daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Development of WC Hardening Materials for Undermine Drilling Tools AITranslate

Zigong New Tungsten Products Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper has summerized the development of WC Hardening material for undermine drilling tools since 1970s with reference to some literatures both at home and abroad and on the basis of some tests made by the writer. Detailed analysis is made of the reasons why fissures,peeling-off, and tooth breaking exist in the build-up welding layer of cast WC for hardening material of steel-toothed gear drills. The effectiiveness of new hardening materials such as YM alloy, sintered WC, veneered hard alloy and nodular hard alloy is well demonstrated from various test datum.

KeyWords AITranslate

undermine drilling tool WC hardening material

1邹序枚.地质岩心钻头钻齿复合材料[J]稀有金属与硬质合金,1988(01).

1戴煜,谭兴龙,李玉玺,羊建高,黄伯云.Influence of fabricating process on microstructure and properties of spheroidal cast tungsten carbide powder[J].中国有色金属学会会刊:英文版,2005,15(2):270-274. 被引量:1

2贾德林,巴爱叶,任云鹏.镍在机械合金化制备WC粉体中的加速作用[J].机械工程材料,2008(9):42-44. 被引量:1

3巴爱叶,孙丹.镍在WC合成中加速效应的机理[J].材料开发与应用,2009,24(5):40-43.

4杨眉,高英,刘清才,刘清友,范舟,黄本生.球形硬质合金YQ3强化物探钻头试验研究[J].石油机械,2010(1):5-7.

5王新洪,邹增大.磨铣工具强化材料及焊接工艺的进展[J].机械工程材料,2001,25(4):4-6. 被引量:2

6王新洪,曲仕尧,宋思利,邹增大.套磨铣工具强化材料的组织与耐磨性能[J].焊接学报,2002,23(5):41-44. 被引量:2

7王新洪,邹增大,张敏,曲仕尧.含稀土氧化物的WC-TiC-TaC-Co/CuZnNi复合耐磨堆焊材料[J].材料科学与工艺,2003,11(3):288-292.

1王新洪,张敏,邹增大,曲仕尧.Microstructure and wear properties of YT758/CuZnNi hardfacing materials[J].中国有色金属学会会刊:英文版,2005,15(4):800-806. 被引量:1

2王延文,王鑫,郝荣明,吕维华,张连涛,张建.高效铣环在胜科1井事故处理中的应用[J].石油钻探技术,2007,35(6):44-46. 被引量:4

3吴春芬,方莹,李镇,孙怀涛,葛鹏鹏.机械合金化制备纳米晶铁-铜合金粉体[J].机械工程材料,2010,34(5):72-75. 被引量:4

4陈颢,羊建高,戴煜,陈米宋,吕健.超高温雾化制备球形铸造碳化钨粉末形貌控制及性能研究[J].中国钨业,2013,28(1):25-29. 被引量:1

5单晓伟.高效修井磨铣工具关键技术的研究[J].中国石油和化工标准与质量,2019,39(6):205-206.

6单晓伟.高效修井磨铣工具新型焊接工艺的研究和应用[J].化工管理,2019(7):155-155. 被引量:1

1黄本生,刘清友,汤小文.盘式钻头齿面强化试验[J].中国矿业,2003,12(5):59-61.

2柳小明,刘晔,王建其,高山.不同钵体研磨地质样品产生的元素污染及粒度分布探讨[J].岩矿测试,2004,23(2):121-124. 被引量:3

3毛启贵,王京彬,方同辉,于明杰,朱江建,张锐,付王伟,高卫宏.东天山红海火山成因块状硫化物矿床地质特征及成因类型探讨[J].矿产勘查,2016,7(1):17-30. 被引量:5

4何源,陈平.井下工程参数测量仪样机在文星5井的应用[J].天然气技术,2010,4(2):47-49. 被引量:2

5杨万里.初夏睡起[J].读读写写,2011(6):51-51.

6郑永乐.从模型试验看逆掩断裂带地震资料复杂化的原因[J].石油地球物理勘探,1989(1):102-107.

7张聪玲.YM区块低信噪比地震资料处理技术[J].物探化探计算技术,2010,32(2):158-163. 被引量:2

8董福新,李文平,赵梅,马志刚.YMCP-1型非接触微波流速仪比测试验及系数分析[J].山西水利科技,2012(3):67-68. 被引量:2

9张韶峰,晋为真,郑金军,许生卫.广角反射在复杂山地地震采集中的应用[J].勘探地球物理进展,2008,31(1):65-68. 被引量:3

10宋旭光,曾征,张金辉.YMH-Ⅱ数据采集机的研究[J].水利水电快报,2002,23(22):26-27.

Basic Information:

DOI:

Chinese Library Classification Number:P634.4[天文地球—地质矿产勘探]

Citation Information:

The paper has summerized the development of WC Hardening material for undermine drilling tools since 1970s with reference to some literatures both at home and abroad and on the basis of some tests made by the writer. Detailed analysis is made of the reasons why fissures,peeling-off, and tooth breaking exist in the build-up welding layer of cast WC for hardening material of steel-toothed gear drills. The effectiiveness of new hardening materials such as YM alloy, sintered WC, veneered hard alloy and nodular hard alloy is well demonstrated from various test datum.

quote

GB/T 7714-2015 [1] ZOU Xu-mei. Development of WC Hardening Materials for Undermine Drilling Tools[J]. Rare Metals and Cemented Carbides, 1995(3): 11-19.
MLA [1] ZOU Xu-mei. "Development of WC Hardening Materials for Undermine Drilling Tools." Rare Metals and Cemented Carbides, no. 3, 1995, pp. 11-19.
APA [1] ZOU Xu-mei. (1995). Development of WC Hardening Materials for Undermine Drilling Tools. Rare Metals and Cemented Carbides(3), 11-19.
IEEE [1] ZOU Xu-mei, "Development of WC Hardening Materials for Undermine Drilling Tools," Rare Metals and Cemented Carbides, no. 3, pp. 11-19, 1995. keywords: {undermine drilling tool, WC hardening material}