Effect of Pulsed Frequency on Microstructure and Microhardness of WC-13Ni Cemented Carbide Irradiated by Intense Pulsed Electron Beam AITranslate

School of Material Science and Engineering,Shaanxi University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of pulsed frequency on microstructure and microhardness of WC-13 Ni cemented carbide irradiated by intense pulsed electron beam(IPEB) was investigated by scanning electron microscope,surface profiler,X-ray diffractometer and Vickers microhardness tester.The results show that at a lower energy density of 3 J/cm^2,the increase of pulse frequency enhances the cumulative effect of thermal shock of IPEB irradiation,resulting in an increase in the number of thermal erosion pits and the content of Ni phase on the surface of the cemented carbide,the surface roughness slowly increasing,and the hardness decreasing at first and then slowly increasing.At a higher energy density of 13 J/cm^2, the increase of pulse frequency enhances the cumulative effect of surface remelting of IPEB irradiation,resulting in an increase in the number and size of ablated holes and the content of WC1-x and W2C phases on the surface of the cemented carbide. At the same time,the surface roughness and microhardness increase at first and then decrease.When the pulse frequency is 1 Hz,the surface microhardness reaches the maximum of 1 380 HV0.2.

KeyWords AITranslate

WC-13Ni cemented carbide intense pulsed electron beam irradiation pulsed frequency microstructure microhardness

1张锋刚.强流脉冲电子束辐照WC-Ni硬质合金表面重熔相变[J].材料热处理学报,2017,38(10):126-132. 被引量:2

2张锋刚,王永善,宋佩维,李文虎.硬质合金表面改性研究现状与展望[J].陕西理工学院学报:自然科学版,2015,31(3):8-13. 被引量:3

1丁紫阳,白玲,晋玉霞,马宗彬.WC添加量对Ni基等离子熔覆层组织与性能的影响[J].稀有金属与硬质合金,2022,50(1):32-36. 被引量:1

1崔陈,朱协彬,程敬卿,刘振华,韩顺顺.等离子熔覆Fe基/WC-10Co-4Cr涂层的组织与性能研究[J].表面技术,2023,52(7):167-176. 被引量:1

1朱威,何代华,刘翔,刘平.脉冲频率及占空比对3D打印Ti6Al4V合金表面生物活性涂层的影响[J].有色金属材料与工程,2019,40(5):14-21.

2杨效田,付小月,段军灵,李文生,王怀志.感应重熔Ni60/铝青铜复合涂层的组织及性能[J].兰州理工大学学报,2019,45(5):12-18. 被引量:2

3魏俊哲,白海强,许云华.原位自生NbC陶瓷增强铁基复合材料研究[J].铸造技术,2019,40(10):1035-1038. 被引量:2

4邱岳贵,朱汝新,陈杰.高能量创伤致长管状骨骨折的手术治疗体会[J].医学信息:医学与计算机应用,2014,0(21):368-368.

5张庭德,邵辉,司宏伟.数字减影血管造影术施术者受照剂量的影响因素[J].辐射防护通讯,2019,39(2):19-22. 被引量:5

6成亦飞,王琳,贺瑞军,王赟.钛合金离子渗氮层的摩擦磨损行为[J].金属热处理,2019,44(10):170-172. 被引量:4

7钱绍祥.Q345D钢表面Fe-Cr-Mo激光熔覆层的组织及摩擦磨损性能[J].金属热处理,2019,44(10):182-186. 被引量:1

8蒋毅,刘美华,高忠峰,国枝正典.内冲液电火花加工弧柱运动的观测研究[J].电加工与模具,2019,0(5):16-19.

9胡树萌.焊缝前端起弧缺陷TIG重熔修复技术的应用[J].企业科技与发展,2019,0(10):79-80.

10李磊,史志铭,魏亮鱼.退火温度对Cu-19Ni合金力学性能及细观损伤演变行为的影响[J].金属热处理,2019,44(10):61-67.

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

The effect of pulsed frequency on microstructure and microhardness of WC-13 Ni cemented carbide irradiated by intense pulsed electron beam(IPEB) was investigated by scanning electron microscope,surface profiler,X-ray diffractometer and Vickers microhardness tester.The results show that at a lower energy density of 3 J/cm^2,the increase of pulse frequency enhances the cumulative effect of thermal shock of IPEB irradiation,resulting in an increase in the number of thermal erosion pits and the content of Ni phase on the surface of the cemented carbide,the surface roughness slowly increasing,and the hardness decreasing at first and then slowly increasing.At a higher energy density of 13 J/cm^2, the increase of pulse frequency enhances the cumulative effect of surface remelting of IPEB irradiation,resulting in an increase in the number and size of ablated holes and the content of WC1-x and W2C phases on the surface of the cemented carbide. At the same time,the surface roughness and microhardness increase at first and then decrease.When the pulse frequency is 1 Hz,the surface microhardness reaches the maximum of 1 380 HV0.2.

quote

GB/T 7714-2015 [1] ZHANG Feng-gang. Effect of Pulsed Frequency on Microstructure and Microhardness of WC-13Ni Cemented Carbide Irradiated by Intense Pulsed Electron Beam[J]. Rare Metals and Cemented Carbides, 2019(5): 74-78.
MLA [1] ZHANG Feng-gang. "Effect of Pulsed Frequency on Microstructure and Microhardness of WC-13Ni Cemented Carbide Irradiated by Intense Pulsed Electron Beam." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 74-78.
APA [1] ZHANG Feng-gang. (2019). Effect of Pulsed Frequency on Microstructure and Microhardness of WC-13Ni Cemented Carbide Irradiated by Intense Pulsed Electron Beam. Rare Metals and Cemented Carbides(5), 74-78.
IEEE [1] ZHANG Feng-gang, "Effect of Pulsed Frequency on Microstructure and Microhardness of WC-13Ni Cemented Carbide Irradiated by Intense Pulsed Electron Beam," Rare Metals and Cemented Carbides, no. 5, pp. 74-78, 2019. keywords: {WC-13Ni cemented carbide;intense pulsed electron beam;irradiation;pulsed frequency;microstructure;microhardness}