Sustainable Polyimidazolium Networks as Versatile Hydrogel Materials AITranslate

Max Planck Institute of Colloids and Interfaces; Max Planck Institute of Colloids and Interfaces
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper discusses the formation and properties of sustainable polyelectrolyte networks. The networks are formed from renewable precursors in a simple and green approach and feature a high density of positive charges in the main chain of the polymer backbone. Furthermore, zwitterionic systems with positive charges in the main chain and carboxylate side groups are presented. Depending on the cross-linking density and nature of the polyelectrolyte, flexible elastic or brittle networks are available which may form hydrogels upon absorption of up to 1500% water respective to their own mass. Reversible swelling in contact with different solvents furthermore envisions possible applications as smart material or selective membrane.

KeyWords AITranslate

polyelectrolyte network hydrogel imidazolium sustainable chemistry sensor smart membrane chitosan
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00491

Chinese Library Classification Number:

Citation Information:

This paper discusses the formation and properties of sustainable polyelectrolyte networks. The networks are formed from renewable precursors in a simple and green approach and feature a high density of positive charges in the main chain of the polymer backbone. Furthermore, zwitterionic systems with positive charges in the main chain and carboxylate side groups are presented. Depending on the cross-linking density and nature of the polyelectrolyte, flexible elastic or brittle networks are available which may form hydrogels upon absorption of up to 1500% water respective to their own mass. Reversible swelling in contact with different solvents furthermore envisions possible applications as smart material or selective membrane.

quote

GB/T 7714-2015 [1] Steffen TrögerMüller, Clemens Liedel. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00491.
MLA [1] Steffen TrögerMüller, and Clemens Liedel. ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00491.
APA [1] Steffen TrögerMüller, & Clemens Liedel. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00491