Facile Route to Inkjet Printed Carbon Nanotube-Based Inverters with High Gain for Biosignal Monitoring Facile Route to Inkjet Printed Carbon Nanotube-Based Inverters with High Gain for Biosignal Monitoring AITranslate
Abstract AITranslate
Single-walled carbon nanotubes (SWCNTs) have gained much attention as a promising semiconducting nanomaterial in the field of electronic, optical, and photonic applications. In order to implement such applications in the form of wearable devices, inkjet printing technology has shown great promise for cost-effective, large-area device fabrication. In designing electrical circuits, however, dissimilar n-type semiconductors are often required because SWCNTs typically exhibit p-type behavior. This may result in the addition of complex fabrication steps and more areal footprint to match the performance imbalance between two dissimilar semiconductors. Herein, we report a facile route to the fabrication of inkjet-printed p-type SWCNT transistor-based inverters, in which their transistor modes can be simply tuned from enhancement mode to depletion mode by increasing the number of printed SWCNT layers. The threshold voltage shift was systematically obtained by increasing the printing counts of SWCNTs in the channel area. With this transistor-mode-change strategy, a high gain inverter-based amplifier circuit is realized to monitor real-time biosignals, including the chest movement during breathing and muscular movement by a hand gesture.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01603
Chinese Library Classification Number:
Citation Information:
Single-walled carbon nanotubes (SWCNTs) have gained much attention as a promising semiconducting nanomaterial in the field of electronic, optical, and photonic applications. In order to implement such applications in the form of wearable devices, inkjet printing technology has shown great promise for cost-effective, large-area device fabrication. In designing electrical circuits, however, dissimilar n-type semiconductors are often required because SWCNTs typically exhibit p-type behavior. This may result in the addition of complex fabrication steps and more areal footprint to match the performance imbalance between two dissimilar semiconductors. Herein, we report a facile route to the fabrication of inkjet-printed p-type SWCNT transistor-based inverters, in which their transistor modes can be simply tuned from enhancement mode to depletion mode by increasing the number of printed SWCNT layers. The threshold voltage shift was systematically obtained by increasing the printing counts of SWCNTs in the channel area. With this transistor-mode-change strategy, a high gain inverter-based amplifier circuit is realized to monitor real-time biosignals, including the chest movement during breathing and muscular movement by a hand gesture.
quote
| GB/T 7714-2015 | [1] Juhee Park, Hyung Woo Choi, Bongjun Kim. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01603. |
| MLA | [1] Juhee Park, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01603. |
| APA | [1] Juhee Park, Hyung Woo Choi, & Bongjun Kim. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01603 |
| IEEE | [1] Juhee Park, Hyung Woo Choi, and Bongjun Kim, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01603. keywords: {printed electronics inkjet printed circuits pMOS inverter depletionload inverter common source amplifier} |