New Micro-filtration Device with Sintered PE Membrane and its Application in the Centralized Purification of Grinding Fluid for Cemented Carbide AITranslate
Abstract AITranslate
The structure, performance, working principle and technical parameters of the new micro-filtration device with sintered polyethylene (PE) membrane are introduced. The micro-filtration devices with sintered PE membrane and inorganic ceramic membrane are commercially applied respectively in the centralized purification treatment Of water-based grinding fluid for cemented carbide. With 40 m^3/h flow and 1μm precision,3-month continuous operation without flow loss is ensured for the micro-filtration device with sintered PE membrane by the simple process of "end filtration + back-blowing/backwashing". Compared with the inorganic ceramic micro-filtration device, the micro-filtration device with sintered PE membrane is much more economical and environmentally-friendly, quite adaptable to the centralized purification of grinding fluid for cemented carbide.
KeyWords AITranslate
1吴凤和.防止硬质合金刀具刃磨裂纹的工艺措施[J].工具技术,2002,36(2):44-44. 被引量:3
2安润喜.不同加工方法切削液的选择[J].机械工程与自动化,2006(4):157-158. 被引量:2
3宋显洪,周志鹤.微米级高分子精密过滤技术及应用[J].湖南化工,1999,29(5):12-13. 被引量:2
4刘晓东,李健生,张爱娟,孙秀云,王连军.氧化铝微滤膜的制备及表征[J].南京理工大学学报,2002,26(4):406-409. 被引量:4
1张琨英.硬质合金磨削液净化及控制系统的选择[J].稀有金属与硬质合金,2012,40(2):53-55.
2李长喜,王柱,王天雷,胡沈辉,赵文立.面向电子视窗硬脆材料的磨削液箱结构方案设计与仿真分析[J].机电工程技术,2019,48(2):4-8.
1彭旭鸣.谈多媒体语言实验室的技术参数[J].科技资讯,2010,8(10):16-16.
2吕丹.创新学习载体 搭建学习平台[J].中国职工教育,2011(2):43-43.
3韩望月.电动机连续运行控制电路信息化教学的实践与探讨[J].内蒙古教育:C,2015,0(9):69-69. 被引量:2
4李婵娟.自制化学实验教具感悟[J].大观周刊,2012(48):313-313.
5艾伦.投影机对比度辨析[J].中国教育技术装备,2010(5):50-51. 被引量:2
6贺忠庭.显微镜的一些常见数字[J].实验教学与仪器,2005,22(3):24-24.
7许振彪,李静.电动机连续运行控制电路信息化教学的实践与探讨[J].职业,2015,0(6):88-88. 被引量:3
8王建.情景课件制作室建设的思考与实践[J].现代教育技术,2007,17(6):85-87. 被引量:1
9陈自洋.视听(电子)阅览室基本功能、装备标准和技术参数考订[J].实验教学与仪器,2002,19(11):45-46.
10钱震.投影机与屏幕的选择[J].现代教育技术,2004,14(2):72-76. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:G580.15[文化科学—教育技术学]
Citation Information:
The structure, performance, working principle and technical parameters of the new micro-filtration device with sintered polyethylene (PE) membrane are introduced. The micro-filtration devices with sintered PE membrane and inorganic ceramic membrane are commercially applied respectively in the centralized purification treatment Of water-based grinding fluid for cemented carbide. With 40 m^3/h flow and 1μm precision,3-month continuous operation without flow loss is ensured for the micro-filtration device with sintered PE membrane by the simple process of "end filtration + back-blowing/backwashing". Compared with the inorganic ceramic micro-filtration device, the micro-filtration device with sintered PE membrane is much more economical and environmentally-friendly, quite adaptable to the centralized purification of grinding fluid for cemented carbide.
quote
| GB/T 7714-2015 | [1] HU Hui-ping, PENG Qi-fan, PENG Quan-fan. New Micro-filtration Device with Sintered PE Membrane and its Application in the Centralized Purification of Grinding Fluid for Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2009(1): 32-34. |
| MLA | [1] HU Hui-ping, et al., "New Micro-filtration Device with Sintered PE Membrane and its Application in the Centralized Purification of Grinding Fluid for Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2009, pp. 32-34. |
| APA | [1] HU Hui-ping, PENG Qi-fan, & PENG Quan-fan. (2009). New Micro-filtration Device with Sintered PE Membrane and its Application in the Centralized Purification of Grinding Fluid for Cemented Carbide. Rare Metals and Cemented Carbides(1), 32-34. |
| IEEE | [1] HU Hui-ping, PENG Qi-fan, and PENG Quan-fan, "New Micro-filtration Device with Sintered PE Membrane and its Application in the Centralized Purification of Grinding Fluid for Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 32-34, 2009. keywords: {sintered PE membrane;micro-filtration;grinding fluid;cemented carbide} |