Preparation and Characterization of WO_3-TiO_2 Film Composite Photocatalyst in Ultrasonic Filed AITranslate
Abstract AITranslate
The nano-crystal composite WO3-TiO2 photocatalyst is prepared by sol-gel process in ultrasonic filed. Study is made of the effects of ammonium tungstate dosage,number of film coatings, sintering temperature and duration, various substrates,pH value,dissolved oxygen and the ultrasonic on the photocatalyric activity in the light of the film photo-degradation of rhodamine B. The results show that when compared with conventional sol-gel process,in the untrasonic field the gelating time of the sol is remarkably shortened, the particle size of the photocatalyst diminishes evidently and the photocatalytic activity increases significantly. The highest photocatalytic activity of WO3-TiO2 film is obtained with ammonium tungstate 0.5 % (mass), the porous Ti plate as sub strate, 9 layers of film coating, 1 h sintering at 575℃. resulting in the WO3-TiO2 film almost all of rutile TiO2.
KeyWords AITranslate
1Yu Jiaguo,et al.Effect of surface structure on photocatalytic activity of TiO2 thin films prepared by sol-gel method[J].Thin Solid Films,2000,(379):7.
2Zhang Qinghong,et al.Effects of calcinations on the photocatalytic properties of nanosized TiO2 powders prepared by TiCl4 hydrolysis[J].Applied Catalysis B(Envirobmental),2000,26:207.
3Gao Lian,et al.Effects of amorphous contents and particle size on the photocatalytic properties of TiO2 nanoparticles[J].Scripta Mater,2001,449:1 195.
4Wonyong Choi,et al.Investigation on TiO2-coated optical fibers for gas-phase photocatalytic oxidation of acetone[J].Applied Catalysis B(Environmental),2001,31:209.
5Sang Bum Kim,et al.Photocatalytic degradation of volatile organic compounds at the gas-solid interface of a TiO2 photocatalyst[J].Chemosphere,2002,48:437.
6Deng Zhongsheng,et al.Preparation and photocatalytic activity of TiO2-SiO2 binary aerogels[J].Nanostructured Materials,1999,11(8):1 313.
7H Cui,et al.Surface acidity and photocatalytic activity of Nb2O5/TiO2 photocatalysis[J].Journal of Solid State Chemistry,1995,115(1):187.
8Tae Kwon Young,et al.Photocatalytic behavior of WO3-loaded TiO2 in an oxidation reaction[J].Journal of Catalysis,2000,191(1):192.
9Nishikawa Harumitsu,et al.Adsorption and photocatalytic decomposition of odor compound containing sulfur using TiO2/SiO2 bead[J].Journal of Molecular Catalysis(A:Chemical),2001,172:247.
10Keller V,et al.Photocatalytic oxidation of butyl acetate in vapor phase on TiO2,Pt/TiO2 and WO3/TiO2 catalysis[J].Joural of Catalysis,2001,215(1):129.
1张惠芳,吕文英,刘国光,蔡河山,余林,李大光,易国斌,郭建伟.超声在TiO_2基光催化剂制备过程中的应用[J].应用化工,2007,36(1):78-80. 被引量:2
2李勇,郭晓玲,秦姹芳.超声波技术在纳米TiO_2制备和光催化中的应用[J].印染助剂,2009,26(9):9-12. 被引量:5
3张文朴.加大含钨催化剂研发力度 发展钨深加工化学品产业[J].中国钨业,2009,24(5):121-124. 被引量:3
4张惠芳,周德艳,孙玲.超声在TiO_2基光催化剂的制备和降解废水中的应用[J].化工新型材料,2011,39(3):19-21. 被引量:2
1王韵芳,樊彩梅.活性炭负载TiO_2的制备及其杀菌性能研究[J].山西化工,2008,28(2):1-4. 被引量:7
2张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3
3董汇泽,杨君丽,李会山.超声辅助光催化对川西獐牙菜种子萌发能力的影响[J].安徽农业科学,2010,38(31):17397-17398. 被引量:2
4周付建,夏畅斌,陈圆,张玲.超声-光催化还原铬(Ⅵ)和铜(Ⅱ)废水的研究[J].湖南科技大学学报:自然科学版,2011,26(3):116-119. 被引量:7
5杨君丽,董汇泽,侯全刚,李屹.超声波对2种蔬菜种子萌发能力的影响[J].种子,2011,30(12):97-98. 被引量:8
6张茜芸,仲兆平,姚杰.超声波强化均匀沉淀法制备纳米TiO_2[J].东南大学学报:自然科学版,2012,42(4):680-684. 被引量:1
7方林霞,刘雪,余萌.漂浮型Fe、Ce共掺杂TiO_2复合光催化剂的制备及性能研究[J].化工新型材料,2013,41(9):65-67. 被引量:1
8向乾坤,赵秀琴.钒氮共掺杂TiO_2降解亚甲基蓝影响因素的研究[J].湖北大学学报:自然科学版,2014,36(1):99-102. 被引量:1
9朱义,曲雯雯,杨坤,朱红波,彭金辉.微波辅助法制备TiO_2及其光催化性能[J].化工新型材料,2014,42(9):42-44. 被引量:2
10李峰,夏法锋,高媛媛,曹阳.超声电沉积在制备纳米复合镀层中的研究进展[J].材料导报,2016,30(3):125-127. 被引量:15
1刘奎仁,韩庆,陈建设,魏绪钧.光降解用WO_3-TiO_2复合光催化剂[J].东北大学学报:自然科学版,2003,24(11):1064-1067. 被引量:10
2李亭,王罗春,陈冠翰.三氧化钨-二氧化钛纳米管研究进展[J].山东化工,2015,44(11):45-48.
