daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Development and Application of Extraction Process for Ammonia Recovery to Prepare Ammonium Chloride AITranslate

Xiamen Tungsten Industry Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Extraction method was employed for ammonia recovery to prepare ammonium chloride instead of the traditional neutralization evaporation crystallization process.Through the selection and application of the organic phase,diluted ammonia from APT evaporation and crystallization stage was extracted and recovered,and then ammonium chloride was prepared by stripping with concentrated hydrochloric acid going back to the circuit as desorption agent.The whole process is in a relatively closed system to reduce the leakage of ammonia and improve the working environment.

KeyWords AITranslate

ammonia recovery ammonium chloride extraction method neutralization evaporation crystalliza tion process development and application

1黄文璞,孟笑.利用萃取吸收在钨冶炼中治理氨氮的方法:中国,CN102923805B[P].2014-03-05.

1李巍.密闭溶气气浮试验装置[J].油田地面工程,1992,11(6):44-49.

2张广瑞,万银霞,龚普勤,刘芳芝,胡利强.煤气化废水生化处理中曝气器的选型和应用[J].氮肥技术,2016,37(5):50-52.

3李玉,张乔,王群.蒸发结晶工艺在火电厂脱硫废水零排放中的应用[J].水处理技术,2016,42(11):121-122. 被引量:23

4周盛兵,芦昱.高效回收镍盐化工污泥制取硫酸镍的工艺研究[J].河南科技,2016,35(1):138-141. 被引量:1

5李涛.燃煤电厂脱硫废水蒸发结晶工艺比较[J].低碳世界,2015,0(28):86-87. 被引量:4

6汤静芳,郑建新.武钢四烧、五烧烟气氨法脱硫工艺比较[J].烧结球团,2015,40(2):45-49. 被引量:2

7彭巧玲,李新华.从黑钨精矿碱压煮萃取蒸发结晶工艺萃余液中回收硫酸钠[J].环境工程,1992,10(3):49-50.

8陈雷,宋东方.爪式干泵真空机组在化学原料药生产中的选型和应用[J].科技与企业,2014(19):191-192. 被引量:2

9四川彭州一制药公司发生爆炸 2人死亡[J].化工安全与环境,2006,19(5):14-14.

10崔凤霞,李荣,陈玮娜.高含盐废水零排放蒸发结晶技术进展[J].广州化工,2017,45(1):21-23. 被引量:19

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

Extraction method was employed for ammonia recovery to prepare ammonium chloride instead of the traditional neutralization evaporation crystallization process.Through the selection and application of the organic phase,diluted ammonia from APT evaporation and crystallization stage was extracted and recovered,and then ammonium chloride was prepared by stripping with concentrated hydrochloric acid going back to the circuit as desorption agent.The whole process is in a relatively closed system to reduce the leakage of ammonia and improve the working environment.

quote

GB/T 7714-2015 [1] HUANG Wen-pu. Development and Application of Extraction Process for Ammonia Recovery to Prepare Ammonium Chloride[J]. Rare Metals and Cemented Carbides, 2016(3): 9-11.
MLA [1] HUANG Wen-pu. "Development and Application of Extraction Process for Ammonia Recovery to Prepare Ammonium Chloride." Rare Metals and Cemented Carbides, no. 3, 2016, pp. 9-11.
APA [1] HUANG Wen-pu. (2016). Development and Application of Extraction Process for Ammonia Recovery to Prepare Ammonium Chloride. Rare Metals and Cemented Carbides(3), 9-11.
IEEE [1] HUANG Wen-pu, "Development and Application of Extraction Process for Ammonia Recovery to Prepare Ammonium Chloride," Rare Metals and Cemented Carbides, no. 3, pp. 9-11, 2016. keywords: {ammonia recovery;ammonium chloride;extraction method;neutralization evaporation crystalliza tion;process development and application}