Understanding the Polymorphism of Cobalt Nanoparticles Formed in Electrodeposition─An In Situ XRD Study AITranslate

Georgia Institute of Technology;Georgia Institute of Technology;University of Maryland; Brookhaven National Laboratory; Argonne National Laboratory;University of Maryland;Georgia Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An advanced synchrotron-based in situ X-ray diffraction (XRD) technique is successfully developed and employed to track and monitor the formation and phase selection of cobalt (Co) in electrodeposition in real time and verify DFT computational results. The impacts of a number of controlling factors including the pH of the electrolyte and deposition overpotential are systematically studied. The results show that the yielded phase of the electrodeposited Co is controlled by both thermodynamics and kinetics. The low pH low overpotential condition favors the formation of the thermodynamically stable fcc phase. While the high pH high overpotential condition promotes the formation of the metastable hcp phase. The experimental results agree well with the nanometric phase diagram computed with DFT. Layer-by-layer alternative stacking of fcc-hcp polymorphic phases can be facilely fabricated by just varying the overpotential. This work not only offers an effective means to control the phase of electroplating of Co but also presents a new approach to reveal the fundamental insights of the formation of metals under electrochemical reduction driving force.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c00861

Chinese Library Classification Number:

Citation Information:

An advanced synchrotron-based in situ X-ray diffraction (XRD) technique is successfully developed and employed to track and monitor the formation and phase selection of cobalt (Co) in electrodeposition in real time and verify DFT computational results. The impacts of a number of controlling factors including the pH of the electrolyte and deposition overpotential are systematically studied. The results show that the yielded phase of the electrodeposited Co is controlled by both thermodynamics and kinetics. The low pH low overpotential condition favors the formation of the thermodynamically stable fcc phase. While the high pH high overpotential condition promotes the formation of the metastable hcp phase. The experimental results agree well with the nanometric phase diagram computed with DFT. Layer-by-layer alternative stacking of fcc-hcp polymorphic phases can be facilely fabricated by just varying the overpotential. This work not only offers an effective means to control the phase of electroplating of Co but also presents a new approach to reveal the fundamental insights of the formation of metals under electrochemical reduction driving force.

quote

GB/T 7714-2015 [1] Xuetian Ma, Yifan Ma, Adelaide M. Nolan, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00861.
MLA [1] Xuetian Ma, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00861.
APA [1] Xuetian Ma, Yifan Ma, Adelaide M. Nolan, Jianming Bai, Wenqian Xu, Yifei Mo, & Hailong Chen. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00861
IEEE [1] Xuetian Ma, Yifan Ma, Adelaide M. Nolan, Jianming Bai, Wenqian Xu, Yifei Mo, and Hailong Chen, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00861.