Improvement in Short-Channel Effects and Bias-Stress Stability of Vertical Thin-Film Transistors Using Atomic-Layer-Deposited In–Ga–Sn–O Channels Improvement in Short-Channel Effects and Bias-Stress Stability of Vertical Thin-Film Transistors Using Atomic-Layer-Deposited In–Ga–Sn–O Channels AITranslate

Kyung Hee University; Kyung Hee University;NCD Co. Ltd, Daejeon 34015;NCD Co. Ltd, Daejeon 34015;NCD Co. Ltd, Daejeon 34015;Electronics and Telecommunications Research Institute;Park Systems Corp.;Park Systems Corp.;Park Systems Corp.; Kyung Hee University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vertical-channel thin-film transistors (VTFTs), featured to uniquely employ the In–Ga–Sn–O (IGTO)-active channel layers prepared by atomic layer deposition, were fabricated with a channel length (Lch) as short as 150 nm and characterized in terms of the short-channel effect (SCE) and operational reliability. All the fabricated devices exhibited sound and stable operations, including durability against SCEs, such as negligible DIBL effects, even for the nanoscale regime in Lch. The IGTO VTFT fabricated with a channel cationic composition (In/Ga/Sn) of 3.8:3.9:1.0 was examined to exhibit excellent device characteristics such as a current drivability (CDR) of 32.2 μA/μm and an on/off current ratio as high as 108. The threshold voltage shift (ΔVTH) representing the positive bias-stress (PBS) stability was secured as low as +0.87 V at a bias stress field of 2 MV/cm for 10,000 s. The ΔVTH values of the IGTO VTFTs were noticeably found to decrease with increasing In compositions in the IGTO channels, showing more robust PBS stability. Feasible scenario for the improvement in the PBS instability for the IGTO VTFT was elucidated by analysis on the correlations between the bulk-trap density and the cationic composition in the ALD IGTO channel. The composition-dependent PBS instabilities were also suggested to be markedly influenced by the magnitude of the bias-stress field owing to the generation of Sn–O weak bonds in the IGTO channel and donation of free carriers during PBS. These obtained insights could provide a beneficial design scheme for improving the PBS instability determined by the structural disadvantages, leading to balancing CDR with the bias-stress stability of the VTFTs, even when Lch was vertically scaled down to 150 nm.

KeyWords AITranslate

In−Ga−Sn–O (IGTO) atomic layer deposition (ALD) oxide semiconductor vertical channel thinfilm transistor (TFT)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01185

Chinese Library Classification Number:

Citation Information:

Vertical-channel thin-film transistors (VTFTs), featured to uniquely employ the In–Ga–Sn–O (IGTO)-active channel layers prepared by atomic layer deposition, were fabricated with a channel length (Lch) as short as 150 nm and characterized in terms of the short-channel effect (SCE) and operational reliability. All the fabricated devices exhibited sound and stable operations, including durability against SCEs, such as negligible DIBL effects, even for the nanoscale regime in Lch. The IGTO VTFT fabricated with a channel cationic composition (In/Ga/Sn) of 3.8:3.9:1.0 was examined to exhibit excellent device characteristics such as a current drivability (CDR) of 32.2 μA/μm and an on/off current ratio as high as 108. The threshold voltage shift (ΔVTH) representing the positive bias-stress (PBS) stability was secured as low as +0.87 V at a bias stress field of 2 MV/cm for 10,000 s. The ΔVTH values of the IGTO VTFTs were noticeably found to decrease with increasing In compositions in the IGTO channels, showing more robust PBS stability. Feasible scenario for the improvement in the PBS instability for the IGTO VTFT was elucidated by analysis on the correlations between the bulk-trap density and the cationic composition in the ALD IGTO channel. The composition-dependent PBS instabilities were also suggested to be markedly influenced by the magnitude of the bias-stress field owing to the generation of Sn–O weak bonds in the IGTO channel and donation of free carriers during PBS. These obtained insights could provide a beneficial design scheme for improving the PBS instability determined by the structural disadvantages, leading to balancing CDR with the bias-stress stability of the VTFTs, even when Lch was vertically scaled down to 150 nm.

quote

GB/T 7714-2015 [1] ShinHo Noh, HyoEun Kim, Young Ha Kwon, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01185.
MLA [1] ShinHo Noh, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01185.
APA [1] ShinHo Noh, HyoEun Kim, Young Ha Kwon, NakJin Seong, Kyujeong Choi, ChiSun Hwang, GyuHo Han, SeungYeon Sung, GooEun Jung, & Sung Min Yoon. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01185
IEEE [1] ShinHo Noh, HyoEun Kim, Young Ha Kwon, NakJin Seong, Kyujeong Choi, ChiSun Hwang, GyuHo Han, SeungYeon Sung, GooEun Jung, and Sung Min Yoon, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01185. keywords: {In−Ga−Sn–O (IGTO) atomic layer deposition (ALD) oxide semiconductor vertical channel thinfilm transistor (TFT)}