Unraveling Piezoelectricity of Two-Dimensional Ferroelectric Metal 1T′′-MoS2 AITranslate
Abstract AITranslate
The recent discovery of ferroelectric behavior in two-dimensional (2D) van der Waals materials has spurred interest in their piezoelectric properties, which are determined by the relative strength of the inter- and intralayer interactions. However, progress in this field is hindered by the high electrical conductivity and weak piezoelectricity of 2D ferroelectrics: establishing not only a magnitude but also a sign of the piezoelectric coefficient in these materials via measurements of the electrically induced strain as a function of polarization proved to be extremely challenging. Here, we report investigation of the longitudinal piezoelectric coefficient in the recently discovered 2D ferroelectric 1T′′-MoS2 by means of local probe microscopy techniques. The electromechanical response and the surface potential of the flexoelectrically poled 1T′′-MoS2 have been tested by piezoresponse and Kelvin probe force microscopies, respectively. The comparative interferometric displacement spectroscopy studies provide solid evidence of the mechanically induced polarization direction in 1T′′-MoS2 and allow quantification of its piezoelectric response. It is found that 1T′′-MoS2 exhibits negative piezoelectricity with a d33 value of the order of −3 pm/V. First-principles density-functional theory calculations support the experimental findings for d33 in both sign and magnitude.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c01051
Chinese Library Classification Number:
Citation Information:
The recent discovery of ferroelectric behavior in two-dimensional (2D) van der Waals materials has spurred interest in their piezoelectric properties, which are determined by the relative strength of the inter- and intralayer interactions. However, progress in this field is hindered by the high electrical conductivity and weak piezoelectricity of 2D ferroelectrics: establishing not only a magnitude but also a sign of the piezoelectric coefficient in these materials via measurements of the electrically induced strain as a function of polarization proved to be extremely challenging. Here, we report investigation of the longitudinal piezoelectric coefficient in the recently discovered 2D ferroelectric 1T′′-MoS2 by means of local probe microscopy techniques. The electromechanical response and the surface potential of the flexoelectrically poled 1T′′-MoS2 have been tested by piezoresponse and Kelvin probe force microscopies, respectively. The comparative interferometric displacement spectroscopy studies provide solid evidence of the mechanically induced polarization direction in 1T′′-MoS2 and allow quantification of its piezoelectric response. It is found that 1T′′-MoS2 exhibits negative piezoelectricity with a d33 value of the order of −3 pm/V. First-principles density-functional theory calculations support the experimental findings for d33 in both sign and magnitude.
quote
| GB/T 7714-2015 | [1] Haidong Lu, Hugo Aramberri, Alexey Lipatov, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c01051. |
| MLA | [1] Haidong Lu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c01051. |
| APA | [1] Haidong Lu, Hugo Aramberri, Alexey Lipatov, Roger Proksch, Alexander Sinitskii, Jorge Íñiguez, & Alexei Gruverman. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c01051 |
| IEEE | [1] Haidong Lu, Hugo Aramberri, Alexey Lipatov, Roger Proksch, Alexander Sinitskii, Jorge Íñiguez, and Alexei Gruverman, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c01051. |