Research on Microstructure and Mechanical Properties of Ti600 High Temperature Titanium Alloy for Engine AITranslate
Abstract AITranslate
The microstructure and mechanical properties of Ti600 high temperature titanium alloy for engine were researched by optical microscope,X-ray diffractometer and mechanical property test. The results show that Ti600 plate is mainly composed of equiaxed primary a grains and a small amount of lamellar α+β eutectic tissue. Ti600 alloy has small grains and uniform microstructure,and its average gain size is about 2- 4 μm. Ti600 alloy plate has high strength and plasticity at room temperature. With the increase of temperature,tensile strength and yield strength show a weak increasing trend, while elongation rate significantly increases. Ti600 titanium alloy plate is characterized by ductile fracture,with a dimple fracture.
KeyWords AITranslate
1侯金健,高强强,安晓婷.国内外高温钛合金研究及应用的最新发展[J].热加工工艺,2014,43(10):11-15. 被引量:19
2魏宝敏,台立民.Ti-Al-Sn-Zr-Mo-Si系高温钛合金的研究进展[J].特种铸造及有色合金,2013,33(5):424-428. 被引量:14
3康凤,陈嫚丽,宁海青,胡传凯,舒大禹,沈蕾芳.TC4钛合金材料的切削变形模拟及试验研究[J].稀有金属与硬质合金,2012,40(6):31-34. 被引量:4
4辛社伟,洪权,卢亚锋,郭萍,戚运莲,曾立英.Ti600高温钛合金600℃下组织稳定性研究[J].稀有金属材料与工程,2010,39(11):1918-1922. 被引量:12
5马陶然,汤海波,方艳丽,王华明.热处理对激光沉积Ti60A高温钛合金组织及性能的影响[J].热加工工艺,2012,41(14):199-202. 被引量:5
6屈雅倩,郭鸿镇,姚泽坤,田宏杰.Ti60高温钛合金的超塑性拉伸行为及组织演变[J].热加工工艺,2014,43(14):50-52. 被引量:4
7纪仁峰,闵新华,胡弘剑,廖洪军.TA15钛合金高温塑性变形流变应力行为研究[J].稀有金属与硬质合金,2009,37(2):12-16. 被引量:7
8黄旭,李臻熙,黄浩.高推重比航空发动机用新型高温钛合金研究进展[J].中国材料进展,2011,30(6):21-27. 被引量:80
9陈玉勇,孔凡涛.TiAl合金显微组织细化[J].金属学报,2008,44(5):551-556. 被引量:23
1黄栋,杨绍利,马兰,廖鑫,朴荣勋.高温钛合金的研究现状及其发展[J].钢铁钒钛,2018,39(1):60-66. 被引量:13
2朱钰玲,杨绍利,马兰,朴荣勋.氢化钛含量对近α型多元高温钛合金的影响[J].钢铁钒钛,2019,40(5):50-54. 被引量:3
1常田仓,章晓林,赵文迪,景满,申培伦.金红石选矿技术研究综述[J].矿产保护与利用,2019,39(5):167-173. 被引量:10
2肖艮,沈旭,殷亚军,李振涛,计效园,周建新.基于PTV的钛合金离心铸造物理模拟流速表征[J].特种铸造及有色合金,2020,40(4):404-408. 被引量:1
3肖子凡,邵旭,王闯,张一堃,张学萍.不同冷却方式对钛合金组织和性能的影响[J].湖北农机化,2020(5):177-177.
4李海燕,寇佩佩,李龙龙,冯瑞成,曹卉.晶向对含空位单晶γ-TiAl合金拉伸性能的影响[J].稀有金属材料与工程,2020,49(5):1593-1600. 被引量:1
5向午渊,江海涛,田世伟.钛及钛合金高温氧化行为研究[J].金属功能材料,2020,27(3):33-39. 被引量:11
6曹贯宇,于天池,王旭峰,张宁,刘慧敏,刘景顺.固溶/时效对Ti-6Al-4V-0.5Fe合金的力学及电化学性能的影响[J].热加工工艺,2020,49(10):99-103. 被引量:1
7孙世臣,田玉晶,胡辰,方晓英,赵而团.TiBw对高温钛基复合材料基体的强化作用研究[J].钛工业进展,2020,37(3):15-19. 被引量:3
8包平,李锦,王明全,朱宝洪,罗志豪.粉末冶金钛合金的In合金化、组织及性能研究[J].热加工工艺,2020,49(18):75-80.
