daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Intrinsically Freezing-Tolerant, Conductive, and Adhesive Proton Donor–Acceptor Hydrogel for Multifunctional Applications AITranslate

Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur; Indian Institute of Technology Kharagpur
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogels have unique liquid-like conductivity and solid-like mechanical properties and are promising materials for a wide range of applications, including tactile sensors and electrolytes for the energy storage device. However, combining suitable mechanical and functional properties in a single hydrogel system remains a central challenge from an application point of view. Besides, freezing of water at subzero temperature severely limits the functional potential of hydrogels. Herein, we have developed a soft yet tough proton donor–acceptor (PDA) hydrogel, combining intrinsic freezing tolerability, conductivity, and adhesiveness with ultrafast complete self-recovery (within 30 s). This unique combination of properties helps us prepare a highly durable tactile sensor (strain, pressure, and temperature) for human motion monitoring at ambient and subzero temperatures. The hydrogels were also used as a matrix to fabricate intrinsically compressible electrolytes for supercapacitor devices. The PDA-based supercapacitors show superior electrochemical performance at ambient temperature and substantially retain it at zero and subzero temperatures. This work also provides a detailed insight into the molecular interactions present in the system and correlates with the bulk mechanical and functional properties, which could guide the development of hydrogels.

KeyWords AITranslate

antifreezing adhesive conductive tactile sensor compressible supercapacitor fast selfrecovery hydrogel electrolyte human Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01285

Chinese Library Classification Number:

Citation Information:

Hydrogels have unique liquid-like conductivity and solid-like mechanical properties and are promising materials for a wide range of applications, including tactile sensors and electrolytes for the energy storage device. However, combining suitable mechanical and functional properties in a single hydrogel system remains a central challenge from an application point of view. Besides, freezing of water at subzero temperature severely limits the functional potential of hydrogels. Herein, we have developed a soft yet tough proton donor–acceptor (PDA) hydrogel, combining intrinsic freezing tolerability, conductivity, and adhesiveness with ultrafast complete self-recovery (within 30 s). This unique combination of properties helps us prepare a highly durable tactile sensor (strain, pressure, and temperature) for human motion monitoring at ambient and subzero temperatures. The hydrogels were also used as a matrix to fabricate intrinsically compressible electrolytes for supercapacitor devices. The PDA-based supercapacitors show superior electrochemical performance at ambient temperature and substantially retain it at zero and subzero temperatures. This work also provides a detailed insight into the molecular interactions present in the system and correlates with the bulk mechanical and functional properties, which could guide the development of hydrogels.

quote

GB/T 7714-2015 [1] Agniva Dutta, Prachishree Panda, Anish Das, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01285.
MLA [1] Agniva Dutta, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01285.
APA [1] Agniva Dutta, Prachishree Panda, Anish Das, Debabrata Ganguly, Santanu Chattopadhyay, Pallab Banerji, Debabrata Pradhan, & Rajat Kumar Das. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01285
IEEE [1] Agniva Dutta, Prachishree Panda, Anish Das, Debabrata Ganguly, Santanu Chattopadhyay, Pallab Banerji, Debabrata Pradhan, and Rajat Kumar Das, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01285. keywords: {antifreezing;adhesive;conductive;tactile sensor;compressible supercapacitor;fast selfrecovery;hydrogel electrolyte;human;Show More}