Ni-Doped Cobalt–Cobalt Nitride Heterostructure Arrays for High-Power Supercapacitors AITranslate

National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore; National University of Singapore
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal nitrides are widely recognized as a class of desirable supercapacitor electrode materials owing to their high electrical conductivity and structural stability. Embedding metal nanoparticles in nitrides can further enhance the conductivity for electron transport. Herein, a heterostructure consisting of Ni-doped Co–Co2N is synthesized by simple thermal annealing of metal–organic framework (MOF)-derived NiCo2O4 in ammonia atmosphere, in the process of which the MOF-derived two-dimensional (2D) nanoflake arrays were well retained, and the metal–metal nitride heterostructure was well established when annealed at 350 °C. Benefiting from the MOF-derived 2D nanoflake morphology and the metal-metal nitride heterostructure, the Ni-doped Co–Co2N delivers a specific capacity of 361.93 C/g. A full cell test has been conducted using Ni-doped Co–Co2N as the positive electrode and porous carbon as the negative electrode, and it shows an energy density of 20.4 Wh/kg at the power density of 9.85 kW/kg with 82.4% of initial energy density being retained after 5000 cycles.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01393

Chinese Library Classification Number:

Citation Information:

Metal nitrides are widely recognized as a class of desirable supercapacitor electrode materials owing to their high electrical conductivity and structural stability. Embedding metal nanoparticles in nitrides can further enhance the conductivity for electron transport. Herein, a heterostructure consisting of Ni-doped Co–Co2N is synthesized by simple thermal annealing of metal–organic framework (MOF)-derived NiCo2O4 in ammonia atmosphere, in the process of which the MOF-derived two-dimensional (2D) nanoflake arrays were well retained, and the metal–metal nitride heterostructure was well established when annealed at 350 °C. Benefiting from the MOF-derived 2D nanoflake morphology and the metal-metal nitride heterostructure, the Ni-doped Co–Co2N delivers a specific capacity of 361.93 C/g. A full cell test has been conducted using Ni-doped Co–Co2N as the positive electrode and porous carbon as the negative electrode, and it shows an energy density of 20.4 Wh/kg at the power density of 9.85 kW/kg with 82.4% of initial energy density being retained after 5000 cycles.

quote

GB/T 7714-2015 [1] Ximeng Liu, Wenjie Zang, Cao Guan, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01393.
MLA [1] Ximeng Liu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01393.
APA [1] Ximeng Liu, Wenjie Zang, Cao Guan, Lei Zhang, Yuhong Qian, Abdelnaby M. Elshahawy, Dan Zhao, Stephen J. Pennycook, & John Wang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01393
IEEE [1] Ximeng Liu, Wenjie Zang, Cao Guan, Lei Zhang, Yuhong Qian, Abdelnaby M. Elshahawy, Dan Zhao, Stephen J. Pennycook, and John Wang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01393.