Synthesis and Photoluminescence Mechanism of Multicolored Nitrogen-Doped Carbon Nanodots and Their Application in Polymer Self-Assemblies AITranslate
Abstract AITranslate
For applications in the fields of biological imaging and chemical sensing, fluorescent carbon nanodots (CNDs) have excellent possibilities because of their unique structure and performance. In this work, we synthesized a series of nitrogen-doped CNDs (N-CNDs) with different fluorescent emission, ranging from blue to yellow, via one-pot solvothermal strategy. Citric acid and urea were employed as the precursors. Formamide, ethanol and N,N-dimethylformamide were used as the solvent, respectively. The excitation-dependent emission and the optimal emission were measured with the ultraviolet–visible and photoluminescence spectra. The morphology and chemical structure of the prepared N-CNDs were characterized via high-resolution transmission electron microscope (HRTEM), atomic force microscope (AFM), X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, carbon nuclear magnetic resonance (13C NMR) spectroscopy, and so forth. The influence of reaction time, temperature, and type of solvent on the structure of N-CNDs were systematically investigated. The photoluminescence mechanism was discussed based on the chemical structure, the crystallinity and the sp2/sp3 carbon ratio of the prepared N-CNDs. In addition, a biocompatible amphiphilic copolymer mPEG-b-PLLA was synthesized and self-assembled in an aqueous system. The prepared N-CNDs were introduced into the polymer self-assemblies as a fluorescent probe by an in situ grafting method. The fluorescence imaging performance of N-CNDs in the polymer self-assemblies was investigated by comparing with organic fluorescent dye coumarin-6.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00385
Chinese Library Classification Number:
Citation Information:
For applications in the fields of biological imaging and chemical sensing, fluorescent carbon nanodots (CNDs) have excellent possibilities because of their unique structure and performance. In this work, we synthesized a series of nitrogen-doped CNDs (N-CNDs) with different fluorescent emission, ranging from blue to yellow, via one-pot solvothermal strategy. Citric acid and urea were employed as the precursors. Formamide, ethanol and N,N-dimethylformamide were used as the solvent, respectively. The excitation-dependent emission and the optimal emission were measured with the ultraviolet–visible and photoluminescence spectra. The morphology and chemical structure of the prepared N-CNDs were characterized via high-resolution transmission electron microscope (HRTEM), atomic force microscope (AFM), X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, carbon nuclear magnetic resonance (13C NMR) spectroscopy, and so forth. The influence of reaction time, temperature, and type of solvent on the structure of N-CNDs were systematically investigated. The photoluminescence mechanism was discussed based on the chemical structure, the crystallinity and the sp2/sp3 carbon ratio of the prepared N-CNDs. In addition, a biocompatible amphiphilic copolymer mPEG-b-PLLA was synthesized and self-assembled in an aqueous system. The prepared N-CNDs were introduced into the polymer self-assemblies as a fluorescent probe by an in situ grafting method. The fluorescence imaging performance of N-CNDs in the polymer self-assemblies was investigated by comparing with organic fluorescent dye coumarin-6.
quote
| GB/T 7714-2015 | [1] Wenyuan Xie, Xing Yu, Tian Tian, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00385. |
| MLA | [1] Wenyuan Xie, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00385. |
| APA | [1] Wenyuan Xie, Xing Yu, Tian Tian, Chenguang Jiang, Ming Yin, Weiming Wu, Yushan Liu, Shubin Wang, & Defeng Wu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00385 |
| IEEE | [1] Wenyuan Xie, Xing Yu, Tian Tian, Chenguang Jiang, Ming Yin, Weiming Wu, Yushan Liu, Shubin Wang, and Defeng Wu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00385. keywords: {Carbon nanodots;Nitrogendoped;Structural composition;Fluorescence properties;Defect state effect} |