Study on the Steel-bonded Cemented Carbide Pre-alloyed Powder AITranslate
Abstract AITranslate
Analysis is made of the structural features of the steel-bonded cemented carbide pre-alloyed powder.Study is made of the influence of different carbon content on the pre-alloyed powder structure.Powder preparation process is developed on the basis of the features of steel-bonded cemented carbide pre-alloyed powder.The O_2 content is reduced by reduction annealing,resulting in improved powder structure.
KeyWords AITranslate
1尧登灿,章跃荣,何秋涛.钢结硬质合金—球铁镶铸工艺[J].铸造,1995,44(12):27-30. 被引量:7
2王澈,钟涛兴,周美玲.烧熔的钢结硬质合金组织的研究[J].稀有金属与硬质合金,2001,29(1):18-23. 被引量:7
1关文勇,丁义超,江书勇.碳化钒钢结硬质合金耐磨性研究[J].热加工工艺,2013,42(18):74-75. 被引量:3
1李万全,陆忠泉,邓正华,刘江,高长银.铝青铜基粉末冶金滑动轴承基体强化工艺的研究[J].热加工工艺,2016,45(10):118-120.
2葛伊伦,丁义超.热处理工艺对40Cr组织和性能的影响[J].成都工业学院学报,2017,20(1):20-23. 被引量:1
3周陈新,罗军明,李乐乐,徐吉林,黄俊.TiB2钢结硬质合金摩擦磨损行为[J].材料热处理学报,2018,39(8):114-121. 被引量:3
1王澈,钟涛兴,周美玲.预合金粉制作钢结硬质合金组织的研究[J].稀有金属与硬质合金,2001,29(3):6-9. 被引量:1
2左洪松,栾道成,王正云,李亚军,秦琴.不同含量复式碳化物对细晶硬质合金性能的影响[J].中国钨业,2011,26(6):27-30. 被引量:6
3陈雪松.影响复式碳化物(TiC-WC)固溶氧含量有关因素的研究[J].硬质合金,1999,16(3):159-161.
4王澈,钟涛兴,周美玲.WC钢结硬质合金再生研究[J].硬质合金,2001,18(3):146-149.
5左中眉,栾道成,田瀚林,陈晓男.(W,Ti,Ta)C复式碳化物对WC-(6%~8%)Co超细硬质合金性能的影响[J].中国钨业,2013,28(5):36-40. 被引量:2
6张立.WC添加方式对Cr_3C_2基硬质合金性能的影响[J].硬质合金,1998,15(2):102-104. 被引量:2
7王澈,钟涛兴,周美玲.烧熔的钢结硬质合金组织的研究[J].稀有金属与硬质合金,2001,29(1):18-23. 被引量:7
8易忠来,邵刚勤,李佳,张卫丰,王冲,段兴龙,林华幌,郭景坤.直接还原碳化法制备TiC-WC-Ni超细粉末[J].材料导报,2004,18(F04):163-164.
9廖诗兰.梯度结构硬质合金涂层刀片的金相观察[J].中国钨业,2009,24(6):35-38. 被引量:1
10高志国,杨涤心,魏世忠,龙锐.钢结硬质合金粉末/碳钢液相烧结复合过程研究[J].材料导报,2005,19(F11):446-447.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.31[冶金工程—粉末冶金]
Citation Information:
Analysis is made of the structural features of the steel-bonded cemented carbide pre-alloyed powder.Study is made of the influence of different carbon content on the pre-alloyed powder structure.Powder preparation process is developed on the basis of the features of steel-bonded cemented carbide pre-alloyed powder.The O_2 content is reduced by reduction annealing,resulting in improved powder structure.
quote
| GB/T 7714-2015 | [1] WANG Che, ZHONG Tao-xing, ZHOU Mei-ling. Study on the Steel-bonded Cemented Carbide Pre-alloyed Powder[J]. Rare Metals and Cemented Carbides, 2002(2): 7-10. |
| MLA | [1] WANG Che, et al., "Study on the Steel-bonded Cemented Carbide Pre-alloyed Powder." Rare Metals and Cemented Carbides, no. 2, 2002, pp. 7-10. |
| APA | [1] WANG Che, ZHONG Tao-xing, & ZHOU Mei-ling. (2002). Study on the Steel-bonded Cemented Carbide Pre-alloyed Powder. Rare Metals and Cemented Carbides(2), 7-10. |
| IEEE | [1] WANG Che, ZHONG Tao-xing, and ZHOU Mei-ling, "Study on the Steel-bonded Cemented Carbide Pre-alloyed Powder," Rare Metals and Cemented Carbides, no. 2, pp. 7-10, 2002. keywords: {Steel-bonded cemented carbide;pre-alloyed powder;carbon content;composite carbide} |