Gas Nitriding and Microstructure of Micro-crystalline Sm-Fe Alloy Produced by Rapid Quenching Process AITranslate
Abstract AITranslate
Micro-crystalline alloys which produced by rapid solidification technologies could have better properties than as-cast alloys.Some Sm-Fe alloys were prepared under different cooling rates in the vacuum rotary quenching furnace.The microstructure and phase composition of the microstructure were studied and gas nitridation was carried out.The results show that with the increase of rapid cooling rate,the segregation of elements in the alloy decreases,and the microstructure of the alloy changes from coarse dendrite to microcrystalline.When the cooling rate reached to 24.0m/s,the alloy with a microcrystalline microstructure could be obtained.The grain growth tendency of microcrystalline Sm-Fe alloy is very small under the condition of direct nitriding of the alloy at 420℃.The grain size is small and the grain boundary area increases,which makes the effective nitriding points increase and promotes the diffusion of nitrogen atoms. However,nitrogen atoms are mainly distributed at grain boundaries in the form of nitrogen compounds, resulting in uneven nitridation between grain boundaries and grain interiors.
KeyWords AITranslate
1马建勋,严密,赵传礼,肖洪博,文玉华,杨德仁.氮化前显微组织对SmFeN合金磁性能的影响[J].材料科学与工程学报,2005,23(2):244-247. 被引量:5
2赵平,赵国际.急冷快淬工艺对Sn-9Zn-0.5Ag焊料组织与熔化特性的影响[J].热加工工艺,2017,46(1):218-220. 被引量:1
3王士显,于敦波,李红卫,罗阳,李扩社.快淬SmFe合金相结构及显微组织研究[J].稀有金属,2012,36(5):721-726. 被引量:5
4齐风春.永磁材料的发展现状[J].材料导报,1994(3):22-26. 被引量:7
5CUI ChunXiang, ZHANG Ying, SUN JiBing & WANG Ru School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300130, China.Fabrication and magnetic properties of Sm_3(Fe,Ti)_(29)N_x/α-Fe dual-phase nanocomposite permanent magnetic material[J].中国科学:技术科学英文版,2007,0(2):184-189. 被引量:1
6张然,刘颖,李芳,高升吉,涂铭旌.Sm_2Fe_(17)合金的氮化处理及其相关影响[J].磁性材料及器件,2004,35(2):39-41. 被引量:4
7方正,秦林,丁俭,赵维民.快速凝固Al-Ti-B-Sc对A356.2铝合金的晶粒细化作用[J].河北工业大学学报,2014,43(2):61-65. 被引量:3
8文磊,袁勇,王亚明,金莹.表面机械研磨处理2024铝合金表面纳米晶层和含铁层对摩擦学行为的影响机制研究(英文)[J].稀有金属材料与工程,2015,44(6):1320-1325. 被引量:5
9邓庚凤,孙光飞,陈菊芳,胡国辉,方克明.Sm_2Fe_(17)N_x永磁材料的研究进展[J].材料导报,2004,18(12):37-40. 被引量:2
10佟伟平,陶乃镕,王镇波,吕坚,卢柯.纳米结构纯铁的气体渗氮[J].热处理,2007,22(2):11-14. 被引量:8
1李文政,王博,郭正洪,顾剑锋.渗氮层组织调控对42CrMo钢磨损性能的影响[J].材料热处理学报,2018,39(1):116-122. 被引量:8
2宋春燕,王书桓,张凯璇,赵定国,柳昆.急冷Sm-Fe合金的显微结构及其氮化的研究[J].稀有金属,2018,42(12):1255-1259. 被引量:1
3文攀,薛长风,裴志胜,公维洁,卓先勤,徐云升.基于电子舌与电子鼻评价烘培时间对黄秋葵籽风味品质的影响[J].食品工业科技,2018,39(24):289-293. 被引量:8
4张颖.尿素在羊饲养生产中的使用技术[J].中国畜禽种业,2019,15(1):109-109. 被引量:1
5杨佳蔚.陕北黄土高原蒸发量时空变化及其影响因素[J].水利科技与经济,2019,25(1):7-11.
6陈川.教学改革大环境下大学英语阅读教学中元认知策略培养的意义[J].校园英语,2018,0(50):41-41.
7葛泮珠,丁石,张乐,李大东,聂红.含氮化合物对柴油超深度加氢脱硫催化剂运行稳定性的影响[J].石油学报(石油加工),2019,35(1):1-10. 被引量:2
8刘献瑶.高一学生英语词汇学习中元认知策略训练的实证研究——以牛津高中《英语》模块三&四为例[J].英语教师,2018,18(24):57-65.
9袁路妍.自适应学习系统个性化知识推荐技术研究[J].中国教育信息化,2018,24(24):94-96. 被引量:4
10马霄燕.浅析高中英语报刊阅读中元认知策略运用[J].现代教学,2019,0(1):74-75. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]
Citation Information:
Micro-crystalline alloys which produced by rapid solidification technologies could have better properties than as-cast alloys.Some Sm-Fe alloys were prepared under different cooling rates in the vacuum rotary quenching furnace.The microstructure and phase composition of the microstructure were studied and gas nitridation was carried out.The results show that with the increase of rapid cooling rate,the segregation of elements in the alloy decreases,and the microstructure of the alloy changes from coarse dendrite to microcrystalline.When the cooling rate reached to 24.0m/s,the alloy with a microcrystalline microstructure could be obtained.The grain growth tendency of microcrystalline Sm-Fe alloy is very small under the condition of direct nitriding of the alloy at 420℃.The grain size is small and the grain boundary area increases,which makes the effective nitriding points increase and promotes the diffusion of nitrogen atoms. However,nitrogen atoms are mainly distributed at grain boundaries in the form of nitrogen compounds, resulting in uneven nitridation between grain boundaries and grain interiors.
quote
| GB/T 7714-2015 | [1] SONG Chun-yan, WANG Shu-huan, ZHANG Kai-xuan, et al. Gas Nitriding and Microstructure of Micro-crystalline Sm-Fe Alloy Produced by Rapid Quenching Process[J]. Rare Metals and Cemented Carbides, 2018(6): 81-85. |
| MLA | [1] SONG Chun-yan, et al., "Gas Nitriding and Microstructure of Micro-crystalline Sm-Fe Alloy Produced by Rapid Quenching Process." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 81-85. |
| APA | [1] SONG Chun-yan, WANG Shu-huan, ZHANG Kai-xuan, & ZHAO Ding-guo. (2018). Gas Nitriding and Microstructure of Micro-crystalline Sm-Fe Alloy Produced by Rapid Quenching Process. Rare Metals and Cemented Carbides(6), 81-85. |
| IEEE | [1] SONG Chun-yan, WANG Shu-huan, ZHANG Kai-xuan, and ZHAO Ding-guo, "Gas Nitriding and Microstructure of Micro-crystalline Sm-Fe Alloy Produced by Rapid Quenching Process," Rare Metals and Cemented Carbides, no. 6, pp. 81-85, 2018. keywords: {rapid quenching;microcrystalline;Sm-Fe alloys;nitriation;microstructure} |