Research Progress of Preparation of Cemented Carbides with WC-Co Composite Powders Prepared by Spray Conversion AITranslate
Abstract AITranslate
Research progress at home and abroad is reviewed of preparation of WC-Co composite powders by spray conversion and cemented carbides with tungsten-cobalt base or tungsten-cobalt-carbon base. The routes,methods and process parameters are mainly discussed for preparing WC-Co composite powders and cemented carbides as well as the alloy properties,to provide research ideas and methods for preparation of cemented carbides with WC-Co composite powders prepared by spray conversion. WC-Co composite pow ders with short process flow, uniform component distribution, low impurity content, narrow particle size distribution,small grain size and low cost can be obtained by continuous optimization and improvement of preparation processes and methods.
KeyWords AITranslate
1朱二涛,羊建高,郭圣达,邓军旺,谭兴龙,吕健.直接碳化与煅烧-碳化工艺对WC-Co复合粉性能的影响[J].硬质合金,2014,31(2):77-85. 被引量:3
2覃群,王天国,张云宋.超细WC-Co硬质合金复合粉末的研究进展[J].硬质合金,2010,27(5):311-315. 被引量:13
3吴鹏,温德才,刘少存,谢桂香,杨守达,兰永祥.烧结温度对纳米WC-6Co复合粉烧结的影响[J].宁德师范学院学报:自然科学版,2016,28(1):45-49. 被引量:1
4郭圣达,鲍瑞,刘亮,杨平,易健宏,羊建高,陈颢.原位合成复合粉制备超细WC-Co硬质合金[J].稀有金属材料与工程,2017,46(12):3977-3982. 被引量:7
5史晓亮,杨华,邵刚勤,段兴龙,熊震,易忠来.微波烧结法制备WC-10Co硬质合金[J].中南大学学报:自然科学版,2006,37(4):665-669. 被引量:18
6杨守达,张寿德,陈先强.WC/Co复合粉制备超细晶挤压圆棒工艺之研究[J].中国钨业,2013,28(6):42-44. 被引量:2
7文彦,张钦英,郭圣达,苏伟,黄柱,陈颢.WC-6Co硬质合金SPS烧结工艺[J].有色金属科学与工程,2017,8(3):74-78. 被引量:11
8欧阳亚非.合成超细碳化钨钴复合粉末的一种新方法[J].硬质合金,1998,15(3):145-149. 被引量:9
9刘艳军,陈康华,李詠侠,吴恩熙,邹丹,谢元彦.硬质合金中碳含量对晶粒生长抑制剂抑制效果的影响[J].稀有金属与硬质合金,2017,45(3):65-70. 被引量:4
10欧阳亚非,邬荫芳,彭泽辉.WC-Co复合粉末的流态化合成及其应用[J].中国钨业,1999,14(5):210-215. 被引量:17
1张璐,李剑峰,尹运春,刘渊溢,陆必志.WC粉末特性对超细晶硬质合金烧结敏感性影响的研究[J].硬质合金,2020,37(1):51-59. 被引量:8
2曾瑞霖,李剑峰,马赛,龙宁华,张湘,吴育藩.WC粉末特性对PCB用超细晶硬质合金棒材微观组织结构和性能的影响[J].硬质合金,2022,39(6):454-460.
1张圆圆,王云鲲,黄伟,钟铭锋.等离子喷涂氧化锆涂层在硬质合金烧结舟皿上的应用[J].世界有色金属,2020(15):173-174. 被引量:2
2付胜,张立,陈焕涛,戴湘平.亚微和超细碳化钨粉末的质量缺陷与粒度表征[J].中国钨业,2020,35(6):1-7. 被引量:3
3冯志,程登峰,黎明华,刘娜娜,朱福明.碳化配碳量对粗颗粒WC粉末形貌及WC-8%Co合金性能的影响[J].硬质合金,2021,38(3):171-178.
4贡泽斌,许祥平,何力,邹家生.WC-10Ni/NiCrBSi复合涂层剪切强度及数学模型建立[J].江苏科技大学学报:自然科学版,2021,35(5):26-31. 被引量:1
5邝宏有,戴炳蔚,吴育藩.WC-11%(Ti,W)(Ta,Nb)C-11%Co合金制取过程中碳量和球磨时间的优化[J].硬质合金,2022,39(2):111-117.
