Fully Biobased Elastomer Composites with Mechanically Robust, Reprocessable, and Biocompatible Properties AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; University of Massachusetts at Amherst
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

It is of importance, though difficult, to integrate reinforcement, functionalization, and recyclability into elastomeric materials. Here we describe a biomass-derived epoxidized natural rubber (ENR) cross-linked with dynamic covalent bonds and reinforced with functional carboxymethyl chitosan (CMCS). The ENR/CMCS composites show enhanced mechanical properties and thermal stability, due to the uniform dispersion of the CMCS fillers and strong interfacial interaction between the ENR matrix and fillers. These cross-linked rubbers can undergo topological network rearrangements through dynamic exchange reactions, endowing the materials with reprocessability and recyclability. Due to the biologically derived and green features of the both polymeric matrix and filler, the fully biobased ENR/CMCS composites also show excellent biocompatibility, which will expand their application in the field of biomaterials.

KeyWords AITranslate

epoxidized natural rubber carboxymethyl chitosan dynamic exchange reaction recyclability biocompatibility
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01179

Chinese Library Classification Number:

Citation Information:

It is of importance, though difficult, to integrate reinforcement, functionalization, and recyclability into elastomeric materials. Here we describe a biomass-derived epoxidized natural rubber (ENR) cross-linked with dynamic covalent bonds and reinforced with functional carboxymethyl chitosan (CMCS). The ENR/CMCS composites show enhanced mechanical properties and thermal stability, due to the uniform dispersion of the CMCS fillers and strong interfacial interaction between the ENR matrix and fillers. These cross-linked rubbers can undergo topological network rearrangements through dynamic exchange reactions, endowing the materials with reprocessability and recyclability. Due to the biologically derived and green features of the both polymeric matrix and filler, the fully biobased ENR/CMCS composites also show excellent biocompatibility, which will expand their application in the field of biomaterials.

quote

GB/T 7714-2015 [1] Shizhen Zhao, Hongkun Yang, Genlai Dong, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01179.
MLA [1] Shizhen Zhao, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01179.
APA [1] Shizhen Zhao, Hongkun Yang, Genlai Dong, Dong Wang, & Thomas P. Russell. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01179
IEEE [1] Shizhen Zhao, Hongkun Yang, Genlai Dong, Dong Wang, and Thomas P. Russell, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01179. keywords: {epoxidized natural rubber;carboxymethyl chitosan;dynamic exchange reaction;recyclability;biocompatibility}