The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; The University of Southern Mississippi; Oak Ridge National Laboratory; University of Tennessee; The University of Southern Mississippi
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A new pore formation process was investigated for the manufacture of composite ultrafiltration membranes. Phase-separated block copolymer (BCP) thin films supported on a compliant macroporous poly(ether sulfone) (PES) support craze under tensile strain, leaving behind pores of predictable size based on the self-assembled nanoscopic domains. The high aspect ratio pores formed in this process were used to create membranes that were highly permeable (959 L/(m2 h bar) with near complete rejection of 40 nm diameter gold nanoparticles (AuNP). By use of BCP’s inherent ability to cavitate under strain, tedious block removal steps are avoided. Membranes can thus be prepared in a simple, roll-to-roll ready, one-step process. In this initial study, BCP craze formation and filtration performance were characterized for various polymer types, molecular weights, and thicknesses. All these factors influenced the BCP’s thin film morphology, mechanical performance, deformation mechanism, and ultimately filtration performance. This work demonstrates a possible new path toward achieving scalable, BCP-based ultrafiltration membranes.

KeyWords AITranslate

block copolymer membrane thin film craze cavitation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00963

Chinese Library Classification Number:

Citation Information:

A new pore formation process was investigated for the manufacture of composite ultrafiltration membranes. Phase-separated block copolymer (BCP) thin films supported on a compliant macroporous poly(ether sulfone) (PES) support craze under tensile strain, leaving behind pores of predictable size based on the self-assembled nanoscopic domains. The high aspect ratio pores formed in this process were used to create membranes that were highly permeable (959 L/(m2 h bar) with near complete rejection of 40 nm diameter gold nanoparticles (AuNP). By use of BCP’s inherent ability to cavitate under strain, tedious block removal steps are avoided. Membranes can thus be prepared in a simple, roll-to-roll ready, one-step process. In this initial study, BCP craze formation and filtration performance were characterized for various polymer types, molecular weights, and thicknesses. All these factors influenced the BCP’s thin film morphology, mechanical performance, deformation mechanism, and ultimately filtration performance. This work demonstrates a possible new path toward achieving scalable, BCP-based ultrafiltration membranes.

quote

GB/T 7714-2015 [1] Daniel W. Weller, Guorong Ma, Luke A. Galuska, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00963.
MLA [1] Daniel W. Weller, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00963.