Interstitial Modification of Palladium Nanocubes with Nitrogen Atoms Promotes Aqueous Electrocatalytic Alkyne Semihydrogenation AITranslate

Tianjin University; Tianjin University; Hebei Normal University; Tianjin University; Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Developing nanostructures to drive the selective and durable electrocatalytic semihydrogenation of alkynes to alkenes with a high Faradaic efficiency (FE) is highly desirable. Here, we propose that the desired catalytic materials should meet three requirements: (1) catalyst oxidation potential higher than alkyne reduction potential, (2) easy desorption of alkene and difficult formation of PdHx, and (3) higher energy barriers for H* self-coupling than H* adds to an alkyne molecule. Thus, Pd2N nanocubes with nitrogen-atom-modified Pd interstitial sites are designed and synthesized to achieve 95.7% alkyne conversion, 97.8% alkene selectivity, and 72.4% alkene FE. The catalyst can be used for 18-cycle measurements without performance decline. A mechanistic study shows that the high selectivity is due to the inhibited PdHx, the weakened alkene adsorption, and the increased energy barrier for alkene hydrogenation. The high energy barrier for H* coupling to release H2 leads to the high alkene FE. In addition, the potential-independent alkene selectivity enables Pd2N to fit the fluctuating voltage in a solar-powered system. Furthermore, Pd2N is suitable for other functionalized alkynes and deuterated alkyne semihydrogenation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00944

Chinese Library Classification Number:

Citation Information:

Developing nanostructures to drive the selective and durable electrocatalytic semihydrogenation of alkynes to alkenes with a high Faradaic efficiency (FE) is highly desirable. Here, we propose that the desired catalytic materials should meet three requirements: (1) catalyst oxidation potential higher than alkyne reduction potential, (2) easy desorption of alkene and difficult formation of PdHx, and (3) higher energy barriers for H* self-coupling than H* adds to an alkyne molecule. Thus, Pd2N nanocubes with nitrogen-atom-modified Pd interstitial sites are designed and synthesized to achieve 95.7% alkyne conversion, 97.8% alkene selectivity, and 72.4% alkene FE. The catalyst can be used for 18-cycle measurements without performance decline. A mechanistic study shows that the high selectivity is due to the inhibited PdHx, the weakened alkene adsorption, and the increased energy barrier for alkene hydrogenation. The high energy barrier for H* coupling to release H2 leads to the high alkene FE. In addition, the potential-independent alkene selectivity enables Pd2N to fit the fluctuating voltage in a solar-powered system. Furthermore, Pd2N is suitable for other functionalized alkynes and deuterated alkyne semihydrogenation.

quote

GB/T 7714-2015 [1] Ziyang Song, Chuanqi Cheng, Changhong Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00944.
MLA [1] Ziyang Song, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00944.
APA [1] Ziyang Song, Chuanqi Cheng, Changhong Wang, Junwei Yao, Cuibo Liu, Bin Zhang, & Yongmeng Wu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00944
IEEE [1] Ziyang Song, Chuanqi Cheng, Changhong Wang, Junwei Yao, Cuibo Liu, Bin Zhang, and Yongmeng Wu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00944.