3D/1D Architecture Using a 1-Hexyl-3-methylimidazolium Lead Triiodide Interlayer for Robust and Highly Performing Perovskite Solar Cells 3D/1D Architecture Using a 1-Hexyl-3-methylimidazolium Lead Triiodide Interlayer for Robust and Highly Performing Perovskite Solar Cells AITranslate

University of Patras; Al-Azhar University;Theoretical and Physical Chemistry Institute; University of Crete;Elettra-Sincrotrone Trieste S.C.p.A., ss 14;Elettra-Sincrotrone Trieste S.C.p.A., ss 14;Institute of Nanoscience and Nanotechnology; University of the Peloponnese; University of Patras;Institute of Nanoscience and Nanotechnology;Institute of Nanoscience and Nanotechnology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The simultaneous improvement in the performance and stability of the perovskite solar cells (PSCs) remains a key challenge toward their commercialization. Herein, we explore the ionic liquid 1-hexyl-3-methylimidazolium iodide (HMImI) for the synthesis of a lead halide derivative, namely, (HMIm)PbI3. According to single-crystal X-ray analysis, (HMIm)PbI3 forms 1D chains of face-sharing [PbI6]4– octahedra and behaves as a semiconductor with a band gap of 2.85 eV. This compound, when deposited on top of the main 3D perovskite (Cs/FA/MA)PbI3–xBrx, passivates the surface of the absorber by lowering the density of the trap states, thus enhancing the radiative recombination and the open circuit voltage. In addition, the hydrophobic character of the alkyl chain of the imidazolium cation prohibits the penetration of the humidity and at the same time prevents ion migration from and toward the main perovskite absorber. Furthermore, the PSCs based on this 3D/1D solar cell architecture achieved a power conversion efficiency (PCE) of almost 20% and retained practically 80% of their initial efficiency after 1700 h of storage under dark and ambient conditions, outperforming the corresponding 3D reference device. This is attributed to the high quality of the perovskite layer, as confirmed by grazing-incidence wide-angle X-ray scattering, scanning electron microscopy, atomic force microscopy, and contact angle measurements. The obtained results clearly indicate that the dimensionality engineering approach involving ionic liquids with the appropriate choice of the organic cation is a very promising strategy for improving the efficiency and stability of the perovskite solar cells.

KeyWords AITranslate

perovskite solar cells dimensionality engineering stability passivation water resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01783

Chinese Library Classification Number:

Citation Information:

The simultaneous improvement in the performance and stability of the perovskite solar cells (PSCs) remains a key challenge toward their commercialization. Herein, we explore the ionic liquid 1-hexyl-3-methylimidazolium iodide (HMImI) for the synthesis of a lead halide derivative, namely, (HMIm)PbI3. According to single-crystal X-ray analysis, (HMIm)PbI3 forms 1D chains of face-sharing [PbI6]4– octahedra and behaves as a semiconductor with a band gap of 2.85 eV. This compound, when deposited on top of the main 3D perovskite (Cs/FA/MA)PbI3–xBrx, passivates the surface of the absorber by lowering the density of the trap states, thus enhancing the radiative recombination and the open circuit voltage. In addition, the hydrophobic character of the alkyl chain of the imidazolium cation prohibits the penetration of the humidity and at the same time prevents ion migration from and toward the main perovskite absorber. Furthermore, the PSCs based on this 3D/1D solar cell architecture achieved a power conversion efficiency (PCE) of almost 20% and retained practically 80% of their initial efficiency after 1700 h of storage under dark and ambient conditions, outperforming the corresponding 3D reference device. This is attributed to the high quality of the perovskite layer, as confirmed by grazing-incidence wide-angle X-ray scattering, scanning electron microscopy, atomic force microscopy, and contact angle measurements. The obtained results clearly indicate that the dimensionality engineering approach involving ionic liquids with the appropriate choice of the organic cation is a very promising strategy for improving the efficiency and stability of the perovskite solar cells.

quote

GB/T 7714-2015 [1] Eleftherios Christopoulos, Mohamed M. Elsenety, Andreas Kaltzoglou, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01783.
MLA [1] Eleftherios Christopoulos, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01783.
APA [1] Eleftherios Christopoulos, Mohamed M. Elsenety, Andreas Kaltzoglou, Constantinos C. Stoumpos, Mattia Gaboardi, Jasper R. Plaisier, Polychronis Tsipas, Elias Stathatos, Evangelos G. Vitoratos, Athanasios Dimoulas, & Polycarpos Falaras. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01783
IEEE [1] Eleftherios Christopoulos, Mohamed M. Elsenety, Andreas Kaltzoglou, Constantinos C. Stoumpos, Mattia Gaboardi, Jasper R. Plaisier, Polychronis Tsipas, Elias Stathatos, Evangelos G. Vitoratos, Athanasios Dimoulas, and Polycarpos Falaras, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01783. keywords: {perovskite solar cells dimensionality engineering stability passivation water resistance}