Research on the Photocatalytic Degradation of Gentian Violet with Strontium Germinate Crystal Nanowires AITranslate

School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology;School of Materials Science and Engineering, Anhui University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The strontium germinate crystal nanowires were prepared by hydrothermal method, and their photocatalytic performance for degrading gentian violet was investigated. The results show that the degradation rate of gentian violet increases by prolonging the photocatalysis time and increasing the dosage of strontium germinate crystal nanowires, but gradually decreases with the increase of initial concentration of gentian violet solution. Under the conditions of photocatalysis time of 4 h, strontium germinate nanowires dosage of 10 mg and initial concentration of gentian violet solution of 10 mg/L,the optimal photocatalytic effect of the strontium germinate nanowires for degrading gentian violet can be obtained, with a degrada- tion rate of 89. 59%.

KeyWords AITranslate

SrGeO3 crystal nanowire gentian violet degradation photocatalysis hydrothermal method

1Matthews R W. Photo-oxidation of organic material in a queous suspensions of titanium dioxide[J]. Water Res, 1986,20(5) :569-578.

2万益群,钟己未,郭岚,付敏恭.网络状纳米氧化锌光催化降解水中有机染料的研究[J].分析科学学报,2007,23(1):48-50. 被引量:14

3许平昌,柳阳,魏建红,熊锐,潘春旭,石兢.溶剂热法制备Ag/TiO_2纳米材料及其光催化性能[J].物理化学学报,2010,26(8):2261-2266. 被引量:44

4Puangpetch T, Sommarkettarin P, Chavadej S, et al. Hydrogen production from water splitting over eosin Y- sensitized mesoporous- assembled perovskite titanate nanocrystal photocatalysts under visible light irradiation [J].Int J Hydrogen Energy, 2010, 35 ( 22 ) : 12 428 - 12 442.

5Miseki Y, Kato H,Kudo A. Water splitting into H2 and O2 over niobate and titanate photocatalysts with (111) [J]. Energy Environ Sci,2009,2:306-314.

6Konta R, Kato H, Kobayashi H, et al. Photophysical properties and photocatalytic activities under visible light irradiation of silver vanadates [J].Phys Chem Chem Phys,2003,5:3 061-3 065.

7Huang J H,Wang X C, Hou Y D,et al. Degradation of benzene over a zinc germanate photocatalyst under ambi- ent conditions[J]. Environ Sci Technol,2008, 42.. 7 387 -7 391.

8Tsai M Y,Yu C Y,Perng T P. Synthesis and photolumi nescence of amorphous strontium germanate nanowires [J]. J Nanosci Nanotechnol,2008,12(8) : 12-17.

9蒋宇翔,李洋,田浪,金海波,杨基磊,王帅,裴立宅.生长条件对锗酸锶纳米线形成的影响[J].铜业工程,2013(3):17-20. 被引量:2

10Mohamed R M, Ismail A A, Othman I, et al. Prepa ration of TiO2-ZSM-5 zeolite for photodegradation of EDTA[J]. J Mol Catal A,2005,288:151-157.

1廖颖敏,李晓慧,蔡婷,张清.改性榴莲壳对结晶紫的吸附性能研究[J].化工新型材料,2019,47(8):228-232. 被引量:1

1窦诗童,廖颖敏,余婷,甘蕊,刘小筱.改性榴莲壳对水中亚甲基蓝的吸附研究[J].化工技术与开发,2020,49(10):64-68. 被引量:2

1陈纯馨,陈忻,刘爱文,林耿标.硼酸类复配物的固相制备及其热变色性能研究[J].化工新型材料,2006,34(2):46-48. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TQ132.33[化学工程—无机化工]

Citation Information:

The strontium germinate crystal nanowires were prepared by hydrothermal method, and their photocatalytic performance for degrading gentian violet was investigated. The results show that the degradation rate of gentian violet increases by prolonging the photocatalysis time and increasing the dosage of strontium germinate crystal nanowires, but gradually decreases with the increase of initial concentration of gentian violet solution. Under the conditions of photocatalysis time of 4 h, strontium germinate nanowires dosage of 10 mg and initial concentration of gentian violet solution of 10 mg/L,the optimal photocatalytic effect of the strontium germinate nanowires for degrading gentian violet can be obtained, with a degrada- tion rate of 89. 59%.

quote

GB/T 7714-2015 [1] JIANG Yu-xiang, LI Yang, TIAN Lang, et al. Research on the Photocatalytic Degradation of Gentian Violet with Strontium Germinate Crystal Nanowires[J]. Rare Metals and Cemented Carbides, 2014(1): 25-28.
MLA [1] JIANG Yu-xiang, et al., "Research on the Photocatalytic Degradation of Gentian Violet with Strontium Germinate Crystal Nanowires." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 25-28.
APA [1] JIANG Yu-xiang, LI Yang, TIAN Lang, JIN Hai-bo, WANG Shuai, & PEI Li-zhai. (2014). Research on the Photocatalytic Degradation of Gentian Violet with Strontium Germinate Crystal Nanowires. Rare Metals and Cemented Carbides(1), 25-28.
IEEE [1] JIANG Yu-xiang, LI Yang, TIAN Lang, JIN Hai-bo, WANG Shuai, and PEI Li-zhai, "Research on the Photocatalytic Degradation of Gentian Violet with Strontium Germinate Crystal Nanowires," Rare Metals and Cemented Carbides, no. 1, pp. 25-28, 2014. keywords: {SrGeO3 crystal nanowire;gentian violet;degradation;photocatalysis;hydrothermal method}