daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Investigation on Effect of CexLa1-x Active Component on Denitration Performance of NH3-SCR AITranslate

State Key Laboratory of Integrated Exploitation of Bayan Obo Multi-metal Resources;State Key Laboratory of Integrated Exploitation of Bayan Obo Multi-metal Resources;State Key Laboratory of Integrated Exploitation of Bayan Obo Multi-metal Resources;State Key Laboratory of Integrated Exploitation of Bayan Obo Multi-metal Resources
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to explore the effect of the combined action of Ce and La in natural bastnaesite on denitration performance,the CexLa1-x active component was prepared by microwave heating and loaded onγ-Al2O3 for activity test.Ce0.8La0.2 catalyst has the best denitration effect and 78%NO conversion at 350℃.The results of BET,NH3-TPD,XRD,Raman and XPS show that the active component of Ce0.8La0.2 catalyst is a solid solution containing Ce and La,which has better adsorption capacity of NH3 and higher specific surface area,and the surface adsorption of oxygen on Ce0.8La0.2 catalyst is one of the reasons for improving the catalytic performance of NH3-SCR.

KeyWords AITranslate

bastnasite Ce/La active component NH3-SCR surface adsorption of oxygen denitration performance NO conversion

1王瑞,归柯庭,梁辉.Ce的掺杂对负载型催化剂LaMnO_3/赤铁矿脱硝性能的影响[J].化工进展,2016,35(B11):192-199. 被引量:7

2士丽敏,储伟,瞿芬芬,胡金燕,李民敏.Catalytic performance for methane combustion of supported Mn-Ce mixed oxides[J].稀土学报:英文版,2008,26(6):836-840. 被引量:6

3郭凤,余剑,朱剑虹,刘云义,许光文.Mn-Fe-Ce/TiO_2低温NH_3选择性催化还原NO[J].过程工程学报,2009,9(6):1192-1197. 被引量:16

4张光学,周安琪,范海燕,王进卿,池作和.铁铈氧化物SCR脱硝催化剂的制备及性能[J].燃料化学学报,2015,43(10):1267-1272. 被引量:10

5王金淑,周美玲,张久兴,聂祚仁,左铁镛.碳化La_2O_3-Mo阴极材料的高温XPS研究[J].稀有金属材料与工程,2000,29(4):225-227. 被引量:15

6唐晓龙,郝吉明,徐文国,李俊华.固定源低温选择性催化还原NO_x技术研究进展[J].环境科学学报,2005,25(10):1297-1305. 被引量:39

7赵莹,范丽.我国SCR催化剂的技术现状综述[J].现代工业经济和信息化,2013,3(18):53-55. 被引量:5

8杨瀚,仲兆平,朱林,王春华.铁铈复合催化剂的低温SCR脱硝性能[J].环境工程学报,2017,11(4):2413-2418. 被引量:6

9姚小江,陈丽,孔婷婷,丁世敏,罗琼,杨复沫.负载型铈基催化剂在NH_3-SCR反应中的载体效应(英文)[J].催化学报(英文),2017,38(8):1423-1430. 被引量:15

10伍斌,童志权,黄妍.MnO_2/NaY催化剂上NH_3低温选择催化还原NO_x[J].石油化工,2006,35(2):178-182. 被引量:24

1吴彦霞,梁海龙,陈鑫,陈琛,王献忠,戴长友,胡利明,陈玉峰.元素(Ce、Co、La、Sn)掺杂对V-Mo/TiO_(2)催化剂脱硝活性的影响[J].材料导报,2021,35(6):6020-6027. 被引量:4

1张柏林,张生杨,张深根.稀土元素在脱硝催化剂中的应用[J].化学进展,2022,34(2):301-318. 被引量:2

2梁海龙,吴彦霞,陈玉峰,胡利明,王春朋.焙烧温度对MnO_(x)催化还原NO性能的影响[J].石油炼制与化工,2022,53(9):78-82.

3吴彦霞,陈玉峰,梁海龙,胡利明,王春朋.掺杂Sn对V/UiO-66催化剂抗碱金属性能的影响[J].稀有金属材料与工程,2023,52(1):41-47.

4宋丽云,邓世林,周宜芸,李双叶,展宗城,李坚,何洪.V_(2)O_(5)-MoO_(3)/TiO_(2)催化剂的NH_(3)-SCR性能:载体的影响[J].材料导报,2023,37(6):67-72.

1张显威,苏亚欣,程江浩,林睿,温妮妮,邓文义,周皞.Ag对Fe/Al-PILC的SCR-C3H6脱硝特性的影响[J].燃料化学学报,2019,47(11):1368-1378. 被引量:6

2宋旭东,袁鸽成,黎小辉,奉隆彪.异步轧制Mg-3Zn-2(Ce/La)-1Mn合金的微观组织及织构演变[J].金属热处理,2020,45(2):1-6. 被引量:3

3其其格吉日嘎拉,李晨曦,叶青,程锦,程水源,康天放.Ce-Fe/ZSM-5催化剂NH3选择性催化还原NO性能研究[J].化工环保,2020,40(2):192-197.

4刘海龙,赵晶,陈涛,金坦,李兴.次氯酸钙溶液的脱硫脱硝特性[J].化工环保,2020,40(1):48-52. 被引量:1

5皇甫林,李长明,王超,李萍,李运甲,高士秋,余剑.硅系黏结剂对涂覆型蜂窝体催化剂性能的影响[J].过程工程学报,2020,20(4):484-492. 被引量:8

6蔡炜,尚希婷,王虎,江晓明,钟秦.前驱体溶液pH对核壳型Cr/CeO2催化剂低温选择性催化氧化脱硝性能的影响[J].化工环保,2020,40(2):154-161.

Basic Information:

DOI:

Chinese Library Classification Number:O643[理学—物理化学]

Citation Information:

In order to explore the effect of the combined action of Ce and La in natural bastnaesite on denitration performance,the CexLa1-x active component was prepared by microwave heating and loaded onγ-Al2O3 for activity test.Ce0.8La0.2 catalyst has the best denitration effect and 78%NO conversion at 350℃.The results of BET,NH3-TPD,XRD,Raman and XPS show that the active component of Ce0.8La0.2 catalyst is a solid solution containing Ce and La,which has better adsorption capacity of NH3 and higher specific surface area,and the surface adsorption of oxygen on Ce0.8La0.2 catalyst is one of the reasons for improving the catalytic performance of NH3-SCR.

quote

GB/T 7714-2015 [1] ZHANG Kai, QI Da-shuang, GONG Zhi-jun, et al. Investigation on Effect of CexLa1-x Active Component on Denitration Performance of NH3-SCR[J]. Rare Metals and Cemented Carbides, 2020(1): 18-24.
MLA [1] ZHANG Kai, et al., "Investigation on Effect of CexLa1-x Active Component on Denitration Performance of NH3-SCR." Rare Metals and Cemented Carbides, no. 1, 2020, pp. 18-24.
APA [1] ZHANG Kai, QI Da-shuang, GONG Zhi-jun, & WU Wen-fei. (2020). Investigation on Effect of CexLa1-x Active Component on Denitration Performance of NH3-SCR. Rare Metals and Cemented Carbides(1), 18-24.
IEEE [1] ZHANG Kai, QI Da-shuang, GONG Zhi-jun, and WU Wen-fei, "Investigation on Effect of CexLa1-x Active Component on Denitration Performance of NH3-SCR," Rare Metals and Cemented Carbides, no. 1, pp. 18-24, 2020. keywords: {bastnasite;Ce/La;active component;NH3-SCR;surface adsorption of oxygen;denitration performance;NO conversion}