Preparation of Carbon-Doped Titanium Nitride Corrosion-Resistant Coating on Surface of Titanium Bipolar Plates AITranslate
Abstract AITranslate
To improve the corrosion resistance and conductivity of titanium bipolar plates in proton exchange membrane(PEM) water electrolyzer, a carbon-doped titanium nitride(C-TiN) composite protective coating was prepared on the surface of the titanium substrate by electrophoretic deposition-heat treatment, and its electrochemical corrosion performance was tested in the solution containing 0.5 mol/L H2SO4and 5 mg/L F-,which simulates the anode environment of PEM water electrolyzer.The results show that electrophoretic deposition and heat treatment improve the connectivity of titanium nitride nano-particles, enhance the adhesion between the coating and the substrate, and realize the rapid transfer of electrons in electroactive materials.The conductivity and corrosion resistance of the carbon-doped TiN coating prepared at 400 ℃ receive great promotion.Compared with the untreated sample, the contact resistance of the sample plated with C-TiN-400 ℃ coating can reach 2.25 mΩ·cm2 at the pressure of 146.3 N/cm2.
KeyWords AITranslate
1米万良,荣峻峰.质子交换膜(PEM)水电解制氢技术进展及应用前景[J].石油炼制与化工,2021,52(10):78-87. 被引量:9
2单东方,申桂鑫,彭善龙,王冬冬,刘月,张衡,王新东.电泳沉积制备质子交换膜水电解用钛双极板氮化钛涂层[J].电镀与涂饰,2022,41(7):497-501. 被引量:1
3崔金萍,陈温贤,郁非繁,曹诗雨,吕维扬,姚玉元.碳掺杂六方氮化硼/二硫化钼吸附还原六价铬和助催化降解有机污染物[J].高等学校化学学报,2021,42(10):3125-3134. 被引量:4
4何旭,罗马吉,陈奔.质子交换膜电解池内氧气泡输运过程特性[J].江苏大学学报:自然科学版,2021,42(2):139-144. 被引量:3
1李兵,章超,陈禄扬,许友生.极板与气体扩散层界面接触电阻研究进展[J].太原学院学报:自然科学版,2023,41(1):54-62.
2华思恒,杨东旺,唐昊,袁雄,展若雨,徐卓明,吕嘉南,肖娅妮,鄢永高,唐新峰.n型B_(i2)Te_(3)基材料表面处理对热电单元性能的影响[J].无机材料学报,2023,38(2):163-169.
3陈继园,李璐,李玉章,李雨耕,张兴国,张韦晨,李传勇.电沉积锌用铅基合金电化学腐蚀性性能研究[J].云南冶金,2023,52(1):100-105.
Basic Information:
DOI:
Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]
Citation Information:
To improve the corrosion resistance and conductivity of titanium bipolar plates in proton exchange membrane(PEM) water electrolyzer, a carbon-doped titanium nitride(C-TiN) composite protective coating was prepared on the surface of the titanium substrate by electrophoretic deposition-heat treatment, and its electrochemical corrosion performance was tested in the solution containing 0.5 mol/L H2SO4and 5 mg/L F-,which simulates the anode environment of PEM water electrolyzer.The results show that electrophoretic deposition and heat treatment improve the connectivity of titanium nitride nano-particles, enhance the adhesion between the coating and the substrate, and realize the rapid transfer of electrons in electroactive materials.The conductivity and corrosion resistance of the carbon-doped TiN coating prepared at 400 ℃ receive great promotion.Compared with the untreated sample, the contact resistance of the sample plated with C-TiN-400 ℃ coating can reach 2.25 mΩ·cm2 at the pressure of 146.3 N/cm2.
quote
| GB/T 7714-2015 | [1] SHAN Dong-fang, SHEN Gui-xin, PENG Shan-long, et al. Preparation of Carbon-Doped Titanium Nitride Corrosion-Resistant Coating on Surface of Titanium Bipolar Plates[J]. Rare Metals and Cemented Carbides, 2023(1): 86-91. |
| MLA | [1] SHAN Dong-fang, et al., "Preparation of Carbon-Doped Titanium Nitride Corrosion-Resistant Coating on Surface of Titanium Bipolar Plates." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 86-91. |
| APA | [1] SHAN Dong-fang, SHEN Gui-xin, PENG Shan-long, WANG Dong-dong, LIUYue, ZHANG Heng, LIU Li-li, & WANG Xin-dong. (2023). Preparation of Carbon-Doped Titanium Nitride Corrosion-Resistant Coating on Surface of Titanium Bipolar Plates. Rare Metals and Cemented Carbides(1), 86-91. |
| IEEE | [1] SHAN Dong-fang, SHEN Gui-xin, PENG Shan-long, WANG Dong-dong, LIUYue, ZHANG Heng, LIU Li-li, and WANG Xin-dong, "Preparation of Carbon-Doped Titanium Nitride Corrosion-Resistant Coating on Surface of Titanium Bipolar Plates," Rare Metals and Cemented Carbides, no. 1, pp. 86-91, 2023. keywords: {proton exchange membrane;carbon-doped titanium nitride;electrophoretic deposition;heat treatment;titanium bipolar plate;interface contact resistance} |