6罗鑫,洪源昆,吴佳逸,李绍轩,羊求民.超细硬质合金WC晶粒大小对其摩擦磨损性能的影响[J].稀有金属与硬质合金,2022,50(3):93-97.
7曾瑞霖,李剑峰,马赛,龙宁华,张湘,吴育藩.WC粉末特性对PCB用超细晶硬质合金棒材微观组织结构和性能的影响[J].硬质合金,2022,39(6):454-460.
8何继坤,马赛,曾惠钦,陆必志.碳化工艺对细晶碳化钨粉末特性与硬质合金晶粒异常长大的影响[J].硬质合金,2023,40(4):279-287.
1姬寿长,李争显,李京龙,畅晨阳.钛表面厚碳化钨涂层研究进展[J].钛工业进展,2018,35(6):20-25. 被引量:4
2卜颖宏.高熵合金制备及其性能研究进展[J].信息记录材料,2019,20(5):2-3. 被引量:3
3王亮,郭涛,邹声文,付锦锋,杨霄云,叶南飚.透明PMMA/SMA合金制备及其性能研究[J].塑料工业,2019,47(4):43-46. 被引量:2
4文泽芳.建筑工程施工项目安全风险管理[J].建筑发展,2019,3(5):1-2.
5高文理,王帅,朱聪聪,毛郭灵,王璀.不同Cd含量对Al-Cu合金组织与性能的影响[J].湖南大学学报:自然科学版,2019,46(6):11-17. 被引量:1
6罗含,孙祝林,彭密雪,吕永根.改进水性中间相沥青的制备[J].合成纤维,2019,48(5):29-34. 被引量:1
7匡宏,索晔.高纯水配置策略探究[J].机电信息,2019(14):55-57.
8陈君,张清.添加稀土Gd对Mg-6Al镁合金组织和耐蚀性的影响[J].材料保护,2019,52(3):35-39. 被引量:3
9李振升.新工法在傣族干栏式民居建筑中的利用[J].三明学院学报,2019,36(3):84-89. 被引量:2
10林国标,赵攀,敖伟.回火温度对中碳合金钢4Cr5MoSiV1Nb组织和性能的影响[J].钢铁,2019,54(5):73-77. 被引量:8
Basic Information:
DOI:
Chinese Library Classification Number:TF124[冶金工程—粉末冶金]
Citation Information:
Research progress at home and abroad is reviewed of preparation of WC-Co composite powders by spray conversion and cemented carbides with tungsten-cobalt base or tungsten-cobalt-carbon base. The routes,methods and process parameters are mainly discussed for preparing WC-Co composite powders and cemented carbides as well as the alloy properties,to provide research ideas and methods for preparation of cemented carbides with WC-Co composite powders prepared by spray conversion. WC-Co composite pow ders with short process flow, uniform component distribution, low impurity content, narrow particle size distribution,small grain size and low cost can be obtained by continuous optimization and improvement of preparation processes and methods.
quote
| GB/T 7714-2015 | [1] ZHU Er-tao, ZHANG Jiu-xing, YANG Jian-gao. Research Progress of Preparation of Cemented Carbides with WC-Co Composite Powders Prepared by Spray Conversion[J]. Rare Metals and Cemented Carbides, 2019(3): 70-78. |
| MLA | [1] ZHU Er-tao, et al., "Research Progress of Preparation of Cemented Carbides with WC-Co Composite Powders Prepared by Spray Conversion." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 70-78. |
| APA | [1] ZHU Er-tao, ZHANG Jiu-xing, & YANG Jian-gao. (2019). Research Progress of Preparation of Cemented Carbides with WC-Co Composite Powders Prepared by Spray Conversion. Rare Metals and Cemented Carbides(3), 70-78. |
| IEEE | [1] ZHU Er-tao, ZHANG Jiu-xing, and YANG Jian-gao, "Research Progress of Preparation of Cemented Carbides with WC-Co Composite Powders Prepared by Spray Conversion," Rare Metals and Cemented Carbides, no. 3, pp. 70-78, 2019. keywords: {WC-Co composite powder;cemented carbide;spray conversion;preparation method;perform ance;research progress} |