3王文涛,钟邦克.以多孔钛片为载体的氧化铝膜的制备和表征[J].物理化学学报,1996,12(1):85-90. 被引量:7
4牛微,张宇,张晨,荆生雨,黄盟盟.WO_3-TiO_2光阳极的制备及其光解水制氢性能研究[J].沈阳工程学院学报:自然科学版,2016,12(1):87-91. 被引量:1
5刘明志,程金树,袁坚.溶胶-凝胶法制备WO_3-TiO_2电致变色薄膜的研究[J].武汉工业大学学报,2000,22(3):22-23. 被引量:12
6杨雁飞,王丽,徐爱琴.TiO_2纳米材料溶胶凝胶法的制备、表征及光催化研究进展[J].长春理工大学学报:自然科学版,2009,32(5):153-154.
7陈伟龙,沈鸿烈,王威,李金泽.WO_3-TiO_2-ZnO溶胶的制备及其光致变色性能研究[J].人工晶体学报,2014,43(12):3113-3117. 被引量:2
8白波,董岁明,种法国.SiO_2-WO_3-TiO_2三元表面协同型光催化剂的性能研究[J].化工新型材料,2005,33(11):60-62. 被引量:4
9温敏,齐公台,孙菊梅.TiO_2溶胶的制备及其胶凝过程影响因素分析[J].表面技术,2004,33(1):30-31. 被引量:7
10向洪平,沈汝梁,邓浩强,戴如勇,吕俊佳,葛建芳.TiO_2溶胶稳定化制备工艺及机理研究[J].硅酸盐通报,2011,30(1):83-88. 被引量:8
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
The nano-crystal composite WO3-TiO2 photocatalyst is prepared by sol-gel process in ultrasonic filed. Study is made of the effects of ammonium tungstate dosage,number of film coatings, sintering temperature and duration, various substrates,pH value,dissolved oxygen and the ultrasonic on the photocatalyric activity in the light of the film photo-degradation of rhodamine B. The results show that when compared with conventional sol-gel process,in the untrasonic field the gelating time of the sol is remarkably shortened, the particle size of the photocatalyst diminishes evidently and the photocatalytic activity increases significantly. The highest photocatalytic activity of WO3-TiO2 film is obtained with ammonium tungstate 0.5 % (mass), the porous Ti plate as sub strate, 9 layers of film coating, 1 h sintering at 575℃. resulting in the WO3-TiO2 film almost all of rutile TiO2.
quote
| GB/T 7714-2015 | [1] YU Hui-wen, LIU Kui-ren, HAN Qing, et al. Preparation and Characterization of WO_3-TiO_2 Film Composite Photocatalyst in Ultrasonic Filed[J]. Rare Metals and Cemented Carbides, 2006(1): 1-4. |
| MLA | [1] YU Hui-wen, et al., "Preparation and Characterization of WO_3-TiO_2 Film Composite Photocatalyst in Ultrasonic Filed." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 1-4. |
| APA | [1] YU Hui-wen, LIU Kui-ren, HAN Qing, & WEI De-zhou. (2006). Preparation and Characterization of WO_3-TiO_2 Film Composite Photocatalyst in Ultrasonic Filed. Rare Metals and Cemented Carbides(1), 1-4. |
| IEEE | [1] YU Hui-wen, LIU Kui-ren, HAN Qing, and WEI De-zhou, "Preparation and Characterization of WO_3-TiO_2 Film Composite Photocatalyst in Ultrasonic Filed," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2006. keywords: {ultrasonic;sol-gel process;WO3-TiO2 film;photocatalytic;photodegradation} |