Improved Dielectric Permittivity and Energy Density of Layered Polymer Composites through the Incorporation of Ultralow Amounts of RGO@BTO Hybrid Nanosheets Improved Dielectric Permittivity and Energy Density of Layered Polymer Composites through the Incorporation of Ultralow Amounts of RGO@BTO Hybrid Nanosheets AITranslate
Abstract AITranslate
Polymer dielectric composites are extensively used in modern electronic devices because of their extremely high power density. However, unfavorable coupling between breakdown strength and dielectric permittivity can make achieving high energy density a challenge. In this study, reduced graphene oxide @ barium titanate (RGO@BTO) hybrid nanosheets have been fabricated and utilized as fillers in the design of RGO@BTO/P(VDF-HFP) single-layer films. An increase in permittivity to 24.8@10 kHz, i.e., equivalent to 253% of the P(VDF-HFP) (∼9.8@10 kHz) matrix, has been achieved with only 1 wt % RGO@BTO nanofillers due to the formation of microcapacitors. Furthermore, the RGO@BTO/P(VDF-HFP) film is hot-pressed with a PEI film and a P(VDF-HFP) film, forming a trilayer structure. Consequently, this trilayer film displays a high breakdown strength of 478 kV/mm, a high energy density of 8.25 J/cm3, and a satisfactory efficiency of 64.3%. Thus, this study provides an efficient route for designing polymer composites that combine high energy density with high permittivity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00636
Chinese Library Classification Number:
Citation Information:
Polymer dielectric composites are extensively used in modern electronic devices because of their extremely high power density. However, unfavorable coupling between breakdown strength and dielectric permittivity can make achieving high energy density a challenge. In this study, reduced graphene oxide @ barium titanate (RGO@BTO) hybrid nanosheets have been fabricated and utilized as fillers in the design of RGO@BTO/P(VDF-HFP) single-layer films. An increase in permittivity to 24.8@10 kHz, i.e., equivalent to 253% of the P(VDF-HFP) (∼9.8@10 kHz) matrix, has been achieved with only 1 wt % RGO@BTO nanofillers due to the formation of microcapacitors. Furthermore, the RGO@BTO/P(VDF-HFP) film is hot-pressed with a PEI film and a P(VDF-HFP) film, forming a trilayer structure. Consequently, this trilayer film displays a high breakdown strength of 478 kV/mm, a high energy density of 8.25 J/cm3, and a satisfactory efficiency of 64.3%. Thus, this study provides an efficient route for designing polymer composites that combine high energy density with high permittivity.
quote
| GB/T 7714-2015 | [1] Shuimiao Xia, Kuan Chen, Kelan Yan, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00636. |
| MLA | [1] Shuimiao Xia, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00636. |
| APA | [1] Shuimiao Xia, Kuan Chen, Kelan Yan, Liming Shen, Meiyu Zhang, Zhicheng Shi, & Runhua Fan. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00636 |
| IEEE | [1] Shuimiao Xia, Kuan Chen, Kelan Yan, Liming Shen, Meiyu Zhang, Zhicheng Shi, and Runhua Fan, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00636. keywords: {dielectric composite electrostatic capacitor graphene oxide multilayer structure nanosheets} |