9朴荣勋,杨绍利,朱钰玲,马兰.TiH2基粉末冶金近α钛合金Ti-1100的热变形行为[J].稀有金属材料与工程,2020,49(10):3314-3324. 被引量:1
10魏鑫成,黄丽霞,戴雪梅,石文泽,李煦钊.钛合金板裂纹损伤声发射源的信号特征分析[J].实验室研究与探索,2021,40(1):1-6. 被引量:2
1朱永兵,慕思国,李华清,郭富安.Cu-Cr-Zr系合金变形过程中的织构分析[J].材料工程,2009,37(7):9-11. 被引量:7
2张谊.建筑用钎焊接头组织与力学性能的研究[J].粉末冶金工业,2017,27(3):44-48. 被引量:1
3田亚强,张明山,董福涛,李红斌,魏英立,陈连生.低碳钢淬火等温碳配分中粒状贝氏体组织演变及性能[J].钢铁研究学报,2017,29(5):420-424. 被引量:7
4冯文荣.热处理工艺对工程机械用钢组织与性能的影响[J].金属热处理,2017,42(6):84-88. 被引量:6
5任家宽,吴思炜,陈其源,周晓光,刘振宇.Ti含量对低碳钢力学性能的影响[J].金属热处理,2017,42(6):137-141. 被引量:7
6张文儒.退火温度和铬元素对电工钢组织和性能的影响[J].热加工工艺,2017,46(12):222-224. 被引量:1
7潘晖,赵海生.钴基钎料钎焊K465合金大间隙接头组织与性能[J].航空材料学报,2017,37(3):50-55. 被引量:3
8牟浩瀚,马帅,胥恩泽,王晓艳,张斌,张廷,仲洪海,蒋阳.时效处理对城市轨道交通铜基受电弓滑板组织与性能的影响[J].粉末冶金材料科学与工程,2017,22(3):435-442. 被引量:1
9B.Я.Белоус,兰金亮,赵清元.气候因素对BHC-73高强钢力学性能和耐腐蚀性的影响研究[J].现代冶金(内蒙古),2017,0(2):22-25.
10王桢,周邦新,王波阳,姚美意,李强,张金龙.Zr-4合金在300℃去离子水中腐蚀初期氧化膜的研究[J].稀有金属材料与工程,2017,46(6):1602-1607. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG156.1[金属学及工艺—热处理]
Citation Information:
The microstructure and mechanical properties of Ti600 high temperature titanium alloy for engine were researched by optical microscope,X-ray diffractometer and mechanical property test. The results show that Ti600 plate is mainly composed of equiaxed primary a grains and a small amount of lamellar α+β eutectic tissue. Ti600 alloy has small grains and uniform microstructure,and its average gain size is about 2- 4 μm. Ti600 alloy plate has high strength and plasticity at room temperature. With the increase of temperature,tensile strength and yield strength show a weak increasing trend, while elongation rate significantly increases. Ti600 titanium alloy plate is characterized by ductile fracture,with a dimple fracture.
quote
| GB/T 7714-2015 | [1] DING Qun-yan. Research on Microstructure and Mechanical Properties of Ti600 High Temperature Titanium Alloy for Engine[J]. Rare Metals and Cemented Carbides, 2017(3): 41-44. |
| MLA | [1] DING Qun-yan. "Research on Microstructure and Mechanical Properties of Ti600 High Temperature Titanium Alloy for Engine." Rare Metals and Cemented Carbides, no. 3, 2017, pp. 41-44. |
| APA | [1] DING Qun-yan. (2017). Research on Microstructure and Mechanical Properties of Ti600 High Temperature Titanium Alloy for Engine. Rare Metals and Cemented Carbides(3), 41-44. |
| IEEE | [1] DING Qun-yan, "Research on Microstructure and Mechanical Properties of Ti600 High Temperature Titanium Alloy for Engine," Rare Metals and Cemented Carbides, no. 3, pp. 41-44, 2017. keywords: {Ti600;high temperature titanium alloy;microstructure;mechanical property} |