Photoactivatable Artificial Peroxidase System Using a Dimanganese Complex and Its Application to Light-Controlled Synthesis of Hydrogel AITranslate

Gwangju Institute of Science and Technology; Gwangju Institute of Science and Technology; Gwangju Institute of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper, we report a photoactivatable, artificial peroxidase system based on a photocaging approach. The photocaged Mn2(bpmp) (bpmp: 2,6-bis((bis(2-pyridylmethyl)amino)-methyl)-4-methylphenolate) complex was developed by a simple design and synthesis of the corresponding bpmp ligand via the introduction of the 1-(o-nitrophenyl)-ethyl (NPE) group, a well-known photoremovable protecting group. Following 365 nm light irradiation of the resulting complex, the intrinsic peroxidase-like activity of the raw Mn2(bpmp) was effectively restored. Interestingly, the degree of activation of the raw Mn2(bpmp) system was found to be altered by varying the irradiation time and/or the light intensity, providing us with a method to tune the in situ reaction kinetics ad libitum. The photocaged Mn2(bpmp) complex was further utilized for light-controlled hydrogelation by exploiting the ability of Mn2(bpmp) to catalyze the synthesis of hydrogels under physiological conditions with a phenol-functionalized hydrophilic polymer as a precursor, and the photocontrollability of this catalytic activity using an external light source. Spatial control of light irradiation using a photomask enabled site-specific activation of peroxidase-like activity, allowing the preparation of a desired shape of the hydrogel. In addition, the mechanical properties of the resultant hydrogel, such as the adhesion strength, could be regulated depending on the light exposure time of the pre-gel solution containing the precursor, H2O2, and photocaged Mn2(bpmp). Furthermore, the biocompatibility of the hydrogel synthesized using the photocaged Mn2(bpmp) was confirmed by an in vitro assay.

KeyWords AITranslate

artificial peroxidase peroxidaselike activity photoactivatable system hydrogel peroxidasemediated hydrogelation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01102

Chinese Library Classification Number:

Citation Information:

In this paper, we report a photoactivatable, artificial peroxidase system based on a photocaging approach. The photocaged Mn2(bpmp) (bpmp: 2,6-bis((bis(2-pyridylmethyl)amino)-methyl)-4-methylphenolate) complex was developed by a simple design and synthesis of the corresponding bpmp ligand via the introduction of the 1-(o-nitrophenyl)-ethyl (NPE) group, a well-known photoremovable protecting group. Following 365 nm light irradiation of the resulting complex, the intrinsic peroxidase-like activity of the raw Mn2(bpmp) was effectively restored. Interestingly, the degree of activation of the raw Mn2(bpmp) system was found to be altered by varying the irradiation time and/or the light intensity, providing us with a method to tune the in situ reaction kinetics ad libitum. The photocaged Mn2(bpmp) complex was further utilized for light-controlled hydrogelation by exploiting the ability of Mn2(bpmp) to catalyze the synthesis of hydrogels under physiological conditions with a phenol-functionalized hydrophilic polymer as a precursor, and the photocontrollability of this catalytic activity using an external light source. Spatial control of light irradiation using a photomask enabled site-specific activation of peroxidase-like activity, allowing the preparation of a desired shape of the hydrogel. In addition, the mechanical properties of the resultant hydrogel, such as the adhesion strength, could be regulated depending on the light exposure time of the pre-gel solution containing the precursor, H2O2, and photocaged Mn2(bpmp). Furthermore, the biocompatibility of the hydrogel synthesized using the photocaged Mn2(bpmp) was confirmed by an in vitro assay.

quote

GB/T 7714-2015 [1] Suji Lee, Jinyoung Oh, Min Su Han. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01102.
MLA [1] Suji Lee, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01102.
APA [1] Suji Lee, Jinyoung Oh, & Min Su Han. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01102
IEEE [1] Suji Lee, Jinyoung Oh, and Min Su Han, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01102. keywords: {artificial peroxidase;peroxidaselike activity;photoactivatable system;hydrogel;peroxidasemediated hydrogelation}