Comparison for Vanadium Leaching Behaviors of Three Kinds of Carbonaceous Shale AITranslate

School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology;School of Resources and Environmental Engineering, Wuhan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the influences of direct acid leaching and black roasting-acid leaching on vanadium leaching behaviors of three kinds of carbonaceous shale from Xiushui or Pengzhe in Jiangxi province and Tongshan in Hubei province,respectively. The results show that under the conditions of leaching temperature 95 ℃ ,leaching time 4 h,mass ratio of liquid to solid 1 : 1 ,volume fraction of H2SO4 15% ,mass fraction of CaF2 5 %,the vanadium leaching rates of three kinds of carbonaceous shale treated with direct acid leaching are 92. 39%, 74. 10%and 40. 53%, respectively, while the above leaching rates with black roasting-acid leaching are 85. 53%,90. 78% and 41.59%,respectively. It is found that both the existing forms of vanadium and iron in carbonaceous shale and the contents of acid-consumable minerals have great effects on vanadium leaching. By blank roasting, vanadium in organics can be transformed into free and soluble vanadium oxide, and mica-contained vanadium can be disintegrated to accelerate vanadium leaching. However,the acid-nonconsumable mineral of pyrite could be transformed into the acid-consumable mineral of hematite to hinder vanadium leaching. It is reasonable for the three kinds of carbonaceous shale in which vanadium exists mainly in the form of aluminosilicate including mica to adopt correspondingly different vanadium leaching processes. Direct acid leaching process is suitable for carbonaceous shale from Xiushui inJiangxi Province,blank roasting-acid leaching process is suitable for carbonaceous shale from Pengzhe in Jiangxi Province,and another vanadium extracting process should be adopted for carbonaceous shale from Tongshan in Hubei Province.

KeyWords AITranslate

carbonaceous shale vanadium direct acid leaching black roasting-acid leaching ROM characteristic existing form

1Wang Fei, Zhang Yi-min, I.iu Tao, et al. Comparison of direct acid leaching process and blank roasting acid leac- hing process in extracting vanadium from stone coal[J]. International Journal of Mineral Processing, 2014, 128: 40-47.

2宾智勇.石煤提钒研究进展与五氧化二钒的市场状况[J].湖南有色金属,2006,22(1):16-20. 被引量:126

3Zhang Yi-min,Bao Shen-xu,Liu Tao,et al. The technol- ogy of extracting vanadium from stone coal in China= history,current status and fulure prospects[J]. Hydro-metallurgy,2011,109(1-2) : 116-124.

4孙伟,王丽,曹学锋,刘润清,徐龙华,韩海生.石煤提钒的浮选工艺及吸附机理[J].中国有色金属学报,2012,22(7):2069-2074. 被引量:34

5常娜,顾兆林,李云.石煤提钒浸出工艺研究[J].无机盐工业,2006,38(7):57-59. 被引量:21

6梁建龙,刘惠娟,史文革,胡鄂明,李熙琪,彭军.湿法冶金提钒浸出新工艺[J].中国矿业,2006,15(7):64-66. 被引量:18

7He D S,Feng Q M,Zhang G F,et al. Study on leaching vanadium from roasting residue of stone coal[J].Miner als and Metallurgical Processing, 2008,25 ( 4 ) : 181-184.

8冯其明,何东升,张国范,欧乐明,卢毅屏.石煤提钒过程中钒氧化和转化对钒浸出的影响[J].中国有色金属学报,2007,17(8):1348-1352. 被引量:85

9居中军,王成彦,尹飞,杨永强,李敦钫.石煤钒矿硫酸活化常压浸出提钒工艺[J].中国有色金属学报,2012,22(7):2061-2068. 被引量:17

10Fei Wang,Yi-Min Zhang,Jing Huang,Tao Liu,Yi Wang,Xiao Yang,Jie Zhao.Mechanisms of aid-leaching reagent calcium fluoride in the extracting vanadium processes from stone coal[J].稀有金属:英文版,2013(1):57-62. 被引量:22

1韩峰,周志强,王疆,杨铖.从石煤钒矿直接酸浸液中提取钒的研究[J].稀有金属与硬质合金,2017,45(3):5-9. 被引量:5

1邹建新.钒渣浸出过程的热力学和动力学研究现状[J].无机盐工业,2018,50(12):5-8.

2吕浩,成宝海,刘芳,包贤慧.P204体系从含钒硫酸浸出液中提取五氧化二钒的清洁工艺研究[J].长春师范大学学报,2020,39(2):194-196.

3刘宏伟,许小弟,祝敏毅,韩恩厚,祝溪桥.钒矿提制高纯钒系产品及清洁生产技术[J].辽宁化工,2020,49(12):1510-1513.

