daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis and Characterization of Polyphosphonates and Polyurethanes Using Chalcone and DOPO-Chalcone as a Flame Retardant AITranslate

Yildiz Technical University; Eskisehir Technical University; Yildiz Technical University; Eskisehir Technical University; Yildiz Technical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We synthesized a series of chalcone-based polyphosphonates and polyurethanes as self-extinguishing flame-retardant polymers and characterized them via FTIR, 1H, 13C, 31P NMR, HRMS, gel permeation chromatography, and inductively coupled plasma–optical emission spectrometry. The thermal stability of the synthesized polymer series was tested by thermogravimetric and evolved gas analysis under both N2 and air atmospheres as well as microscale combustion calorimetry analysis. After thermal treatment, residue analysis was carried out using scanning electron microscopy with energy-dispersive X-ray analysis and X-ray photoelectron spectroscopy, and decomposition mechanisms are proposed.

KeyWords AITranslate

chalcone DOPO polyphosphonates polyurethanes flame retardants fire mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01054

Chinese Library Classification Number:

Citation Information:

We synthesized a series of chalcone-based polyphosphonates and polyurethanes as self-extinguishing flame-retardant polymers and characterized them via FTIR, 1H, 13C, 31P NMR, HRMS, gel permeation chromatography, and inductively coupled plasma–optical emission spectrometry. The thermal stability of the synthesized polymer series was tested by thermogravimetric and evolved gas analysis under both N2 and air atmospheres as well as microscale combustion calorimetry analysis. After thermal treatment, residue analysis was carried out using scanning electron microscopy with energy-dispersive X-ray analysis and X-ray photoelectron spectroscopy, and decomposition mechanisms are proposed.

quote

GB/T 7714-2015 [1] Ilay C. Çetinkaya, Gamze Yüksel, Caner Macit, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01054.
MLA [1] Ilay C. Çetinkaya, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01054.
APA [1] Ilay C. Çetinkaya, Gamze Yüksel, Caner Macit, Mustafa E. Üreyen, & Tarik Eren. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01054
IEEE [1] Ilay C. Çetinkaya, Gamze Yüksel, Caner Macit, Mustafa E. Üreyen, and Tarik Eren, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01054. keywords: {chalcone;DOPO;polyphosphonates;polyurethanes;flame retardants;fire mechanism}