Application of Warm Compaction in the Fabrication of P/M Ti Alloy AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper is described warm compaction and study of its application in the fabrication of P/M Ti alloy,as well as its potential application.The importance of lubricant design in Ti powder warm compaction was stressed.

KeyWords AITranslate

powder metallurgy warm compaction Ti alloy lubricant design

1Allison J E,et al.Titanium in engine valve systems[J].JOM, 1987,39(3):15.

2Sherman A M,et al.The use of titanium in production automobiles: potential and challenges[J].JOM,1997,49(5):38.

3Faller K,et al.The use of titanium in family automobiles:current trends[J].JOM,2001,53(2):27.

4刘咏.添加稀土元素对粉末Ti合金显微组织和力学性能的影响[A].中南大学.2003全国粉末冶金学术会议论文集[C].长沙:中南大学出版社,2003.171.

5Stanley Abkowitz.Isostatic pressing of complex shapes from titanium and titanium alloys[A].Froes F H,et al.Powder Metallurgy of Titanium Alloys[C].Las Vegas NV:Proceedings of TMS-AIME symposium,l980.291.

6刘咏,黄伯云,贺跃辉,王彬.热压反应合成 TiAl 合金的密度及孔隙分布[J].中南工业大学学报,1998,29(5):446-449. 被引量:10

7Rutz H G,et al.Warm compaction offers high density at low cost[J].Metal Powder Report,1994,49(9):40.

8李明怡,果世驹,康志君,林涛.不同类型金属粉末的温压行为[J].粉末冶金技术,2000,18(4):261-264. 被引量:38

9李元元,项品峰,徐铮,倪东惠,吴苑标.温压技术中的致密化机制[J].材料科学与工程,2001,19(1):39-42. 被引量:21

10韦嘉.[D].中南大学,2003.

1李卓梁,丁桦,李继忠.钛及钛合金剧烈塑性变形的研究进展[J].航空制造技术,2013,0(16):139-142. 被引量:13

1白小雷,李建平,刘珍光,高秀华,吴迪.异步热轧及热处理对钛合金TC4组织和力学性能的影响[J].热加工工艺,2015,44(7):44-46. 被引量:1

2张文井,丁桦,王凯.钛及钛合金剧烈塑性变形研究进展[J].钛工业进展,2017,34(3):1-8. 被引量:3

3“一种钛及钛合金球形粉末的真空感应熔炼气雾化制备方法”发明专利[J].钛工业进展,2017,34(3):8-8.

4李景艺,潘强,杨华,王晓敏,李国洲,张静.钛合金板锻造的工艺实践[J].四川冶金,2017,39(6):60-62.

5李七平,潘强,刘永利,李慧,詹劲,许敬月.钛合金板的锻造工艺方案研究[J].金属世界,2018(1):41-44.

6李七平,潘强,李慧,韩文科,许敬月,王波.钛合金板锻造工艺研究[J].装备机械,2018(1):25-28. 被引量:1

7纪小虎,李萍,时迎宾,严思梁,薛克敏.TA15钛合金等温多向锻造晶粒细化机理与力学性能[J].中国有色金属学报,2019,29(11):2515-2523. 被引量:15

8黄子坤,孙威.钛合金动态塑性变形过程中绝热剪切带的形成机理[J].材料导报,2021,35(3):3122-3128. 被引量:1

9李烨,刘世锋,王利卿,王建,王建忠.Ti-6.5Al-1Mo-1V-2Zr钛合金的组织和力学性能研究[J].热加工工艺,2021,50(14):31-35. 被引量:1

10杨蒙.浅谈钛合金材料特性及其磨削特点[J].信息记录材料,2022,23(1):41-44.

1亓家钟.铁基材料高密度温压工艺[J].粉末冶金工业,1996,6(2):14-18. 被引量:12

2易健宏,叶途明,彭元东.粉末冶金温压工艺的研究进展及展望[J].粉末冶金技术,2005,23(2):140-144. 被引量:23

3洪晓玲.转炉双渣冶炼安全留渣及其工艺[J].梅山科技,1996(1):51-53. 被引量:1

4叶途明,彭元东,易健宏,吕豫湘,胡礼福.粉末冶金温压工艺的研究进展及其展望[J].粉末冶金材料科学与工程,2003,8(4):323-328. 被引量:5

5张建勇,刘越表.国内外洁净钢生产技术综述[J].现代冶金(内蒙古),2000(1):1-9. 被引量:1

6王小宇,刘奇,薄新维,蒋春东,何浩然.W90Ni7Fe3合金制备工艺研究[J].中国金属通报,2015(S1):26-28.

7贝克.,BH,马乐天.高温特性在耐火材料选择中的重要性[J].国外耐火材料,1990,15(8):1-8.

8毛志刚.国内炼铁还原新技术的发展[J].科技资讯,2006,4(26):3-3.

9汪怡.国内直接还原与熔融还原技术的发展[J].科技资讯,2008(34):243-243.

10陈建新.50吨LF钢包炉精炼工艺的研究与应用[J].首钢科技,1997(2):29-35.

Basic Information:

DOI:

Chinese Library Classification Number:TF124.37[冶金工程—粉末冶金]

Citation Information:

In this paper is described warm compaction and study of its application in the fabrication of P/M Ti alloy,as well as its potential application.The importance of lubricant design in Ti powder warm compaction was stressed.

quote

GB/T 7714-2015 [1] LIN Xin-ping, CAO Shun-hua, LI Jiong-yi. Application of Warm Compaction in the Fabrication of P/M Ti Alloy[J]. Rare Metals and Cemented Carbides, 2004(3): 36-39.
MLA [1] LIN Xin-ping, et al., "Application of Warm Compaction in the Fabrication of P/M Ti Alloy." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 36-39.
APA [1] LIN Xin-ping, CAO Shun-hua, & LI Jiong-yi. (2004). Application of Warm Compaction in the Fabrication of P/M Ti Alloy. Rare Metals and Cemented Carbides(3), 36-39.
IEEE [1] LIN Xin-ping, CAO Shun-hua, and LI Jiong-yi, "Application of Warm Compaction in the Fabrication of P/M Ti Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 36-39, 2004. keywords: {powder metallurgy;warm compaction;Ti alloy;lubricant design}