Brief description is made of the preparation of ultra-pure W powder and W materials abroad.In the paper is reported assaying results of the ultra-pure W powdet and WSi_x.
KeyWords AITranslate
1山口悟 等.横滨金属部品工场にぉけゐグステン精练[J].资源と素材,1993,109(12):1-1.
1王庆相,范志康.W和W/Ti合金靶材的应用及其制备技术[J].粉末冶金技术,2009,27(1):52-57. 被引量:7
2万林生,陈玲,肖学有,赵立夫,章小兵,李飞.高纯钨酸铵溶液中活性炭深度除硫研究[J].中国钨业,2009,24(3):36-38. 被引量:3
3肖学有,赵立夫,万林生,李飞,杨亮,陈玲.二次离子交换饱和吸附工艺制备超纯APT[J].中国钨业,2009,24(3):39-42. 被引量:3
4万林生,代亚琦,赵立夫,肖学有,章小兵,李飞.高纯钨酸铵溶液中活性炭深度除钼研究[J].中国钨业,2009,24(6):20-22. 被引量:9
5刘文胜,龙路平,马运柱.高纯钨研究现状及制备工艺方法综述[J].粉末冶金技术,2012,30(3):223-228. 被引量:13
6李宝城,刘英,李继东,童坚,程紫辉,张金娥,臧慕文.GD-MS法测定高纯钨锭中多种痕量杂质元素[J].矿冶,2013,22(B11):149-151. 被引量:5
7刘文胜,龙路平,马运柱,刘业,刘书华.电子束熔炼提纯钨中杂质脱除静态动力学研究[J].稀有金属材料与工程,2015,44(1):113-117. 被引量:1
8张俊敏,闻明,谭志龙,王传军,沈月,易伟,管伟明,李艳琼.扩散阻挡层用WTi合金的制备及其表征[J].功能材料,2016,47(B12):125-129. 被引量:1
9崔子振,林岩松,石刚,李阳,张德智.退火温度对高纯钨靶显微组织和内应力的影响[J].宇航材料工艺,2017,47(4):63-65. 被引量:2
10魏修宇.半导体用高纯钨靶材的制备技术与应用[J].硬质合金,2017,34(5):353-359. 被引量:8
1沈洁,武甲,周志超,雷娜,杨艳龙,张敬蕊,张秀丽,刘利民.合金钢晶间氧化试样制备方法[J].理化检验:物理分册,2022,58(6):38-40.
2赵立夫,肖学有,万林生,李飞,杨亮,陈玲.二次离子交换饱和吸附法制取超高纯仲钨酸铵工艺优化[J].中国钨业,2009,24(4):32-35. 被引量:4
3万林生,代亚琦,赵立夫,肖学有,章小兵,李飞.高纯钨酸铵溶液中活性炭深度除钼研究[J].中国钨业,2009,24(6):20-22. 被引量:9
4万林生,习雪康,严永海,章小兵.高纯钨酸铵溶液结晶制取超高纯APT的研究[J].稀有金属与硬质合金,2010,38(4):6-9.
5鲁伟,徐蕾,余军霞,池汝安,郭嘉.含钨工业废料中提取与分离三氧化钨的研究[J].当代化工,2011,40(1):45-47. 被引量:3
6储志强.国内外磁控溅射靶材的现状及发展趋势[J].金属材料与冶金工程,2011,39(4):44-49. 被引量:23
7李宇凡.关于你和我的发烧[J].音响世界,2000(2):28-31.
8刘文胜,龙路平,马运柱.高纯钨研究现状及制备工艺方法综述[J].粉末冶金技术,2012,30(3):223-228. 被引量:13
9邓攀,曾颜亮,王坤,刘德刚.钼资源的回收技术现状及发展[J].山西冶金,2012,35(5):1-3. 被引量:5
10郭让民,淡新国,侯军涛.加压方式对钨钛合金真空热压烧结工艺的影响[J].热加工工艺,2013,42(10):120-122. 被引量:1
1钟培全.高纯钨粉生产新方法[J].中国钨业,1994,0(3):33-33. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]
Citation Information:
Brief description is made of the preparation of ultra-pure W powder and W materials abroad.In the paper is reported assaying results of the ultra-pure W powdet and WSi_x.
quote
| GB/T 7714-2015 | [1] ZHAO Qin-sheng. Preparation of Ultra-pure Tungsten Powder and Tungsten Material Abroad[J]. Rare Metals and Cemented Carbides, 2003(4): 56-57. |
| MLA | [1] ZHAO Qin-sheng. "Preparation of Ultra-pure Tungsten Powder and Tungsten Material Abroad." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 56-57. |
| APA | [1] ZHAO Qin-sheng. (2003). Preparation of Ultra-pure Tungsten Powder and Tungsten Material Abroad. Rare Metals and Cemented Carbides(4), 56-57. |
| IEEE | [1] ZHAO Qin-sheng, "Preparation of Ultra-pure Tungsten Powder and Tungsten Material Abroad," Rare Metals and Cemented Carbides, no. 4, pp. 56-57, 2003. keywords: {tungsten;high purity;powder;target materials} |