A Physically Cross-Linked Sodium Alginate–Gelatin Hydrogel with High Mechanical Strength AITranslate
Abstract AITranslate
Hydrogels constructed from pure biomacromolecules with multifunctions of good mechanical performances, ionic environmental stability, self-healing, biocompatibility, and ionic conductivity are desirable but remain as a challenge. In this work, hydrogels composed of pure biomacromolecules of gelatin and sodium alginate were constructed through a simple repeated acid soaking–drying–swelling process. The obtained hydrogel with a physically cross-linked interpenetrated network of gelatin and sodium alginate contained 79% water and had a relatively high fracture tensile stress and strain of 0.46 MPa and 2.4, respectively. As the gel was cross-linked with a hydrogen bond and alginic acid, it exhibited good stability in a physiological saline solution. Furthermore, the gel exhibited good biocompatibility, self-healing properties, and ionic conductivity, demonstrating its excellent potential for applications in biomedical materials and biosensors.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00404
Chinese Library Classification Number:
Citation Information:
Hydrogels constructed from pure biomacromolecules with multifunctions of good mechanical performances, ionic environmental stability, self-healing, biocompatibility, and ionic conductivity are desirable but remain as a challenge. In this work, hydrogels composed of pure biomacromolecules of gelatin and sodium alginate were constructed through a simple repeated acid soaking–drying–swelling process. The obtained hydrogel with a physically cross-linked interpenetrated network of gelatin and sodium alginate contained 79% water and had a relatively high fracture tensile stress and strain of 0.46 MPa and 2.4, respectively. As the gel was cross-linked with a hydrogen bond and alginic acid, it exhibited good stability in a physiological saline solution. Furthermore, the gel exhibited good biocompatibility, self-healing properties, and ionic conductivity, demonstrating its excellent potential for applications in biomedical materials and biosensors.
quote
| GB/T 7714-2015 | [1] Lini Wang, Hui Jie Zhang, Xueqian Liu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00404. |
| MLA | [1] Lini Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00404. |
| APA | [1] Lini Wang, Hui Jie Zhang, Xueqian Liu, Yun Liu, Xing Zhu, Xinhua Liu, & Xiangyu You. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00404 |
| IEEE | [1] Lini Wang, Hui Jie Zhang, Xueqian Liu, Yun Liu, Xing Zhu, Xinhua Liu, and Xiangyu You, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00404. keywords: {hydrogel;sodium alginate;gelatin;mechanical performance;biocompatibility} |