daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Study on Contact Resistance as a Function of Surface Treatment in Perovskite Field-Effect Transistors A Study on Contact Resistance as a Function of Surface Treatment in Perovskite Field-Effect Transistors AITranslate

Wake Forest University; Wake Forest University; Wake Forest University; Wake Forest University; Princeton University; Appalachian State University; Wake Forest University; Appalachian State University; Princeton University; Wake Forest University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal halide perovskites are versatile materials which have already demonstrated exceptional performance in diverse optoelectronic devices. The progress has been significant; however, the fundamental understanding of the physics of charge injection remains elusive, impeding further advancements. Here, we use field-effect transistors (FETs) to investigate the impact of surface functionalization on the charge injection and transport in thin films of phenethylammonium tin iodide (PEA2SnI4). We show that self-assembled monolayers (SAMs) can both assist in reducing the Schottky barrier and act as an ion blocking layer between the contact and the perovskite film, limiting interfacial chemical reactions. Consequently, the contact resistance is lowered by more than 3 times compared to untreated contacts. The temperature dependence of the charge carrier mobility is discussed considering the contributions from the channel and contacts, respectively. Our results provide a quantitative framework for the charge injection in metal halide perovskites and will contribute toward the progress of high-performance optoelectronic devices including solar cells, light-emitting diodes, as well as X-ray and photodetectors.

KeyWords AITranslate

perovskite FETs contact resistance mobility transistors charge injection
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00149

Chinese Library Classification Number:

Citation Information:

Metal halide perovskites are versatile materials which have already demonstrated exceptional performance in diverse optoelectronic devices. The progress has been significant; however, the fundamental understanding of the physics of charge injection remains elusive, impeding further advancements. Here, we use field-effect transistors (FETs) to investigate the impact of surface functionalization on the charge injection and transport in thin films of phenethylammonium tin iodide (PEA2SnI4). We show that self-assembled monolayers (SAMs) can both assist in reducing the Schottky barrier and act as an ion blocking layer between the contact and the perovskite film, limiting interfacial chemical reactions. Consequently, the contact resistance is lowered by more than 3 times compared to untreated contacts. The temperature dependence of the charge carrier mobility is discussed considering the contributions from the channel and contacts, respectively. Our results provide a quantitative framework for the charge injection in metal halide perovskites and will contribute toward the progress of high-performance optoelectronic devices including solar cells, light-emitting diodes, as well as X-ray and photodetectors.

quote

GB/T 7714-2015 [1] Colin Tyznik, Matthew Waldrip, Ryan P. Sullivan, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00149.
MLA [1] Colin Tyznik, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00149.
APA [1] Colin Tyznik, Matthew Waldrip, Ryan P. Sullivan, Motahhare Mirhosseini, Adam Berry, Sean Dwyer, Hurriyet Yuce Cakir, Tonya Coffey, YuehLin Loo, & Oana D. Jurchescu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00149
IEEE [1] Colin Tyznik, Matthew Waldrip, Ryan P. Sullivan, Motahhare Mirhosseini, Adam Berry, Sean Dwyer, Hurriyet Yuce Cakir, Tonya Coffey, YuehLin Loo, and Oana D. Jurchescu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00149. keywords: {perovskite FETs contact resistance mobility transistors charge injection}