Treatment of Copper-separated Residue from Copper Anode Slime by Chlorination Leaching and Reduction AITranslate

School of Metallurgy and Energy Engineering, Kunming University of Technology;School of Metallurgy and Energy Engineering, Kunming University of Technology;School of Metallurgy and Energy Engineering, Kunming University of Technology;School of Metallurgy and Energy Engineering, Kunming University of Technology;School of Metallurgy and Energy Engineering, Kunming University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Gold, selenium and tellurium were separated from copper-separated residue from copper anode slime by Chlorination leaching,and then the gold was selectively reduced from the leaching solution with ferrous sulfate. The results show that under the optimized conditions of leaching time of 150 min,leaching temperature of 60 ℃ ,sodium chlorate conentration of 65 g/L,the ratio of liquid to solid of 4 : 1, sodium chloride concentration of 50 g/L, sulfuric acid concentration of 300 g/L, the leaching rates of gold, selenium and tellurium can reach 93.7%, 93.7% and 93.7%, respectively. It is feasible to reduce gold chloric acid from the chloridizing leaching solution with ferrous sulfate,and the reduction rate of gold is 99.7%. In the reduction product, gold exists as elemental gold, almost without elemental selenium, elemental tellurium and other impurities.

KeyWords AITranslate

copper-separated residue from copper anode slime chlorination leaching selective reduction gold selenium tellurium

1柳青,王吉坤.国内主要厂家阳极泥处理工艺流程改进状况[J].南方金属,2008(2):25-27. 被引量:14

2邱光文,徐远志.高银铜阳极泥湿法处理流程研究[J].有色金属设计,2000,27(2):19-24. 被引量:18

3梁君飞,柳松,谢西京.铜阳极泥处理工艺的研究进展[J].黄金,2008,29(12):32-38. 被引量:27

4马志玫.铜阳极泥硫酸化焙烧工艺改造与实践[J].甘肃冶金,2010,32(3):115-117. 被引量:9

5谢红艳,王吉坤,路辉.从铜阳极泥中回收碲研究现状[J].湿法冶金,2010,29(3):143-146. 被引量:17

6张博亚,王吉坤,彭金辉.加压酸浸从铜阳极泥中脱除碲的研究[J].有色金属:冶炼部分,2007(4):27-29. 被引量:21

7黎鼎鑫 王永录 等.贵金属提取与精炼[M].长沙:中南工业大学出版社,2000..

1李栋,徐润泽,许志鹏,郭学益.硒资源及其提取技术研究进展[J].有色金属科学与工程,2015,6(1):18-23. 被引量:16

2杨大锦.2014年云南冶金年评[J].云南冶金,2015,44(2):44-66.

3胡意文,何强.复杂稀贵金属物料的氯化浸出实验研究[J].铜业工程,2016(2):58-60.

4胡意文,何强,王日,汪秋雨,黄绍勇.控制电位还原法回收氯化浸出液中的贵金属[J].中国有色金属学报,2017,27(3):621-628. 被引量:6

5何几文,刘欢,胡智东,张福元,华中胜.铜阳极泥中碲的回收研究进展[J].稀有金属与硬质合金,2018,46(4):20-28. 被引量:11

6薛超群,郭敏,张婵.超声提取-三氯化钛还原-原子荧光光谱法对土壤样品中不同价态碲的测定[J].中国测试,2018,44(4):53-56. 被引量:2

7李超,刘述平,徐凌飞,黄雯孝,梁冠杰,何兰军.铜阳极泥中综合回收硒、碲、金等金属的研究[J].广州化工,2019,47(24):90-92. 被引量:3

8廖春发,彭珊,邹耕,曾颜亮.基于RSM超声波-微波协同氧化浸出铜阳极泥分铜渣中碲的研究[J].稀有金属与硬质合金,2020,48(2):10-17. 被引量:4

9王明双.高银合质金快速提取金的工艺研究[J].矿产综合利用,2021(4):150-153. 被引量:3

10宋旭俊,施辉献.浮选渣中碲的浸出研究[J].有色金属设计,2022,49(2):18-22.

1王雨红,吕艳,农敬义,蓝姿柳,蒋佳鸾,粟海锋.铁粉还原脱除电解锰阳极液中的硒[J].化工学报,2015,66(9):3698-3704. 被引量:6

2曾宪日,王雨红,屈欣轲,何旻雁,粟海锋.碱浸回收电解锰阳极泥中硒的研究[J].有色金属:冶炼部分,2016(8):48-51. 被引量:7

3郭学益,徐润泽,田庆华,李栋.铜阳极泥低温碱性熔炼浸出液中杂质分离[J].中国有色金属学报,2017,27(10):2120-2127. 被引量:6

4张福元,郑雅杰,彭国敏.沉金后液回收硒、碲还原剂的选择(英文)[J].中国有色金属学报:英文版,2017,27(4):917-924. 被引量:11

5何云龙,徐瑞东,何世伟,朱云,沈庆峰,陈汉森,李阔.铅阳极泥处理技术的研究进展[J].有色金属科学与工程,2017,8(5):40-51. 被引量:16

6王周亮,王雨红,粟海锋.电解锰阳极液脱硒渣中硒和铁回收工艺探索[J].中国锰业,2018,36(6):155-160.

