daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhancing the Stability of Stretchable Buckling Electrodes by Incorporating a Sulfhydryl-Anchored Interface with Disordered Pores for Deformable Electronics Enhancing the Stability of Stretchable Buckling Electrodes by Incorporating a Sulfhydryl-Anchored Interface with Disordered Pores for Deformable Electronics AITranslate

Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech); Nanjing Tech University (Nanjing Tech)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Stretchable electrodes have received rising attention due to their potential applications in flexible and wearable devices. However, the mechanical instability of stretchable electrodes limits their practical applications. Here, we demonstrate an efficient approach to enhancing the stability of stretchable serpentine-shaped electrodes by incorporating a sulfhydryl-anchored interface with disordered cones. The sulfhydryl-anchored interface provides strong adhesion (2.3 MPa) between the gold electrode and polymer substrate, while the disordered cones allow for deformation of the electrode with less cracks or fractures. By using this synergistic strategy, the electrode exhibits a large tensile limit exceeding 50% uniaxial tensile and superior electrical stability from 6.3 to 11.5 Ω under 20% uniaxial tensile for more than 200 cycles. Our approach has the potential for foldable electronics and health monitoring.

KeyWords AITranslate

interfacial engineering disordered nanopores flexible electrode stretchability adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00801

Chinese Library Classification Number:

Citation Information:

Stretchable electrodes have received rising attention due to their potential applications in flexible and wearable devices. However, the mechanical instability of stretchable electrodes limits their practical applications. Here, we demonstrate an efficient approach to enhancing the stability of stretchable serpentine-shaped electrodes by incorporating a sulfhydryl-anchored interface with disordered cones. The sulfhydryl-anchored interface provides strong adhesion (2.3 MPa) between the gold electrode and polymer substrate, while the disordered cones allow for deformation of the electrode with less cracks or fractures. By using this synergistic strategy, the electrode exhibits a large tensile limit exceeding 50% uniaxial tensile and superior electrical stability from 6.3 to 11.5 Ω under 20% uniaxial tensile for more than 200 cycles. Our approach has the potential for foldable electronics and health monitoring.

quote

GB/T 7714-2015 [1] Xuemei Dong, Yijie Nie, Hongchao Sun, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00801.
MLA [1] Xuemei Dong, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00801.
APA [1] Xuemei Dong, Yijie Nie, Hongchao Sun, Xinkai Qian, Min Xu, Zicheng Zhang, Bin Liu, Zixi He, Yinxiang Li, Chunyang Miao, & Juqing Liu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00801
IEEE [1] Xuemei Dong, Yijie Nie, Hongchao Sun, Xinkai Qian, Min Xu, Zicheng Zhang, Bin Liu, Zixi He, Yinxiang Li, Chunyang Miao, and Juqing Liu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00801. keywords: {interfacial engineering disordered nanopores flexible electrode stretchability adhesion}