Abstract AITranslate

Vitrimers are a class of cross-linked polymers with the potential of reprocessing/reshaping, repairing, and recycling. In this paper, carbon nanotubes were either dispersed in the epoxy matrix or used as functional coatings for the development of vitrimer-based polymer systems with short stress relaxation times, relatively high electrical conductivities, and possibility of reshaping using electro-triggering. By selecting the location where the electrical voltage was applied, it was possible to control through electrical resistance heating the activation of the dynamic bonds of the vitrimer matrix, enabling the reconfiguration of the material. It is worth noting that this strategy will pave way for the manufacture of thermosetting polymers with both reconfigurability and functional properties.

KeyWords AITranslate

vitrimer composites aromatic disulfide bonds CNTs stress relaxation electrical activation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01412

Chinese Library Classification Number:

Citation Information:

Vitrimers are a class of cross-linked polymers with the potential of reprocessing/reshaping, repairing, and recycling. In this paper, carbon nanotubes were either dispersed in the epoxy matrix or used as functional coatings for the development of vitrimer-based polymer systems with short stress relaxation times, relatively high electrical conductivities, and possibility of reshaping using electro-triggering. By selecting the location where the electrical voltage was applied, it was possible to control through electrical resistance heating the activation of the dynamic bonds of the vitrimer matrix, enabling the reconfiguration of the material. It is worth noting that this strategy will pave way for the manufacture of thermosetting polymers with both reconfigurability and functional properties.

quote

GB/T 7714-2015 [1] Evanthia Tzouma, Alkiviadis S. Paipetis, NektariaMarianthi Barkoula. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01412.
MLA [1] Evanthia Tzouma, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01412.
APA [1] Evanthia Tzouma, Alkiviadis S. Paipetis, & NektariaMarianthi Barkoula. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01412
IEEE [1] Evanthia Tzouma, Alkiviadis S. Paipetis, and NektariaMarianthi Barkoula, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01412. keywords: {vitrimer composites;aromatic disulfide bonds;CNTs;stress relaxation;electrical activation}