V2+/V3+ Redox Kinetics on Glassy Carbon in Acidic Electrolytes for Vanadium Redox Flow Batteries AITranslate

University of Michigan; University of Michigan; University of Michigan; University of Michigan
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vanadium redox flow batteries are a promising technology for energy storage, yet the mechanism of the kinetically limiting V2+/V3+ redox reaction remains poorly understood. Here, we elucidate the impact of anion complexation on V2+/V3+ kinetics on a glassy carbon electrode in three common electrolytes: hydrochloric acid, sulfuric acid, and mixed HCl/H2SO4. The V2+/V3+ kinetics are ∼2.5 times faster in HCl and have lower apparent activation energies than those in H2SO4 or HCl/H2SO4. We also identify the presence of [V(H2O)4Cl2]+ species in HCl by UV–vis spectroscopy. We confirm that the V2+/V3+ reaction proceeds via an adsorbed intermediate and propose a bridging mechanism through adsorbed *Cl (in HCl) and *OH (in H2SO4 or HCl/H2SO4). A bridging mechanism through *Cl is supported by even faster redox kinetics in HBr than in HCl, possibly due to the higher polarizability of *Br. By measuring the exchange current densities using steady-state current measurements and impedance spectroscopy, we show that the overall reaction is a two-electron process in HCl as opposed to a one-electron process in H2SO4 and HCl/H2SO4.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01423

Chinese Library Classification Number:

Citation Information:

Vanadium redox flow batteries are a promising technology for energy storage, yet the mechanism of the kinetically limiting V2+/V3+ redox reaction remains poorly understood. Here, we elucidate the impact of anion complexation on V2+/V3+ kinetics on a glassy carbon electrode in three common electrolytes: hydrochloric acid, sulfuric acid, and mixed HCl/H2SO4. The V2+/V3+ kinetics are ∼2.5 times faster in HCl and have lower apparent activation energies than those in H2SO4 or HCl/H2SO4. We also identify the presence of [V(H2O)4Cl2]+ species in HCl by UV–vis spectroscopy. We confirm that the V2+/V3+ reaction proceeds via an adsorbed intermediate and propose a bridging mechanism through adsorbed *Cl (in HCl) and *OH (in H2SO4 or HCl/H2SO4). A bridging mechanism through *Cl is supported by even faster redox kinetics in HBr than in HCl, possibly due to the higher polarizability of *Br. By measuring the exchange current densities using steady-state current measurements and impedance spectroscopy, we show that the overall reaction is a two-electron process in HCl as opposed to a one-electron process in H2SO4 and HCl/H2SO4.

quote

GB/T 7714-2015 [1] Harsh Agarwal, Jacob Florian, Bryan R. Goldsmith, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01423.
MLA [1] Harsh Agarwal, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01423.
APA [1] Harsh Agarwal, Jacob Florian, Bryan R. Goldsmith, & Nirala Singh. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01423
IEEE [1] Harsh Agarwal, Jacob Florian, Bryan R. Goldsmith, and Nirala Singh, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01423.