Regulating Lignin-Based Epoxy Vitrimer Performance by Fine-Tuning the Lignin Structure AITranslate

Shaanxi University of Science and Technology; Qilu University of Technology (Shandong Academy of Sciences); Shaanxi University of Science and Technology; AnHui Agricultural University; Beijing Forestry University; Shaanxi University of Science and Technology; Shaanxi University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lignin is the second most abundant lignocellulosic biomass, and as a natural polymer, it shows great potential in preparing functional materials to meet the demand for green/sustainable development. Unfortunately, the inherent heterogeneity of lignin largely limits its applications. Furthermore, the effect of the lignin structure on the performance of the final materials has seldom been investigated. In this work, a totally biobased dynamic cross-linked vitrimer with up to 70% lignin content was successfully prepared from epoxidized fractionated lignin and sebacic acid without additional chemical modifications. The lignin structure effect on the performance of the resultant lignin-based epoxy vitrimers (LEVs) was systematically investigated. The experimental results show that the phenolic hydroxyl content and the ratio of flexible to rigid linkages in lignin have strong correlations with the tensile strength, toughness, self-repair ability, and reprocessability of the resultant LEVs. Meanwhile, the molecular weight and the S/G ratio of lignin show strong correlations with the thermal properties of the resultant materials. This study not only presents a fundamental study regarding the relationships between lignin properties, and the resultant LEVs have great potential applications as advanced packaging materials for light-sensitive commodities due to the inherent UV resistance of lignin.

KeyWords AITranslate

fractionated lignin vitrimers relationship selfrepairing reprocessability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01541

Chinese Library Classification Number:

Citation Information:

Lignin is the second most abundant lignocellulosic biomass, and as a natural polymer, it shows great potential in preparing functional materials to meet the demand for green/sustainable development. Unfortunately, the inherent heterogeneity of lignin largely limits its applications. Furthermore, the effect of the lignin structure on the performance of the final materials has seldom been investigated. In this work, a totally biobased dynamic cross-linked vitrimer with up to 70% lignin content was successfully prepared from epoxidized fractionated lignin and sebacic acid without additional chemical modifications. The lignin structure effect on the performance of the resultant lignin-based epoxy vitrimers (LEVs) was systematically investigated. The experimental results show that the phenolic hydroxyl content and the ratio of flexible to rigid linkages in lignin have strong correlations with the tensile strength, toughness, self-repair ability, and reprocessability of the resultant LEVs. Meanwhile, the molecular weight and the S/G ratio of lignin show strong correlations with the thermal properties of the resultant materials. This study not only presents a fundamental study regarding the relationships between lignin properties, and the resultant LEVs have great potential applications as advanced packaging materials for light-sensitive commodities due to the inherent UV resistance of lignin.

quote

GB/T 7714-2015 [1] Rui Tang, Bailiang Xue, Jiaojun Tan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01541.
MLA [1] Rui Tang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01541.
APA [1] Rui Tang, Bailiang Xue, Jiaojun Tan, Ying Guan, Jialong Wen, Xinping Li, & Wei Zhao. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01541
IEEE [1] Rui Tang, Bailiang Xue, Jiaojun Tan, Ying Guan, Jialong Wen, Xinping Li, and Wei Zhao, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01541. keywords: {fractionated lignin;vitrimers;relationship;selfrepairing;reprocessability}