7宁瑞,余珊,房孟钊,李伟,李飞燕.提高分金工序中碲浸出率的试验研究[J].湖南有色金属,2019,35(2):39-41. 被引量:2

8黎邹江,李栋,许志鹏,郭学益,李伟,朱刘.旋流电积在有色冶金中的应用[J].有色金属科学与工程,2019,10(5):1-7. 被引量:7

9吴展,李云峰,王亚东,胡琴.铜阳极泥回收碲的工艺优化研究[J].中国有色冶金,2019,48(6):6-9. 被引量:5

10徐小娟.氢化物发生-原子荧光光谱法在化探样品测试中的应用进展[J].安徽化工,2020,46(2):12-16. 被引量:3

1王超,蒋训雄,蒋伟,汪胜东,冯林永,董竑君.从铜阳极泥分银渣中回收铋和锑[J].有色金属:冶炼部分,2014(9):16-18. 被引量:21

2韩守礼,王金营,赵雨,贺小塘,吴喜龙,王欢,李勇,李红梅.难溶铑粉的溶解工艺研究[J].有色金属:冶炼部分,2017,0(3):40-43. 被引量:5

3黄启明,许绍权.硫酸亚铁还原Au(Ⅲ)的固相反应[J].华南师范大学学报:自然科学版,1998(3):32-34. 被引量:1

4从氯化浸出液中选择性分离锡[J].国外锡工业,1998,26(3):33-36.

5沈庆峰,杨显万,刘春侠,谢克强.硫酸亚铁还原银锰矿提取银的工艺研究[J].云南冶金,2006,35(5):26-28. 被引量:1

6张豫,华宏全.真空冶炼提纯硒的技术研发与生产实践[J].有色金属:冶炼部分,2013(10):64-68. 被引量:2

7沈庆峰,杨显万,刘春侠,谢克强.硫酸亚铁还原银锰共生矿提取银的工艺研究[J].昆明理工大学学报:理工版,2006,31(6):12-16. 被引量:3

8江涛,苏元复.从菱锌矿氯化浸出液中萃取锌和镉——Ⅰ.萃取提锌过程[J].华东化工学院学报,1991,17(1):1-9. 被引量:1

9钟扬,陈进中,伍廉奎,曹华珍,郑国渠.铅阳极泥氯化浸出液除氟研究[J].有色金属:冶炼部分,2015(10):14-17. 被引量:1

10谢醒悔.从砂砾中提取氯金酸(氯化金)的工艺[J].黄金科学技术,2004,12(4):30-30.

Basic Information:

DOI:

Chinese Library Classification Number:TF803.2[冶金工程—有色金属冶金]

Citation Information:

Gold, selenium and tellurium were separated from copper-separated residue from copper anode slime by Chlorination leaching,and then the gold was selectively reduced from the leaching solution with ferrous sulfate. The results show that under the optimized conditions of leaching time of 150 min,leaching temperature of 60 ℃ ,sodium chlorate conentration of 65 g/L,the ratio of liquid to solid of 4 : 1, sodium chloride concentration of 50 g/L, sulfuric acid concentration of 300 g/L, the leaching rates of gold, selenium and tellurium can reach 93.7%, 93.7% and 93.7%, respectively. It is feasible to reduce gold chloric acid from the chloridizing leaching solution with ferrous sulfate,and the reduction rate of gold is 99.7%. In the reduction product, gold exists as elemental gold, almost without elemental selenium, elemental tellurium and other impurities.

quote

GB/T 7714-2015 [1] ZHANG Shang-fa, WANG Chong, WANG Hua, et al. Treatment of Copper-separated Residue from Copper Anode Slime by Chlorination Leaching and Reduction[J]. Rare Metals and Cemented Carbides, 2014(1): 5-8.
MLA [1] ZHANG Shang-fa, et al., "Treatment of Copper-separated Residue from Copper Anode Slime by Chlorination Leaching and Reduction." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 5-8.
APA [1] ZHANG Shang-fa, WANG Chong, WANG Hua, YANG Kun-bin, & LI Ying-wei. (2014). Treatment of Copper-separated Residue from Copper Anode Slime by Chlorination Leaching and Reduction. Rare Metals and Cemented Carbides(1), 5-8.
IEEE [1] ZHANG Shang-fa, WANG Chong, WANG Hua, YANG Kun-bin, and LI Ying-wei, "Treatment of Copper-separated Residue from Copper Anode Slime by Chlorination Leaching and Reduction," Rare Metals and Cemented Carbides, no. 1, pp. 5-8, 2014. keywords: {copper-separated residue from copper anode slime;chlorination leaching;selective reduction;gold;selenium;tellurium}