4程倩,王明,宁新霞,李洁,曹欢,郭金玉.从某低品位炭质钒矿石中酸浸-萃取-氨沉淀提钒实验研究[J].矿产综合利用,2021(3):17-21. 被引量:6

5王阳,郭万进,隆长命.某难选钒矿提取钒实验研究[J].矿产综合利用,2022(5):141-147.

1李庚进.氧化锰矿直接浸出工艺的应用[J].中国锰业,1989(5):35-38. 被引量:7

2鲁兆伶,谷万成.从石煤中提取钒的焙烧试验研究[J].湿法冶金,2009,28(2):88-91. 被引量:7

3吕宁宁,于景坤,苏畅,王洪章.LF精炼废渣中硫赋存形式的研究[J].东北大学学报:自然科学版,2013,34(9):1261-1264. 被引量:3

4梁泰然,谭立新.复合型助浸剂对钒浸出率的影响[J].材料研究与应用,2016,10(4):255-257. 被引量:5

5Hans.,DT,吕兴华.从含钡矿物中回收钒的方法[J].钒钛,1989(3):1-8.

6张斌,陈启元,姜涛,杨永斌.锰银矿同步浸出锰、银新工艺试验研究[J].黄金,2001,22(7):26-29. 被引量:10

7杨华明,胡岳华,杨武国,邱冠周.复杂铝硅酸盐矿物热处理过程的结构变化[J].金属矿山,2003(8):25-27. 被引量:2

8汤艳杰,刘建朝,贾建业.豫西铝土矿中镓的赋存状态研究[J].西安工程学院学报,2002,24(4):1-5. 被引量:17

9吕宪俊,邱俊,陈平,胡术刚.新疆某低品位铁矿石工艺矿物学研究[J].金属矿山,2009(6):99-101. 被引量:6

10冯其明,何东升,张国范,欧乐明,卢毅屏.石煤提钒过程中钒氧化和转化对钒浸出的影响[J].中国有色金属学报,2007,17(8):1348-1352. 被引量:85

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

Study is made on the influences of direct acid leaching and black roasting-acid leaching on vanadium leaching behaviors of three kinds of carbonaceous shale from Xiushui or Pengzhe in Jiangxi province and Tongshan in Hubei province,respectively. The results show that under the conditions of leaching temperature 95 ℃ ,leaching time 4 h,mass ratio of liquid to solid 1 : 1 ,volume fraction of H2SO4 15% ,mass fraction of CaF2 5 %,the vanadium leaching rates of three kinds of carbonaceous shale treated with direct acid leaching are 92. 39%, 74. 10%and 40. 53%, respectively, while the above leaching rates with black roasting-acid leaching are 85. 53%,90. 78% and 41.59%,respectively. It is found that both the existing forms of vanadium and iron in carbonaceous shale and the contents of acid-consumable minerals have great effects on vanadium leaching. By blank roasting, vanadium in organics can be transformed into free and soluble vanadium oxide, and mica-contained vanadium can be disintegrated to accelerate vanadium leaching. However,the acid-nonconsumable mineral of pyrite could be transformed into the acid-consumable mineral of hematite to hinder vanadium leaching. It is reasonable for the three kinds of carbonaceous shale in which vanadium exists mainly in the form of aluminosilicate including mica to adopt correspondingly different vanadium leaching processes. Direct acid leaching process is suitable for carbonaceous shale from Xiushui inJiangxi Province,blank roasting-acid leaching process is suitable for carbonaceous shale from Pengzhe in Jiangxi Province,and another vanadium extracting process should be adopted for carbonaceous shale from Tongshan in Hubei Province.

quote

GB/T 7714-2015 [1] WANG Fei, ZHANG Yi-min, LIU Tao, et al. Comparison for Vanadium Leaching Behaviors of Three Kinds of Carbonaceous Shale[J]. Rare Metals and Cemented Carbides, 2014(4): 1-6.
MLA [1] WANG Fei, et al., "Comparison for Vanadium Leaching Behaviors of Three Kinds of Carbonaceous Shale." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 1-6.
APA [1] WANG Fei, ZHANG Yi-min, LIU Tao, HUANG Jing, HUANG Xian-bao, XUE Nan-nan, & YUAN Yi-zhong. (2014). Comparison for Vanadium Leaching Behaviors of Three Kinds of Carbonaceous Shale. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] WANG Fei, ZHANG Yi-min, LIU Tao, HUANG Jing, HUANG Xian-bao, XUE Nan-nan, and YUAN Yi-zhong, "Comparison for Vanadium Leaching Behaviors of Three Kinds of Carbonaceous Shale," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 2014. keywords: {carbonaceous shale;vanadium;direct acid leaching;black roasting-acid leaching;ROM characteristic;existing form}