Metalloporphyrinyl-Phosphonates with Serrated Chain Structures: Exfoliation and NIR Photothermal Effect Metalloporphyrinyl-Phosphonates with Serrated Chain Structures: Exfoliation and NIR Photothermal Effect AITranslate
Abstract AITranslate
Near-infrared (NIR) photothermal materials have received significant attention due to their potential applications in photothermal therapy, diagnosis, and imaging. In this work, we constructed three mixed-ligand metal phosphonates, namely, Co(Ni–H6TPPP)(phen)(H2O)2 (CoNi), Ni(Ni–H6TPPP)(phen)(H2O)2 (NiNi), and Co(Co–H6TPPP)(phen)(H2O)2 (CoCo), where H10TPPP is 5,10,15,20-tetrakis(p-phenylphosphonic acid)-porphyrin and phen is 1,10-phenanthroline. These compounds are isostructural showing 1D serrated chain structures in which the porphyrin rings are stacked between the chains with π–π interactions. All displayed a broad absorption from the UV–vis to NIR (ca. 1500 nm) regions in the solid state. Interestingly, the chains in these compounds can be chemically exfoliated in water by adjusting the pH, forming interwoven nanostrands/nanosheets with thicknesses of one to several chains. The photothermal effect was observed for CoNi, NiNi, and CoCo in the solid state and in HEPES solution (pH = 7.4) upon 808 nm laser irradiation, among which CoCo showed the highest photothermal conversion efficiency. The important role of the cobalt(II) ion in the porphyrin ring and phenylphosphonic unit in extending π-electron delocalization and enhancing the absorption in the NIR region in CoCo is revealed by theoretical calculations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01438
Chinese Library Classification Number:
Citation Information:
Near-infrared (NIR) photothermal materials have received significant attention due to their potential applications in photothermal therapy, diagnosis, and imaging. In this work, we constructed three mixed-ligand metal phosphonates, namely, Co(Ni–H6TPPP)(phen)(H2O)2 (CoNi), Ni(Ni–H6TPPP)(phen)(H2O)2 (NiNi), and Co(Co–H6TPPP)(phen)(H2O)2 (CoCo), where H10TPPP is 5,10,15,20-tetrakis(p-phenylphosphonic acid)-porphyrin and phen is 1,10-phenanthroline. These compounds are isostructural showing 1D serrated chain structures in which the porphyrin rings are stacked between the chains with π–π interactions. All displayed a broad absorption from the UV–vis to NIR (ca. 1500 nm) regions in the solid state. Interestingly, the chains in these compounds can be chemically exfoliated in water by adjusting the pH, forming interwoven nanostrands/nanosheets with thicknesses of one to several chains. The photothermal effect was observed for CoNi, NiNi, and CoCo in the solid state and in HEPES solution (pH = 7.4) upon 808 nm laser irradiation, among which CoCo showed the highest photothermal conversion efficiency. The important role of the cobalt(II) ion in the porphyrin ring and phenylphosphonic unit in extending π-electron delocalization and enhancing the absorption in the NIR region in CoCo is revealed by theoretical calculations.
quote
| GB/T 7714-2015 | [1] MingFeng Qin, LiFeng Zheng, SongSong Bao, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01438. |
| MLA | [1] MingFeng Qin, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01438. |
| APA | [1] MingFeng Qin, LiFeng Zheng, SongSong Bao, FeiHu Xue, Jian Su, Jing Ma, & LiMin Zheng. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01438 |
| IEEE | [1] MingFeng Qin, LiFeng Zheng, SongSong Bao, FeiHu Xue, Jian Su, Jing Ma, and LiMin Zheng, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01438. keywords: {metalloporphyrine phosphonate chain NIR photothermal effect nanosheet} |