Colorfully Patterned Epoxy Resin Films with a Cholesteric Structure Prepared through a Photopolymerization Approach AITranslate

Soochow University; Soochow University; Soochow University; Soochow University; Soochow University; Soochow University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Structurally colored epoxy resin films were prepared using a liquid crystalline (LC) epoxy monomer of E11M and a chiral additive of CA-iso through a photopolymerization approach. With the addition of the co-photoinitiator isopropyl thioxanthone and comonomer 3′,4′-epoxycyclohexylmethyl 3,4-epoxycyclohexylcarboxylate, the polymerization rate was increased. Since the epoxy resin films can be obtained within several seconds, they are feasible for large-area preparation on the coating line. The reflective wavelength was tunable by changing the concentration of CA-iso in the LC mixture. Diffuse-reflectance circular dichroism spectra indicated a right-handed helical supramolecular structure. Field-emission scanning electron microscopy images indicated a multilayer structure. Since the LC mixtures were thermochromic, colorfully patterned epoxy resin films were prepared by controlling the polymerization temperature. Moreover, LC gratings were also prepared, which were expected to be applied for anticounterfeiting.

KeyWords AITranslate

photopolymerization epoxy resin liquid crystal grating structural colors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01432

Chinese Library Classification Number:

Citation Information:

Structurally colored epoxy resin films were prepared using a liquid crystalline (LC) epoxy monomer of E11M and a chiral additive of CA-iso through a photopolymerization approach. With the addition of the co-photoinitiator isopropyl thioxanthone and comonomer 3′,4′-epoxycyclohexylmethyl 3,4-epoxycyclohexylcarboxylate, the polymerization rate was increased. Since the epoxy resin films can be obtained within several seconds, they are feasible for large-area preparation on the coating line. The reflective wavelength was tunable by changing the concentration of CA-iso in the LC mixture. Diffuse-reflectance circular dichroism spectra indicated a right-handed helical supramolecular structure. Field-emission scanning electron microscopy images indicated a multilayer structure. Since the LC mixtures were thermochromic, colorfully patterned epoxy resin films were prepared by controlling the polymerization temperature. Moreover, LC gratings were also prepared, which were expected to be applied for anticounterfeiting.

quote

GB/T 7714-2015 [1] Xiaoli Zhang, Yongxing Guo, Yi Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01432.
MLA [1] Xiaoli Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01432.
APA [1] Xiaoli Zhang, Yongxing Guo, Yi Li, Wei Liu, Hongkun Li, & Yonggang Yang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01432
IEEE [1] Xiaoli Zhang, Yongxing Guo, Yi Li, Wei Liu, Hongkun Li, and Yonggang Yang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01432. keywords: {photopolymerization;epoxy resin;liquid crystal;grating;structural colors}