daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Transparent Optoelectronic Synapse Based on a CuI Electrode for Arithmetic Operation Transparent Optoelectronic Synapse Based on a CuI Electrode for Arithmetic Operation AITranslate

East China Normal University; East China Normal University; East China Normal University; East China Normal University; East China Normal University; East China Normal University; East China Normal University; East China Normal University; Shanxi University; Shanxi University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Transparent optoelectronic synapses are attracting great attention due to their great potentials in constructing “invisible” electronic products. In this work, CuI, a p-type semiconductor with good conductivity and transparency, is adopted as the electrode material. A transparent optoelectronic synapse is fabricated with a structure of CuI/copper-phthalocyanine (CuPc)/indium-tin oxide. The device shows a sensitive and linear response to the light stimulation with a wavelength of 660 nm. Some basic functions of biological synapses, such as paired-pulse facilitation, spike-rate-dependent plasticity, spike-number-dependent plasticity, and so forth, are successfully simulated by this transparent optoelectronic synapse. Furthermore, based on the high linear relationship between the device response and the number of light pulses, basic arithmetic operations of addition, subtraction, multiplication, and division within 20 are realized. The experimental results not only show the good performance of the device as an artificial synapse but also illustrate the great application potential of CuI in transparent and metallic electrode-free optoelectronics.

KeyWords AITranslate

optoelectronic synapse memristor transparency arithmetic operation copper(II) phthalocyanine copper(I) iodide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00155

Chinese Library Classification Number:

Citation Information:

Transparent optoelectronic synapses are attracting great attention due to their great potentials in constructing “invisible” electronic products. In this work, CuI, a p-type semiconductor with good conductivity and transparency, is adopted as the electrode material. A transparent optoelectronic synapse is fabricated with a structure of CuI/copper-phthalocyanine (CuPc)/indium-tin oxide. The device shows a sensitive and linear response to the light stimulation with a wavelength of 660 nm. Some basic functions of biological synapses, such as paired-pulse facilitation, spike-rate-dependent plasticity, spike-number-dependent plasticity, and so forth, are successfully simulated by this transparent optoelectronic synapse. Furthermore, based on the high linear relationship between the device response and the number of light pulses, basic arithmetic operations of addition, subtraction, multiplication, and division within 20 are realized. The experimental results not only show the good performance of the device as an artificial synapse but also illustrate the great application potential of CuI in transparent and metallic electrode-free optoelectronics.

quote

GB/T 7714-2015 [1] Yanting Li, Rongxue Ji, Pengfei Zhao, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00155.
MLA [1] Yanting Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00155.
APA [1] Yanting Li, Rongxue Ji, Pengfei Zhao, Jie Lao, Chunli Jiang, Bobo Tian, Chunhua Luo, Hechun Lin, Hui Peng, & ChunGang Duan. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00155
IEEE [1] Yanting Li, Rongxue Ji, Pengfei Zhao, Jie Lao, Chunli Jiang, Bobo Tian, Chunhua Luo, Hechun Lin, Hui Peng, and ChunGang Duan, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00155. keywords: {optoelectronic synapse memristor transparency arithmetic operation copper(II) phthalocyanine copper(I) iodide}