suitable HTL matrix. Simultaneously, moderate electron mobility reduction is also needed, which could be realized by PVP doping in the ZnO electron transport layer (ETL). The highly hole-mobile poly(9,9-dioctylfluorene-co-N-(4-(3-methylpropyl))diphenylamine) (TFB) was wrapped in the cross-linked CPB-V framework to further improve hole mobility and hole injection. The high level charge balance after the matching of 20 wt % TFB:CBP-V and 0.75 wt % PVP:ZnO enables high-performance blue QLEDs, with the EQE reaching 17.11% and the lifetime of 216 h at 100 cd/m2. Our investigation builds a general principle of both HTL and ETL material regulation for high-level injection balance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00955

Chinese Library Classification Number:

Citation Information:

The insufficient hole injection and excess electron injection unfortunately result in inferior performance in blue QLEDs. To study the predominant factors for hole injection, six different hole transport materials were investigated. The smaller energy barrier between the hole transport layer (HTL) and QDs dominates the injection, and high hole mobility further accelerates the process, which qualifies 4,4′-bis(3-vinyl-9H-carbazol-9-yl)-1,1′-biphenyl (CBP-V) as the most suitable HTL matrix. Simultaneously, moderate electron mobility reduction is also needed, which could be realized by PVP doping in the ZnO electron transport layer (ETL). The highly hole-mobile poly(9,9-dioctylfluorene-co-N-(4-(3-methylpropyl))diphenylamine) (TFB) was wrapped in the cross-linked CPB-V framework to further improve hole mobility and hole injection. The high level charge balance after the matching of 20 wt % TFB:CBP-V and 0.75 wt % PVP:ZnO enables high-performance blue QLEDs, with the EQE reaching 17.11% and the lifetime of 216 h at 100 cd/m2. Our investigation builds a general principle of both HTL and ETL material regulation for high-level injection balance.

quote

GB/T 7714-2015 [1] Xinyu Zhang, Shirong Wang, Dewang Li, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00955.
MLA [1] Xinyu Zhang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00955.
APA [1] Xinyu Zhang, Shirong Wang, Dewang Li, Jingxiang Wang, & Hongli Liu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00955
IEEE [1] Xinyu Zhang, Shirong Wang, Dewang Li, Jingxiang Wang, and Hongli Liu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00955.