daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Pyridine-Dicarbohydrazone-Based Polyacrylate Hydrogels with Strong Mechanical Property, Tunable/Force-Induced Fluorescence, and Thermal/pH Stimuli Responsiveness AITranslate

South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The smart fluorescent hydrogels exhibiting tunable fluorescence have been used as biosensors, probes, light-emitting devices, and information storage and confidentiality. However, they usually show single stimuli responsiveness and possess weak mechanical properties, which limit their applications. Herein, we report a pyridine-dicarbohydrazone-based polyacrylate hydrogel (the As-prepared hydrogel and Eu-hydrogel) showing strong mechanical property, tunable fluorescence ability, and thermal and pH stimuli responsiveness. The As-prepared hydrogel is prepared by light-induced micellar copolymerization, and Eu-hydrogel is obtained after the formation of Eu3+-(pyridine-dicarbohydrazone) coordination. The As-prepared hydrogel could be made in large size (side length of 15 cm), exhibiting a tensile strength of 1.55 MPa and a fracture tensile strain of 800%. The fluorescence intensity of Eu-hydrogel is tunable by [Eu3+] (approaching 655% of the minimum state at [Eu3+] = 0.1 mol). It is demonstrated that Eu-hydrogels display force-induced fluorochromic response during stretching. The transmittance temperature of the As-prepared hydrogel ranges from 36 to 42 °C. Reversible Eu3+-(pyridine-dicarbohydrazone) coordination enables Eu-hydrogels to have excellent fatigue resistance. The pH stimuli responsiveness of the As-prepared hydrogel and Eu-hydrogel is triggered by switchable covalent hydrozone bonds. In terms of the shape-memory ability, the As-prepared hydrogel could be reconstructed by Eu3+ and Eu-hydrogel could be deformed by H+. This mechanically strong (pyridine-dicarbohydrazone)-based polyacrylate hydrogel with multistimuli responsive behaviors is promising to be used in information transmission, smart windows, load-bearing devices, energy-absorbing materials, and soft wearable devices.

KeyWords AITranslate

polyacrylate hydrogel strong mechanical property stimuli responsiveness dicarbohydrazone tunable fluorescence
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00541

Chinese Library Classification Number:

Citation Information:

The smart fluorescent hydrogels exhibiting tunable fluorescence have been used as biosensors, probes, light-emitting devices, and information storage and confidentiality. However, they usually show single stimuli responsiveness and possess weak mechanical properties, which limit their applications. Herein, we report a pyridine-dicarbohydrazone-based polyacrylate hydrogel (the As-prepared hydrogel and Eu-hydrogel) showing strong mechanical property, tunable fluorescence ability, and thermal and pH stimuli responsiveness. The As-prepared hydrogel is prepared by light-induced micellar copolymerization, and Eu-hydrogel is obtained after the formation of Eu3+-(pyridine-dicarbohydrazone) coordination. The As-prepared hydrogel could be made in large size (side length of 15 cm), exhibiting a tensile strength of 1.55 MPa and a fracture tensile strain of 800%. The fluorescence intensity of Eu-hydrogel is tunable by [Eu3+] (approaching 655% of the minimum state at [Eu3+] = 0.1 mol). It is demonstrated that Eu-hydrogels display force-induced fluorochromic response during stretching. The transmittance temperature of the As-prepared hydrogel ranges from 36 to 42 °C. Reversible Eu3+-(pyridine-dicarbohydrazone) coordination enables Eu-hydrogels to have excellent fatigue resistance. The pH stimuli responsiveness of the As-prepared hydrogel and Eu-hydrogel is triggered by switchable covalent hydrozone bonds. In terms of the shape-memory ability, the As-prepared hydrogel could be reconstructed by Eu3+ and Eu-hydrogel could be deformed by H+. This mechanically strong (pyridine-dicarbohydrazone)-based polyacrylate hydrogel with multistimuli responsive behaviors is promising to be used in information transmission, smart windows, load-bearing devices, energy-absorbing materials, and soft wearable devices.

quote

GB/T 7714-2015 [1] Ye Yuan, He Zhang, Jinqing Qu. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00541.
MLA [1] Ye Yuan, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00541.
APA [1] Ye Yuan, He Zhang, & Jinqing Qu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00541
IEEE [1] Ye Yuan, He Zhang, and Jinqing Qu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00541. keywords: {polyacrylate hydrogel;strong mechanical property;stimuli responsiveness;dicarbohydrazone;tunable fluorescence}